China factories

Chat Now Send Email
China factory - China Hunan High Broad New Material Co.Ltd

China Hunan High Broad New Material Co.Ltd

  • China,Changsha ,Hunan
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China High Purity Scandium Metal Applied In Various Superalloys
China High Purity Scandium Metal Applied In Various Superalloys

  1. China High Purity Scandium Metal Applied In Various Superalloys
  2. China High Purity Scandium Metal Applied In Various Superalloys
  3. China High Purity Scandium Metal Applied In Various Superalloys

High Purity Scandium Metal Applied In Various Superalloys

  1. MOQ: 100g
  2. Price: TBA
  3. Get Latest Price
Payment Terms T/T, Western Union, L/C, D/A, D/P, T/T,
Packaging Details Scandium in vacuum packaging
Supply Ability 100kgs each year
Delivery Time About 7 days
Material Scandium
Purity TREM 99-99.95%, Sc/TREM 99.9% min.
Crystal Structure: Hexagonal closed-packed
Chemical Formula Sc
Application 99.9 Scandium Metal Applied In Various Superalloys
Brand Name High Broad
Model Number 99.9 Scandium
Certification ISO
Place of Origin CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T, Western Union, L/C, D/A, D/P, T/T, Packaging Details Scandium in vacuum packaging
Supply Ability 100kgs each year Delivery Time About 7 days
Material Scandium Purity TREM 99-99.95%, Sc/TREM 99.9% min.
Crystal Structure: Hexagonal closed-packed Chemical Formula Sc
Application 99.9 Scandium Metal Applied In Various Superalloys Brand Name High Broad
Model Number 99.9 Scandium Certification ISO
Place of Origin CHINA
High Light High Purity Scandium Metal ,ISO Scandium Metal ,7440-20-2 Scandium Metal

High Purity Scandium Metal Applied In Various Superalloys

 

High Broad is able to supply scandium metal in purities from 99.5% to 99.999%, as well as scandium oxide (Sc2O3) in purities from 99.99% min. Please contact us with your specific requirement or for a current scandium price.

 

Scandium is a very light elemental metal that is often found alongside the rare earth elements. Due to it's rarity and high price, scandium does not have a lot of commercial applications, but is used in specialty halide lamps, as well as lightweight, high-strength alloys. It is estimated that only as little as a couple hundred kilograms of scandium metal are produced each year.

 

Chemical Formula: Sc
Description: Light, silvery-grey metal
Purity: TREM 99-99.95%, Sc/TREM 99.9% min.
Packing: As required
CAS No: 7440-20-2

 

RE Element Max. Impurity (ppm) Element Max Impurity (ppm)
La 4.5 Mn 9.3
Ce 7.3 Fe 20.8
Pr 3.5 Si 10.2
Nd 6.9 Ca 9.9
Sm 4.3 Mg 1.3
Eu 1.9 Cu 9.4
Gd 8.3 Ni 5.7
Tb 4.4 Al 34.9
Dy 5.9 Zn 4.0
Ho 8.2 Ti 35.2
Er 5.5 Ag 1.6
Tm 6.3 Cd 0.8
Yb 2.0 O 280

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Exporter,Seller

  • Year Established:

    2006

  • Total Annual:

    15000000-20000000

  • Employee Number:

    50~100

  • Ecer Certification:

    Verified Supplier

China Hunan High Broad New Material was founded in 2006, focus on the business in advanced new material and service. Including: design, installation, material , engineering, maintenance and technical support.   Our sales office located in Changsha, Hunan province, plant located in Hunan,S... China Hunan High Broad New Material was founded in 2006, focus on the business in advanced new material and service. Including: design, installation, material , engineering, maintenance and technical support.   Our sales office located in Changsha, Hunan province, plant located in Hunan,S...

+ Read More

Get in touch with us

  • Reach Us
  • China Hunan High Broad New Material Co.Ltd
  • No.70 Chezhan North Road,Changsha,Hunan,China
  • https://www.cathodicprotection-anodes.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement