| Temperature Fluctuation | ±0.1℃ |
| Model | DSC-600 |
| Temperature Range | Room temperature ~ 800℃ Air cooling |
| Temperature Resolution | 0.1℃ |
| Heating Rate | 0.1~80 ℃/min |
| Certificate | ISO, CE |
| Product name | Durable Differential Scanning Calorimetry Machine for Precise Thermal Measurement of Plastics Polymers and Material Testing |
| Payment Terms | T/T,L/C,Western Union,D/A,D/P |
| Supply Ability | 30 sets per month |
| Delivery Time | 7 work days |
| Packaging Details | Standard export wooden box |
| DSC Range | 0~±500mW |
| Brand Name | JINHAIHU |
| Model Number | DSC-600 |
| Certification | ISO9001, CE |
| Place of Origin | BEIJING, CHINA |
View Detail Information
Explore similar products
Plastics 500mW Dsc Differential Scanning Calorimetry Machine
Determination Glass Transition Temperature Differential Scanning Calorimetry
0.1mW Oxidation Induction Time Test Machine For Plastic Analysis
Melting Crystallization Temperature Enthalpy ISO Heat Measure Instrument
Product Specification
| Temperature Fluctuation | ±0.1℃ | Model | DSC-600 |
| Temperature Range | Room temperature ~ 800℃ Air cooling | Temperature Resolution | 0.1℃ |
| Heating Rate | 0.1~80 ℃/min | Certificate | ISO, CE |
| Product name | Durable Differential Scanning Calorimetry Machine for Precise Thermal Measurement of Plastics Polymers and Material Testing | Payment Terms | T/T,L/C,Western Union,D/A,D/P |
| Supply Ability | 30 sets per month | Delivery Time | 7 work days |
| Packaging Details | Standard export wooden box | DSC Range | 0~±500mW |
| Brand Name | JINHAIHU | Model Number | DSC-600 |
| Certification | ISO9001, CE | Place of Origin | BEIJING, CHINA |
| High Light | durable differential scanning calorimetry machine ,precise thermal measurement machine for plastics ,material testing DSC machine with warranty | ||
Differential Scanning Calorimetry (DSC) is a classical thermal analysis technique designed to characterize thermal effects of materials under programmed temperature conditions. It is extensively employed across materials science and chemistry sectors—including R&D, process optimization, quality control, and failure analysis—for its high precision and versatility.
DSC enables systematic investigation of key material properties: phase transitions of inorganic materials, melting and crystallization behaviors of polymer materials, polymorphism of pharmaceutical compounds, and the solid-liquid phase ratio of oils and fats.
Differential Scanning Calorimetry (DSC) enables precise quantification of heat-associated physical and chemical changes in materials, covering key parameters including:
| Parameter | Specification |
|---|---|
| DSC Range | 0~±500mW |
| Temperature Range | Room temperature ~ 800℃ Air cooling |
| Heating Rate | 0.1~80 ℃/min |
| Temperature Resolution | 0.1℃ |
| Temperature Fluctuation | ±0.1℃ |
| Temperature Repeatability | ±0.1℃ |
| DSC Noise | 0.01mW |
| DSC Resolution | 0.01mW |
| DSC Accuracy | 0.01mW |
| DSC Sensitivity | 0.01mW |
| Temperature Control Mode | Heating, constant temperature (full program automatic control) |
| Curves Scan | Heating scan |
| Atmosphere Control | Instrument automatically switches |
| Display | 24bit color 7-inch LCD touch-screen display |
| Data Interface | Standard USB interface |
| Parameter Standards | With a standard substance; a key calibration function; the user can correct the temperature and enthalpy personally |
| Remark | All the technical indicators can be adjusted according to user needs |
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2013
Employee Number:
50~100
Ecer Certification:
Verified Supplier
Beijing Jinshengxin testing machine Co., Ltd, covering 20,000 square meters, is located in Jinhaihu Town of Beijing. Since founded in 2003, our company has been devoted to the research, development and manufacture of testing machines for metallic and non-metallic materials, especially b... Beijing Jinshengxin testing machine Co., Ltd, covering 20,000 square meters, is located in Jinhaihu Town of Beijing. Since founded in 2003, our company has been devoted to the research, development and manufacture of testing machines for metallic and non-metallic materials, especially b...
Get in touch with us
Leave a Message, we will call you back quickly!