| Payment Terms | L/C,D/A,D/P,T/T |
| Production Schedule | 15-30 days from order confirmation |
| Product Form | Cast master alloy bar, round section |
| Packaging Details | Rod bundles with protective wrapping, export wooden cases |
| Delivery Time | 5-20 Days |
| Melting Route | Vacuum melting |
| Grade | K213 |
| Grade Agreement | Composition and impurity limits fixed on the order |
| Supply Ability | 10,000 tons per year |
| Diameter Range | 8.0 mm to 200 mm |
| Customization | Diameter and cut length to order |
| Model Number | K213 |
| Brand Name | DLX |
| Place of Origin | Changzhou, Jiangsu, China |
| Certification | ISO9001 & SGS |
View Detail Information
Explore similar products
Nimonic 75 N06075 ISO 9001 High Temperature Nickel Alloy
Nickel Alloy Wire With High Electrical And Thermal Conductivity Corrosion
Non Magnetic Polished High Temperature Nickel Alloy Tube High Strength
780 MPA ISO 9001 Nimonic 80A High Temperature Nickel Alloy
Product Specification
| Payment Terms | L/C,D/A,D/P,T/T | Production Schedule | 15-30 days from order confirmation |
| Product Form | Cast master alloy bar, round section | Packaging Details | Rod bundles with protective wrapping, export wooden cases |
| Delivery Time | 5-20 Days | Melting Route | Vacuum melting |
| Grade | K213 | Grade Agreement | Composition and impurity limits fixed on the order |
| Supply Ability | 10,000 tons per year | Diameter Range | 8.0 mm to 200 mm |
| Customization | Diameter and cut length to order | Model Number | K213 |
| Brand Name | DLX | Place of Origin | Changzhou, Jiangsu, China |
| Certification | ISO9001 & SGS |
K213 master alloy bar is cast to order in Changzhou in round sections from 8.0 mm to 200 mm. Grade and cut length are agreed before the cast, so the lot enters the schedule in one pass and leaves for the nominated port packed and documented.
![]()
Buyers who have ordered melt additions before know the pattern: the melt itself is quick, and the time is spent in front of it. An order that arrives without a cut length waits for an answer. One that arrives without a packing instruction waits again. Each missing item becomes a separate exchange, and the lot moves back in the queue while the answer is pending.
That is why this page is arranged around the sequence rather than the material. What is settled at the enquiry decides when the cast can be scheduled. What is settled at the cast decides when the bar can be cut, packed and handed to the forwarder.
![]()
![]()
| Grade | K213 |
| Product Form | Cast master alloy bar, round section |
| Diameter Range | 8.0 mm to 200 mm |
| Melting Route | Vacuum melting |
| Casting Route | Bar casting |
| Grade Agreement | Composition and impurity limits fixed on the order |
| Cut Length | Made to the charging length used at the foundry |
| Internal Quality | Uniform structure assessed where the order requires it |
| Surface | Clean, consistent finish |
| Case Marking | Grade, diameter and lot number on each case |
| Packing | Rod bundles with protective wrapping, export wooden cases |
| Production Schedule | 15-30 days from order confirmation |
A melt addition is cast against a particular composition rather than drawn from general stock, because the grade agreement belongs to the customer who placed the order. A supplier that offers a grade as shelf stock is really offering whatever was left from another cast. Ordering a lot against your own grade agreement is the slower route on paper, and it is the one that keeps the incoming inspection predictable.
Five items open the schedule: the grade, the diameter, the cut length, the quantity and the packing instruction. When all five are on the enquiry, the cast can be placed without a round of questions. When one is missing, the exchange that fills it is what stands between the enquiry and the furnace.
Cut length is the item most often left open, and it is the one that costs the most time later. If the foundry charges with pieces of a fixed length, that length is stated on the order and the bar is cut to it at the works. Bar that arrives in a different length is cut again on site, which adds a handling step in the foundry and a second weighing before the heat.
The cut bar is bundled and wrapped against moisture, then cased. Each case carries the grade, the diameter and the lot number, and the case numbers repeat on the packing list. The consignment is then booked for the sea leg against the port named on the enquiry. Marking and packing happen as the lot leaves the line, so the cases and the list are prepared before the container is loaded rather than after.
Master alloy bar in K213 is charged in investment casting operations for parts that run at high temperature, among them aero engine castings, automotive turbocharger wheels, chemical pumps and valves, and glass manufacturing hardware.
![]()
![]()
Composition and impurity limits are checked against the grade agreed on the order, the surface is inspected for cracks, pits and contamination, and internal soundness is confirmed where the order asks for it. The certificate issued with the lot describes the material as packed, so the consignee can set the document against the cases at the port and against the previous lot on a repeat order.
![]()
![]()
Grade names on this page follow the cast grade series for high-temperature alloys in the Chinese standard system. Each lot is checked against the grade agreed on the order, and the chemistry and structure of that lot are set against the works inspection record and the certificate released with the consignment.
Bar is bundled with protective wrapping and packed in export wooden cases, marked with the grade, the diameter and the lot number. A production lot takes 15-30 days on the schedule, counted from order confirmation, and a smaller quantity is placed ahead of the production run. Freight terms are quoted to the destination port on FOB, CFR or CIF against the port named on the enquiry.
![]()
Changzhou DLX Alloy Co., Ltd. began melting alloys in 2002 and has run the same works since, adding capacity as the order book grew. Today the site covers 12,000 m², carries ISO 9001 and SGS certification, and turns out up to 10,000 tons a year for customers in more than 60 export countries. Master alloy lots are scheduled against the grade agreed with the customer, and the handling sequence described above is the one used for them.
Put the grade, the diameter, the cut length and the quantity in the enquiry and the lot is placed in the schedule from there.
![]()
Q: Is K213 master alloy bar available from stock?
A: Lots are cast against the grade agreed with the customer rather than drawn from general stock, because the composition belongs to the order. What a recent cast does shorten is the scheduling, since the grade is already set up.
Q: What shortens the time between enquiry and cast?
A: A complete enquiry. The grade, the diameter, the cut length, the quantity and the packing instruction let the cast be placed without a round of questions.
Q: Why does the cut length matter so much?
A: Bar cut to the charging length in use at the foundry goes into the crucible directly. Bar in another length is cut again on site, which adds a step and a weighing before the heat.
Q: How are the cases prepared for dispatch?
A: The cut bar is bundled, wrapped against moisture and cased, with the grade, the diameter and the lot number on each case and case numbers that match the packing list.
Q: Which shipping terms are quoted?
A: FOB, CFR or CIF to the port named on the enquiry, quoted with the lot rather than separately.
Q: What is the minimum order quantity?
A: It is fixed by the diameter and the quantity needed, and is settled at the same time as the grade so the cast size is known.
Q: What is the delivery time?
A: A production lot is placed 15-30 days after order confirmation, and a smaller quantity is scheduled ahead of the production run.
Q: Can a grade be cast again to the same agreement later?
A: Yes. The lot record is retained, so a repeat order is set against the grade agreement already used and does not need to be re-specified.
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2002
Total Annual:
1000000-120000000+
Employee Number:
100~150
Ecer Certification:
Verified Supplier
Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...
Get in touch with us
Leave a Message, we will call you back quickly!