China Astm B574 Uns N06455 Nickel Based Superalloy Hastelloy C-4 2.4610 Hastelloy Pipe
China Astm B574 Uns N06455 Nickel Based Superalloy Hastelloy C-4 2.4610 Hastelloy Pipe

  1. China Astm B574 Uns N06455 Nickel Based Superalloy Hastelloy C-4 2.4610 Hastelloy Pipe
  2. China Astm B574 Uns N06455 Nickel Based Superalloy Hastelloy C-4 2.4610 Hastelloy Pipe

Astm B574 Uns N06455 Nickel Based Superalloy Hastelloy C-4 2.4610 Hastelloy Pipe

  1. MOQ: Not limited
  2. Price: As Per Quotation
  3. Get Latest Price
Payment Terms T/T
Supply Ability 5000kg per Week
Delivery Time 25-35 days
Packaging Details Plywood Box
Brand Name ZHEMU
Model Number Standard and Customization
Certification ISO
Place of Origin CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 5000kg per Week
Delivery Time 25-35 days Packaging Details Plywood Box
Brand Name ZHEMU Model Number Standard and Customization
Certification ISO Place of Origin CHINA
High Light astm b574 uns n06455 ,Nickel Based Superalloy Hastelloy C-4 ,2.4610 hastelloy pipe
UNS N06455 Alloy HC4 Hastelloy Alloy Plate Pipe Forging Fitting Round Bar Stripe For Chemical Industry
 
PRODUCT DESCRIPTION

Introduction

Hastelloy C4 is a nickel-chromium-molybdenum alloy which has improved thermal stability. In this alloy, the tungsten was totally omitted and the iron content was reduced to approximately 1%. The alloy also contains approximately 0.3% Ti.

Density:8.64g/cm3

 

Character

Outstanding high-temperature stability; exhibits good ductility and corrosion resistance after long-time aging at 650 to 1040 °C (1200–1900 °F). Resists formation of grain-boundary precipitates in weld heat-affected zones, and is suitable for most chemical process applications in the as-welded condition. Has excellent resistance to stress-corrosion cracking and to oxidizing atmospheres up to 1040 °C (1900 °F).

 

Hastelloy C4 has exceptional resistance to a variety of chemical process environments, including hot contaminated mineral acids, solvents, chlorine, and chlorine-contaminated media (organic and inorganic, dry chlorine, formic and acetic acids, acetic anhydride, seawater, and brine). The general corrosion resistance of Alloy C276 and Alloy C4 was essentially the same in many corrosive environments, except that in strongly reducing media like hydrochloric acid, Alloy C276 was better; but in highly oxidizing media, the opposite was true, that is, Alloy C4 was better. Alloy C4 offers good corrosion resistance to a wide variety of media including organic acids and acid chloride solutions. This alloy has found greater acceptance in European countries in contrast to Alloy C276, which is more widely used and accepted in the United States.

 

Application

It has been widely used in the field of chemical engineering and high temperature environment. Typical application areas:

  • Flue gas desulfurization system
  • Acid pickling and acid recycling plant
  • Acetic acid and agricultural chemicals production
  • Titanium dioxide production (chlorine method)
  • Electrolytic plating

Chemical composition (%)

Cr=14.00~18.00, Mo=14.00~17.00, Fe≤3.00, C≤0.015, Si≤0.08, Co≤2.00, Mn≤1.00, P=≤0.04, S≤0.03, Ti≤0.07, Ni=Remainder

 

Forms of supply

  • Sheet
  • Plate
  • Bar
  • Pipe & Tube (welded & seamless)
  • Fittings
  • Wire

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Exporter,Seller

  • Year Established:

    2005

  • Employee Number:

    >100

  • Ecer Certification:

    Verified Supplier

Suzhou Zhemu Material Co., Ltd (refered as Zhemu afterwards) is a professional supplier of high performance alloys. Our factory is specialized in suppling Nickel alloys , Hastelloy Alloy, Incoloy Alloy, Monel Alloy, Duplex Stainless Steel, Titanium Alloy, Zirconium Alloy, Copper Alloy and other spec... Suzhou Zhemu Material Co., Ltd (refered as Zhemu afterwards) is a professional supplier of high performance alloys. Our factory is specialized in suppling Nickel alloys , Hastelloy Alloy, Incoloy Alloy, Monel Alloy, Duplex Stainless Steel, Titanium Alloy, Zirconium Alloy, Copper Alloy and other spec...

+ Read More

Get in touch with us

  • Reach Us
  • Suzhou Zhemu Industrial Equipment Co.,Ltd
  • Room 1002, Building 1, No. 18, Wuzhong East Road, Shuangta Street, Gusu District, Suzhou City, Jiangsu Province
  • https://www.alloy-nickel.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement