| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | 500 tons per month |
| Delivery Time | 5-20 Days |
| Packaging Details | Hastelloy X packed in spool,in coil then in carton,in woodencase |
| Material | Ni Cr Fe Mo |
| Elongation | 30 % |
| Brinell hardness HB | ≤220 |
| Density | 8.22 g/cm3 |
| Tensile strength Rm N/mm² | 760MPA |
| Yieldstrength R P0. 2 N/mm² | 345MPA |
| Electrical Resistivity(24℃)) | 1180 µΩ·m |
| Thermal Conductivity(32℃) | 9.1 W/m·K |
| Melting Range | 260-1355°C |
| Specific Heat | 486 J/kg·K |
| Standard | Rod: ASTM B572 |
| Brand Name | DLX |
| Model Number | Hot Selling Nickel Based alloy Bright Soft Hastelloy B-3 Alloy Wire |
| Place of Origin | China Jiangsu |
| Certification | CE,ROHS |
View Detail Information
Explore similar products
Hastelloy C276 UNS N10276 B574 Nickel Chromium Molybdenum
Hastelloy C22 UNS N06022 ASTM B574 Chromium Molybdenum
Acetic Anhydride 345MPA C4 N06455 Soft Hastelloy Alloy
Soft 760 MPA N06455 C4 ASTM B575 Nickel Chromium Molybdenum
Product Specification
| Payment Terms | L/C, T/T, Western Union, MoneyGram | Supply Ability | 500 tons per month |
| Delivery Time | 5-20 Days | Packaging Details | Hastelloy X packed in spool,in coil then in carton,in woodencase |
| Material | Ni Cr Fe Mo | Elongation | 30 % |
| Brinell hardness HB | ≤220 | Density | 8.22 g/cm3 |
| Tensile strength Rm N/mm² | 760MPA | Yieldstrength R P0. 2 N/mm² | 345MPA |
| Electrical Resistivity(24℃)) | 1180 µΩ·m | Thermal Conductivity(32℃) | 9.1 W/m·K |
| Melting Range | 260-1355°C | Specific Heat | 486 J/kg·K |
| Standard | Rod: ASTM B572 | Brand Name | DLX |
| Model Number | Hot Selling Nickel Based alloy Bright Soft Hastelloy B-3 Alloy Wire | Place of Origin | China Jiangsu |
| Certification | CE,ROHS | ||
| High Light | Hastelloy X Seamless Tube ,UNS N06002 Hastelloy Tube ,ASTM B622 Nickel Based Superalloy | ||
![]()
ASTM B622 Nickel-Based Superalloy UNS N06002 hastelloy X seamless tube | Pipe
Hastelloy X tubes in various components due to their excellent high-temperature strength, oxidation resistance, and corrosion resistance. Some specific areas within gas turbine engines where Hastelloy X tubes are utilized include:
Combustion Chambers: Hastelloy X tubes are used in the combustion chambers of gas turbine engines where they are exposed to high temperatures, combustion gases, and thermal cycling. The high-temperature strength and resistance to oxidation make Hastelloy X tubes ideal for withstanding the harsh conditions within the combustion chamber.
Afterburners: In afterburner systems of gas turbine engines, where additional thrust is generated by igniting fuel in the exhaust stream, Hastelloy X tubes are employed due to their ability to withstand high temperatures and thermal stresses. The corrosion resistance of Hastelloy X is also beneficial in this demanding environment.
Exhaust Systems: Hastelloy X tubes are used in the exhaust systems of gas turbine engines to channel hot gases away from the engine and into the atmosphere. The high-temperature strength and resistance to oxidation of Hastelloy X ensure that the tubes can withstand the high exhaust temperatures without degrading.
Heat Exchangers: In some gas turbine engine designs, Hastelloy X tubes are also used in heat exchangers to transfer heat between different fluid streams. The corrosion resistance and thermal stability of Hastelloy X make it suitable for use in heat exchanger applications within gas turbine engines.
Overall, Hastelloy X tubes play a critical role in ensuring the reliability and performance of gas turbine engines by providing the necessary strength and resistance to high temperatures and harsh operating conditions. Their use in key components helps enhance the efficiency and durability of gas turbine engines in aerospace, power generation, and other industrial applications.
Hastelloy X is commonly used in high-temperature applications such as gas turbine engines, industrial furnace components, and structural components for aerospace and power generation industries. Its unique combination of properties makes it suitable for environments where high temperatures, oxidation, and corrosion resistance are critical requirements.
| The Chemical Composition of Hastelloy X, % | |
|---|---|
| Ni | balance |
| Cr | 20.5-23.0 |
| Fe | 17.0-20.0 |
| Mo | 8.0-10.0 |
| Co | 0.5-2.5 |
| W | 0.20-1.00 |
| C | 0.05-0.15 |
| Mn | ≤1.00 |
| Si | ≤1.00 |
| P | ≤0.040 |
| S | ≤0.030 |
| Density | Melting Range | Specific Heat | Thermal Conductivity | Electrical Resistivity |
|---|---|---|---|---|
| g/cm3 | °C | J/kg.k | W/m.k | µΩ·m |
| 8.22 | 1260-1355 | 486 | 9.1 | 1180 |
| Product Form | Standard |
|---|---|
| Rod | ASTM B572 |
| Plate, sheet and strip | ASTM B435, B906 |
| Seamless pipe and tube | ASTM B622 |
| Welded pipe | ASTM B619, B775 |
| Welded tube | ASTM B626, B751 |
| Welding fitting | ASTM B366 |
| Billet and bar for reforging | ASTM B472 |
![]()
![]()
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2002
Total Annual:
1000000-120000000+
Employee Number:
100~150
Ecer Certification:
Verified Supplier
Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...
Get in touch with us
Leave a Message, we will call you back quickly!