| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | 30000PCS/MONTH |
| Delivery Time | 10-25 working days |
| Packaging Details | foam sheet inside and wooden case outside |
| chemical composition | CoCrW |
| Advantage | wear and corrosion and high temperature resistance |
| Hardness | 38-55HRC |
| Density | 8.4-8.8g/cm3 |
| drawing made | accept |
| size | OD 8-200mm |
| Process | casting |
| Brand Name | SYTOP |
| Model Number | TP002 |
| Certification | ISO9001 |
| Place of Origin | Liaoning,Shenyang |
View Detail Information
Explore similar products
Cobalt Chrome Molybdenum Alloy Castings , Cobalt Steel Alloy Rods
Glasswool Industry Nickel Cobalt Alloy Castings Centrifugal Pump Apparatus
2.4879 Iron Nickel Based Cobalt Chrome Alloy Centrifugal Spinners For Glass Wool
Different Specifications Cobalt Alloy Castings , Cobalt Chromium Tungsten Round
Product Specification
| Payment Terms | L/C, T/T, Western Union, MoneyGram | Supply Ability | 30000PCS/MONTH |
| Delivery Time | 10-25 working days | Packaging Details | foam sheet inside and wooden case outside |
| chemical composition | CoCrW | Advantage | wear and corrosion and high temperature resistance |
| Hardness | 38-55HRC | Density | 8.4-8.8g/cm3 |
| drawing made | accept | size | OD 8-200mm |
| Process | casting | Brand Name | SYTOP |
| Model Number | TP002 | Certification | ISO9001 |
| Place of Origin | Liaoning,Shenyang | ||
| High Light | nickel alloy castings ,cobalt based alloys | ||
SYTOP cobalt base alloys is a range of cobalt-chromium-tungsten alloys with wear resistance, corrosion and high thermal resistance. It is widely used in oil & gas, machinery, wood cutting, automotive, paper and food processing industry etc.
| Material Choose | Typical Application | Process |
| ST 6 | Steam and chemical valve seat , oil and gas pump sleeve, ,butterfly valve bushing ,hot-dip galvanized production line used bushing etc. | investment casting
|
| ST 3 | Pump sleeve ,rotary ring , valve seats | |
| ST 12 | Extrusion die , hot impact die and saw teeth | |
| ST 100 | Extrusion die , hot-impact die and saw teeth | |
| ST 20 | Pump sleeves , rotary rings , bearing sleeves , valve balls |
Chemical compositions and properties (%)
| Brand | C | Mn | Si | Cr | Ni | Mo | W | Co | Fe | P | S | Density (g/cm3) | Hardness (HRC) |
| ST 3 | 2.0-2.7 | 1.0 | 1.0 | 29-33 | 3.0 | 11-14 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.55 | 51-55 | |
| ST 6 | 0.9-1.4 | 1.0 | 1.5 | 27-31 | 3.0 | 1.5 | 3.5-5.5 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.35 | 38-44 |
| ST 12 | 1.1-1.7 | 1.0 | 1.0 | 28-32 | 3.0 | 7.0-9.5 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.40 | 44-49 | |
| ST 20 | 2.2-3.0 | 2.0 | 30-34 | 3.0 | 1.0 | 14-18 | Bal. | 3.0 | ≤0.05 | ≤0.05 | 8.65 | 53-59 | |
| Tantung-G 25 | 2.2-2.8 | 1-3 | 27-32 | 7 | Ta/Nb | 14-19 | Bal. | 2-5 | 8.84 | 57-60 | |||
| Tantung-G35 | 3.3-3.8 | 1-3 | 27-32 | 7 | Ta/Nb | 14-19 | Bal. | 2-5 | 8.80 | 60-63 | |||
| Tribaloy 400 | 0.04 | 2.5-2.7 | 8-10 | 27-29 | Bal. | 55 | |||||||
| Tribaloy 800 | 0.04 | 3.2-3.6 | 16-18 | 27-29 | Bal. | 58 |
Production process of our thermowell tube
1. Powder metallurgy process
A. Better metallurgical structure, better strength
B. Various types of automatic pressing machines from 3 tons to 630 tons. The ordered profiles can be very flexible.
2. Investment casting process
Different volume of furnaces, the order quantity can be very flexible.
3. Machining
CNC, lathing, drilling, milling, grinding, wire cutting, polishing
![]()
Production process
Powder metallurgy pocess. It has better strength than casting parts, better granule structure and avoiding the troubles caused by casting defects.
![]()
Company activity :
![]()
Related products :
![]()
FAQ
| Q1: What is the Warranty for our products ? |
| A1: We own high precision grading machine to control geometry dimensions and apply ultra fine grain size substrate coated with high performance coatings to guarantee the lifetime of our products, which can satisfy every working condition.If any quality problems on our side occurred in this period , we will take on the shipping cost and replacement. |
| Q2: Do you provide free samples? |
| A2: Yes, usually we provide free samples for testing under the condition of freight paid by customer. |
| Q3: What is your minimum order requirement? |
| A3: We will indicate the MOQ for each item in the quotation sheet. We accept the sample and trial order. If the quantity of single item can't reach the MOQ, the price should be sample price. |
| Q4: What is the delivery time of your products? |
| A4: It depends on the inventory availability.If items needed are in stock, the delivery time would be within 8 work days, but if not the delivery time would be around 20 work days. |
| Q5: Can you manufacture Special-shaped products? |
| A5: Yes, we can. We can produce both standard and special prosucts. We can make them according to your drawings and samples. |
| Q6: May I have my order working schedule? |
| A6: Yes, we will send working schedule of your order each week. We will inspect and test all merchandise in case of damaging and missing parts before shipment. The detailed inspection pictures of the order will be sent to you for your confirmation before delivery. |
Our service
Research and development(R &D):
We have a mature technical team that can assist customers to develop new products and grow together;
Design:
We can provide free design according to the samples or drawings provided by customers;
Customer service:
We can provide complete customer service support, including logistics, technical services, equipment commissioning etc;
Processing:
We can provide OEM manufacturing services according to customer’s demand.
Note: The price is determined by the design drawings and mould size , please provide the drawings or sample data to us, we will give you a quote ASAP(within 8 hours).
Send your inquiry details right now !!!
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Exporter,Seller
Year Established:
2001
Total Annual:
3million-5million
Employee Number:
50~100
Ecer Certification:
Verified Supplier
Founded in 2001, Shenyang Top New Materials Co., Ltd. has concentrated on research, development and production of cobalt-base alloys, silver tungsten alloys and metal ceramics for many years. The company has established good cooperative relations with scientific research institution... Founded in 2001, Shenyang Top New Materials Co., Ltd. has concentrated on research, development and production of cobalt-base alloys, silver tungsten alloys and metal ceramics for many years. The company has established good cooperative relations with scientific research institution...
Get in touch with us
Leave a Message, we will call you back quickly!