China K418 (713C) Cast Superalloy Master Alloy Bar
China K418 (713C) Cast Superalloy Master Alloy Bar

  1. China K418 (713C) Cast Superalloy Master Alloy Bar
  2. China K418 (713C) Cast Superalloy Master Alloy Bar
  3. China K418 (713C) Cast Superalloy Master Alloy Bar
  4. China K418 (713C) Cast Superalloy Master Alloy Bar
  5. China K418 (713C) Cast Superalloy Master Alloy Bar
  6. China K418 (713C) Cast Superalloy Master Alloy Bar
  7. China K418 (713C) Cast Superalloy Master Alloy Bar
  8. China K418 (713C) Cast Superalloy Master Alloy Bar
  9. China K418 (713C) Cast Superalloy Master Alloy Bar

K418 (713C) Cast Superalloy Master Alloy Bar

  1. MOQ: Trial quantity available; production minimum confirmed per grade and diameter
  2. Price: Quoted per order against grade, diameter and quantity
  3. Get Latest Price
Product Form Master alloy bar, cast round bar
Packaging Details Rod bundles with protective wrapping, export wooden cases
Casting Route Bar casting
Batch Records Lot-specific records issued with the bar
Grade K418 (713C)
Customization Diameter and cut length to order
Supply Ability 10,000 tons per year
Impurity Control Limits defined for the critical elements of the grade
Melting Route Vacuum melting
Composition Control Verified against the grade agreed on the order
Delivery Time 15-30 days
Surface Clean, consistent finish
Internal Quality Uniform structure assessed where the order requires it
Diameter Range 8.0 mm to 200 mm
Model Number K418 (713C)
Brand Name DLX
Place of Origin Changzhou, Jiangsu, China
Certification ISO 9001, SGS

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Product Form Master alloy bar, cast round bar Packaging Details Rod bundles with protective wrapping, export wooden cases
Casting Route Bar casting Batch Records Lot-specific records issued with the bar
Grade K418 (713C) Customization Diameter and cut length to order
Supply Ability 10,000 tons per year Impurity Control Limits defined for the critical elements of the grade
Melting Route Vacuum melting Composition Control Verified against the grade agreed on the order
Delivery Time 15-30 days Surface Clean, consistent finish
Internal Quality Uniform structure assessed where the order requires it Diameter Range 8.0 mm to 200 mm
Model Number K418 (713C) Brand Name DLX
Place of Origin Changzhou, Jiangsu, China Certification ISO 9001, SGS
ISO 9001 & SGS Certified | Vacuum Melted Master Alloy | 12,000 m² Plant

K418 (713C) master alloy bar is cast in diameters from 8.0 mm to 200 mm for foundries that introduce alloying elements at the melt. Vacuum melting and bar casting run on one site, the composition of each lot is verified against the grade agreed on the order, and trial quantities can be supplied ahead of a production lot.

Cast Superalloy Master Alloy Bar

Master Alloy Bar: What It Is and Where It Stops

A master alloy is an intermediate material. It is added to a melt to introduce selected alloying elements and to bring the heat to the target composition, and it is consumed at that stage instead of being machined into a component. That places it in a different category from a finished alloy bar, a wire or a strip. Those products are bought for the geometry and the properties of the part being made. This one is bought for what it carries into the melt and for how consistently it carries it.

The grade name is a melt addition specification. K418 (713C) master alloy bar is ordered by grade and diameter, and acceptance is set by the composition and the impurity limits agreed for that grade rather than by a component drawing.

Cast Superalloy Master Alloy Bar Precision Application

Cast Superalloy Master Alloy Bar Product


Specifications

Grade K418 (713C)
Product Form Master alloy bar, cast round bar
Diameter Range 8.0 mm to 200 mm
Melting Route Vacuum melting
Casting Route Bar casting
Composition Control Verified against the grade agreed on the order
Impurity Control Limits defined for the critical elements of the grade
Internal Quality Uniform structure assessed where the order requires it
Surface Clean, consistent finish
Length Cut to order
Trial Quantity Supplied ahead of a production lot
Packing Rod bundles with protective wrapping, export wooden cases

Key Strengths

  • Cast in diameters from 8.0 mm to 200 mm.
  • Composition verified against the agreed grade before dispatch.
  • Impurity limits set for critical elements such as Al, Si and Fe.
  • Vacuum melting and bar casting on one site.
  • Trial quantities available before a production lot.

Technical Details

What a Melt Addition Has to Deliver

Three requirements travel with a master alloy. The elements it carries have to arrive in the proportion the heat needs. The elements that must stay low have to stay low, because a small quantity of a tramp element introduced at this stage spreads through the entire heat. And the bar has to behave predictably when it is charged, which depends on the melting route and on how the bar is dimensioned for the charging practice in use.

