China factories

Chat Now Send Email
China factory - BEST PIPELINE EQUIPMENT CO.,LTD

BEST PIPELINE EQUIPMENT CO.,LTD

  • China,Suzhou ,Jiangsu
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China Alloy 718 Quenched and Tempered Forged Flange - Nickel-Based Superalloy for High
China Alloy 718 Quenched and Tempered Forged Flange - Nickel-Based Superalloy for High

  1. China Alloy 718 Quenched and Tempered Forged Flange - Nickel-Based Superalloy for High
  2. China Alloy 718 Quenched and Tempered Forged Flange - Nickel-Based Superalloy for High

Alloy 718 Quenched and Tempered Forged Flange - Nickel-Based Superalloy for High

  1. MOQ:
  2. Price:
  3. Get Latest Price

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

High Light Alloy 718 forged flange ,Nickel-based superalloy flange ,High-temperature welding neck flange
Alloy 718 Quenched and Tempered Forged Flange
Alloy 718 (commonly called Inconel 718 or Alloy 718) is a nickel-based superalloy widely used in aerospace, power generation, and high-temperature applications due to its excellent strength, creep resistance, and corrosion resistance.
Chemical Composition
The chemical composition is typically specified in weight percent. A standard composition range (per common specifications like ASTM and AMS) is approximately:
Element Composition Range
Nickel (Ni) 50.0 – 55.0%
Chromium (Cr) 17.0 – 21.0%
Iron (Fe) Balance (usually around 17 – 19%)
Niobium (Nb) + Tantalum (Ta) 4.75 – 5.50%
Molybdenum (Mo) 2.80 – 3.30%
Titanium (Ti) 0.65 – 1.15%
Aluminum (Al) 0.20 – 0.80%
Cobalt (Co) ≤ 1.0%
Manganese (Mn) ≤ 0.35%
Silicon (Si) ≤ 0.35%
Copper (Cu) ≤ 0.30%
Carbon (C) ≤ 0.08%
Phosphorus (P) ≤ 0.015%
Sulfur (S) ≤ 0.015%
Boron (B) ≤ 0.006%
Key Composition Features
  • Nickel-chromium base: The high nickel (around half the alloy) and significant chromium content provide excellent high-temperature strength and oxidation/corrosion resistance.
  • Nb, Ti, and Al for strengthening: Niobium, titanium, and aluminum form precipitates (γ'' and γ' phases) during heat treatment, which gives Alloy 718 its remarkable strength up to around 650°C.
  • Iron as balance: Unlike some other nickel superalloys that are almost all Ni + Cr, 718 keeps costs more manageable by using iron as a balancing element while maintaining high performance.
  • Tight control of impurities: Low carbon, sulfur, and phosphorus levels are crucial for weldability, toughness, and resistance to cracking.
Important Note: When selecting or verifying Alloy 718 for engineering or industrial use, always refer to the exact specification you're working to (e.g., ASTM B637, AMS 5662/5663/5664, etc.), as slight variations in composition and heat treatment are allowed depending on product form and required properties.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company,Seller,Other

  • Year Established:

    2010

  • Total Annual:

    1000000-5000000

  • Employee Number:

    116~209

  • Ecer Certification:

    Verified Supplier

Best Alloy Engineering Alloy Pipe as s a reference point for excellence in the manufacture and distribution of fittings, piping, bends, forged flanges , clad products and specialties for the upstream, midstream and downstream sectors of oil & gas, thermal and nuclear power generation. The C... Best Alloy Engineering Alloy Pipe as s a reference point for excellence in the manufacture and distribution of fittings, piping, bends, forged flanges , clad products and specialties for the upstream, midstream and downstream sectors of oil & gas, thermal and nuclear power generation. The C...

+ Read More

Get in touch with us

  • Reach Us
  • BEST PIPELINE EQUIPMENT CO.,LTD
  • China Factory : Suzhou Industrial Park, JiangSu Province,China
  • https://www.alloysteelseamlesspipe.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement