| Payment Terms | TT L/C |
| Supply Ability | 10000000per month |
| Packaging Details | standard waterproof package |
| Delivery Time | 7-14 business days |
| Thickness | 3-120mm |
| Martensite-Ferritic | Ss 405 , 409, 409L, 410, 420, 420J1 , 420J2 , 420F , 430 ,431... |
| Surface Finish | No. 1, No. 4, No. 8, HL, 2B, BA |
| Standard | ASTM, JIS, DIN, AISI, KS, EN |
| OEM | YES |
| Name | Stainless Steel Rod Bar |
| Place of Origin | Made in China |
| Brand Name | Vespolari Jiangsu |
| Certification | ISO SGS ROHS |
View Detail Information
Explore similar products
329 347H 310S Stainless Steel Rod Bar Oxidation Resistance 5mm SS Rod
UNS S31600 EN1.4401 Stainless Steel Rod Bar Polished SS 316 Round Bar
UNS S32100 EN1.4541 Stainless Steel Rod Bar 15mm SS 321 Round Bar
16mm 18mm 20mm Stainless Steel Rod Bar Duplex 2205 Round Bar
Product Specification
| Payment Terms | TT L/C | Supply Ability | 10000000per month |
| Packaging Details | standard waterproof package | Delivery Time | 7-14 business days |
| Thickness | 3-120mm | Martensite-Ferritic | Ss 405 , 409, 409L, 410, 420, 420J1 , 420J2 , 420F , 430 ,431... |
| Surface Finish | No. 1, No. 4, No. 8, HL, 2B, BA | Standard | ASTM, JIS, DIN, AISI, KS, EN |
| OEM | YES | Name | Stainless Steel Rod Bar |
| Place of Origin | Made in China | Brand Name | Vespolari Jiangsu |
| Certification | ISO SGS ROHS | ||
| High Light | Ferritic Austenitic Duplex Stainless Steel Rod ,OEM duplex stainless steel rod ,Pitting Corrosion Resistance 2507 Round Bar | ||
2507 Stainless steel bar
| Specifications of Stainless Steel Bar | |||
| Commodity | Stainless Steel Round Bar/Flat Bar/Angle Bar/Square Bar/Channel | ||
| Standard | AISI, ASTM, DIN, GB, JIS, SUS | ||
| Material | 301, 304, 304L, 309S, 321, 316, 316L, 317, 317L, 310S, 201,202,321, 329, 347, 347H 201, 202, 410, 420, 430, S20100, S20200, S30100, S30400, S30403, S30908, S31008, S31600, S31635, etc. | ||
| Certification | SGS, BV, etc | ||
| Surface | Bright, Polished, Turn smooth(Peeled),Brush, Mill, Pickled etc. | ||
| Delivery Time | 7-15 days after confirming the order. | ||
| Trade Time | FOB, CIF, CFR | ||
| Payment | T/T or L/C | ||
| MOQ | 1 Ton | ||
| Specification | Item | Size | Finish |
| Stainless steel round bar | 19*3mm-140*12mm | Black&Pickled&Bright | |
| Stainless steel flat bar | 19*3mm-200*20mm | Black&Pickled&Bright | |
| Stainless steel square bar | Hot rolled: S10-S40mm Cold rolled: S5-S60mm | Hot rolled&Annealed&Pickled | |
| Stainless steel angle bar | 20*20*3/4mm-180*180*12/14/16/18mm | White acid& Hot rolled&Polished | |
| Stainless steel channel | 6#, 8#, 10#, 12#, 14#, 16#, 18#, 20#, 22#, 24# | White acid& Hot rolled&Polished&Sandblast | |
| Chemical Properties of Frequently-used Austenitic Stainless Steel Material Grade | |||||||||||
| ASTM | UNS | EN | JIS | C% | Mn% | P% | S% | Si% | Cr% | Ni% | Mo% |
| 201 | S20100 | 1.4372 | SUS201 | ≤0.15 | 5.5-7.5 | ≤0.06 | ≤0.03 | ≤1.00 | 16.00-18.00 | 3.5-5.5 | - |
| 202 | S20200 | 1.4373 | SUS202 | ≤0.15 | 7.5-10.0 | ≤0.06 | ≤0.03 | ≤1.00 | 17.00-19.00 | 4.0-6.0 | - |
| 301 | S30100 | 1.4319 | SUS301 | ≤0.15 | ≤2.00 | ≤0.045 | ≤0.03 | ≤1.00 | 16.00-18.00 | 6.0-8.0 | - |
| 304 | S30400 | 1.4301 | SUS304 | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 18.00-20.00 | 8.0-10.5 | - |
| 304L | S30403 | 1.4306 | SUS304L | ≤0.03 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 18.00-20.00 | 8.0-12.0 | - |
| 309S | S30908 | 1.4883 | SUS309S | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 22.00-24.00 | 12.0-15.0 | - |
| 310S | S31008 | 1.4845 | SUS310S | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤1.50 | 24.00-26.00 | 19.0-22.0 | - |
| 316 | S31600 | 1.4401 | SUS316 | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 16.00-18.00 | 10.0-14.0 | - |
| 316L | S31603 | 1.4404 | SUS316L | ≤0.03 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 16.00-18.00 | 10.0-14.0 | 2.0-3.0 |
| 317L | S31703 | 1.4438 | SUS317L | ≤0.03 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 18.00-20.00 | 11.0-15.0 | 2.0-3.0 |
| 321 | S32100 | 1.4541 | SUS321 | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 17.00-19.00 | 9.0-12.0 | 3.0-4.0 |
| 347 | S34700 | 1.4550 | SUS347 | ≤0.08 | ≤2.00 | ≤0.045 | ≤0.03 | ≤0.75 | 17.00-19.00 | 9.0-13.0 | - |
![]()
![]()
![]()
![]()
| Packing: seaworthy wooden pallets,water proof paper,pvc film,interleaving paper, in 20' or 40' container or as per customers' requirements. |
| -- 20ft GP:5898mm(Length)x2352mm(Width)x2393mm(High) |
| -- 40ft GP:12032mm(Length)x2352mm(Width)x2393mm(High) |
| -- 40ft HC:12032mm(Lengh)x2352mm(Width)x2698mm(High) |
![]()
![]()
Q1:How about the shipping fees?
Shipping costs will depend upon many factors. Express will be the quickest but will be most expensive. Sea freight is ideal for large quantities, but slower. Please contact us for specific shipping quotes, which are dependent upon quantity, weight, mode and destination.
Q2:What are your prices?
Our prices are subject to change depending on supply and other market factors. We will send you an updated price list after you contact us for further information.
Q3:Do you have a minimum order quantity?
Yes, we do have minimum orders for specific international products, please contact us for more information.
Company Details
Business Type:
Manufacturer,Exporter,Trading Company,Seller
Year Established:
2021
Total Annual:
6000000-10000000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
JIANGSU VESPOLARI STEEL IMPORT & EXPORT CO., LTD. VESPOLARI is a professional manufacturer of Aluminum products in China. Dedicated to strict quality control and thoughtful customer service, our experienced staff member available to discuss your requirements and ensure full custom... JIANGSU VESPOLARI STEEL IMPORT & EXPORT CO., LTD. VESPOLARI is a professional manufacturer of Aluminum products in China. Dedicated to strict quality control and thoughtful customer service, our experienced staff member available to discuss your requirements and ensure full custom...
Get in touch with us
Leave a Message, we will call you back quickly!