Five Checks Applied to Every Lot

  • Composition control: each lot is verified against the grade agreed on the order before it is released.
  • Impurity limits: the elements that affect the target alloy are held inside the limits agreed for the grade.
  • Microstructure: structure uniformity is assessed where the order calls for it.
  • Melt compatibility: the grade is matched to the base alloy and to the melting practice it will be charged into.
  • Batch consistency: lot-specific records are kept so a repeat order can be compared with the previous one.

Vacuum Melting, Composition Control and Bar Casting

The route runs in seven steps, from material selection through vacuum melting, composition control and bar casting to cutting and cleaning, then inspection and packing of the finished master alloy bar. The melt is made under vacuum, and the composition check sits between the melt and the casting step, so any correction is made before the bar is cast.

Trial Quantity Before a Production Lot

A foundry charging a new grade usually wants one heat's worth of material first. Trial quantities are supplied for that purpose and are cast through the same route as a production lot, so the trial heat represents what follows. The grade, the diameter and the quantity are agreed at that stage and carried forward to the production order.

Cast Superalloy Master Alloy Bar Attributes


Application Field

Master alloy bar in K418 (713C) is charged in investment casting operations and in the production of cast components for high-temperature duty. Typical settings include aero engine castings, automotive turbocharger wheels, chemical pumps and valves, and glass manufacturing hardware.


Cast Superalloy Master Alloy Bar Application Field

Quality Assurance

Each lot is analysed for composition and verified against the grade agreed on the order. Surface is checked for cracks, pits and contamination, and internal soundness is confirmed by inspection where the order requires it. The mill test certificate issued for the lot states the composition of the material supplied, so the bar and the certificate can be checked against each other on arrival.

Cast Superalloy Master Alloy Bar Comparison

Cast Superalloy Master Alloy Bar Process

References

Grade classification follows the cast superalloy grade series used in the Chinese standard system for high-temperature alloys. Composition and impurity limits are verified against the grade agreed on the order, and batch-level chemistry and structure are checked against in-house inspection records and the mill test certificate issued with each lot.

Packaging & Delivery

Bar is supplied in rod bundles with protective wrapping, packed in export wooden cases and labelled with the grade, the diameter and the lot number. Production runs are scheduled 15-30 days from order confirmation, and trial quantities are scheduled ahead of the production run. Freight is quoted to the destination port.

Cast Superalloy Master Alloy Bar Supply & Delivery


About DLX Alloy

Changzhou DLX Alloy Co., Ltd. has melted and processed alloys since 2002, on a 12,000 m² site with ISO 9001 and SGS certification and an annual capacity of 10,000 tons. The master alloy line applies the same melting and casting discipline used across the alloy range: the composition of the heat is fixed before the bar is cast, and the lot record follows the material to the customer.

Send the grade, the diameter, the quantity and the destination port for a quotation.

changzhou dlx alloy

FAQ

Q: What is a master alloy bar used for?
A: It is added to a melt to introduce selected alloying elements and to bring the heat to the target composition. It is consumed at the melting stage.

Q: Should a foundry order K418 (713C) master alloy bar or a finished alloy bar?
A: The two are bought for different reasons. A finished bar is bought for the geometry and the properties of the part made from it. A master alloy bar is bought for the elements it carries into the melt.

Q: How is the composition controlled?
A: Each lot is verified against the grade agreed on the order, and the mill test certificate issued with it states the composition of the material supplied.

Q: Which diameters can be supplied?
A: 8.0 mm to 200 mm as standard, with the cut length made to order.

Q: Can a trial quantity be ordered before a production lot?
A: Yes. Trial quantities are cast through the same route as a production lot, and the grade, diameter and quantity agreed at that stage carry forward to the production order.

Q: What is the minimum order quantity?
A: The minimum is set by the diameter and the quantity required, and is confirmed together with the grade when the order is placed.

Q: Which documents come with a lot?
A: A mill test certificate stating the composition of the lot, with the packing list and the export documents for the destination.

Q: How is the bar packed for shipment?
A: Rod bundles with protective wrapping in export wooden cases, labelled with the grade, the diameter and the lot number.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Seller

  • Year Established:

    2002

  • Total Annual:

    1000000-120000000+

  • Employee Number:

    100~150

  • Ecer Certification:

    Verified Supplier

Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...

+ Read More

Get in touch with us

  • Reach Us
  • Changzhou DLX Alloy Co., Ltd.
  • NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
  • https://www.dlx-alloy.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement