Payment Terms | T/T, L/C, D/P, Western Union, MoneyGram |
Supply Ability | 7500 tons/per month |
Delivery Time | 60-120 days |
Packaging Details | 24 pallets for one 20GP container |
Al2O3 | 40-55 |
Fe2O3 | 0-1.7 |
Apparent porosity | 20-28 |
Bulk density | 2.1-2.2 |
Cold crushing strength | 30-60 |
0.2MPa,Refractoriness under load | 1400-1550 |
PLC | 0.1~0.4 |
Refractoriness | 30~40 |
Brand Name | Annec |
Certification | ISO |
Place of Origin | China |
View Detail Information
Explore similar products
2.20 Low Bulk Density Coke Oven SiO2 Clay Refractory Brick
Lite refractory fire clay bricks with Cheap, durable, fire, insulation, sound
Pizza Oven Light Weight High Density 2.3g Clay Fired Brick
Anti Corrosion Hot Blast Stove 55 Al2O3 Clay Refractory Brick
Product Specification
Payment Terms | T/T, L/C, D/P, Western Union, MoneyGram | Supply Ability | 7500 tons/per month |
Delivery Time | 60-120 days | Packaging Details | 24 pallets for one 20GP container |
Al2O3 | 40-55 | Fe2O3 | 0-1.7 |
Apparent porosity | 20-28 | Bulk density | 2.1-2.2 |
Cold crushing strength | 30-60 | 0.2MPa,Refractoriness under load | 1400-1550 |
PLC | 0.1~0.4 | Refractoriness | 30~40 |
Brand Name | Annec | Certification | ISO |
Place of Origin | China | ||
High Light | 1730 degrees Clay Refractory Brick ,1690 Degrees Clay Refractory Brick ,1690 Degrees Fire Resistant Clay Bricks |
Smelting Furnace 1690 1730 Degrees Clay Refractory Brick
Definition:
Fire Resistant Clay Fire Bricks is made from clinker clay by mixing, forming, drying, sintering and matching characterized by good resistance to corrosion and abrasion, good thermal shock resistance, good spelling resistance, high mechanical strength, good volume stability under very high temperature.
The resistance of Fire Resistant Clay Fire Bricks is comparable to that of silica bricks, up to 1690~1730℃, but the softening temperature under load is more than 200℃ lower than that of silica bricks. In addition to the high refractory mullite crystals, the Fire Resistant Clay Fire Bricksalso contain nearly half of the low melting point amorphous glass phase.
In the temperature range less than1000℃, the volume of clay brick expands evenly with the increase of temperature. The linear expansion curve is approximately a straight line, and the linear expansion rate is 0.6%~0.7%, which is only about half of that of silica brick.
When the temperature reaches 1200 ℃ and going on rise, its volume will start to shrink from the maximum expansion.
The residual shrinkage of Fire Resistant Clay Fire Bricksleads to the loosening of mortar joints in masonry, which is a major disadvantage of Fire Resistant Clay Fire Bricks.
When the temperature exceeds 1200°C, the low melting point substances in the clay bricks gradually melt, and the particles are tightly pressed against each other due to surface tension, resulting in volume shrinkage.
Advantage:
1. High refractoriness,
2. High-temperature endurable.
3. Good corrosion resistance.
4. Good spalling resistance and wear resistance.
5. Good thermal shock resistance.
6. High mechanical strength.
7. High-temperature creep rate is low.
8. Good volume stability at high temperature.
Application:
The refractory linings of hot surfaces or backing heat-insulating layers of other refractory materials. The refractory linings or heat-insulating materials of the industrial furnaces in the petroleum or chemical industries , such as , ethylene pyrolysis furnaces, tubular furnaces, reforming furnaces of synthetic ammonia, gas generators and high-temperature shuttle kilns, etc.
Product Description:
Fired Clay Refractory Assembly Brick | ||||
Item | Unit | RN-42 | HRN-42 | HRN-48 |
AL2O3 % | % | ≥42 | ≥42 | ≥48 |
Fe2O3 % | % | ≤ 1.7 | ≤ 1.7 | ≤ 1.7 |
Refractoriness | ℃ | ≥1750 | ≥1750 | ≥1750 |
Bulk density | g/cm3 | ≥2.15 | ≥2.15 | ≥2.35 |
Apparent porosity | % | ≤ 24/23 | ≤ 24/21 | ≤ 24/21 |
cold crushing strength | Mpa | ≥30 | ≥40 | ≥40 |
0.2MPa,Refractoriness under load,℃ | ℃ | ≥ 1400 | ≥ 1520 | ≥ 1550 |
Permanent linear change | % | 0~-0.3 | 0~-0.3 | 0~-0.3 |
thermal shock resistance, | cycle | ≥ 20 | ≥30 | ≥40 |
Packaging and shipping
Standard packing: waterproof inner packing + outer packing suitable for container transportation
Company Details
Business Type:
Manufacturer,Exporter
Year Established:
2003
Total Annual:
100,000,000-120,000,000
Employee Number:
700~730
Ecer Certification:
Verified Supplier
Zhengzhou ANNEC Industrial CO., Ltd. was founded at Sep, 2003, and has been a NASDAQ listed corporation since 2011(Stock code: ANNC). ANNEC had become refractory industrial leader provide core service such as refractory production, technology of blast furnace and hot blast stove and EP... Zhengzhou ANNEC Industrial CO., Ltd. was founded at Sep, 2003, and has been a NASDAQ listed corporation since 2011(Stock code: ANNC). ANNEC had become refractory industrial leader provide core service such as refractory production, technology of blast furnace and hot blast stove and EP...
Get in touch with us
Leave a Message, we will call you back quickly!