| Delivery Time | 5-20 Days |
| Payment Terms | L/C,T/T,Western Union,MoneyGram |
| Supply Ability | 500 tons per month |
| Elongation | 30% |
| Brand No | Alloys 625 NS3306 NO6625 2.4856 |
| Application | Heat Exchanger |
| Specific Heat | 444 J/kg-°C |
| Melting Range | 1332-1380 ℃ |
| Type | Nickel Pipe |
| Low Temperature Resistance | Down To -253°C |
| Specific Heat Capacity | 0.431 J/g-°C |
| Brand Name | DLX |
| Model Number | Inconel Alloy |
| Place of Origin | China Jiangsu |
| Certification | CE,ROHS |
View Detail Information
Explore similar products
1034 MPA High Temperature Nickel Alloy 625 Tubing
Vessels 1034 MPA Bright Bar Inconel Alloy 625 Inconel Alloy
Hard Bright UNS N06625 1034 MPA Inconel 625 Sheet
Refining RoHS Bright Surface Inconel 601 Round Bar
Product Specification
| Delivery Time | 5-20 Days | Payment Terms | L/C,T/T,Western Union,MoneyGram |
| Supply Ability | 500 tons per month | Elongation | 30% |
| Brand No | Alloys 625 NS3306 NO6625 2.4856 | Application | Heat Exchanger |
| Specific Heat | 444 J/kg-°C | Melting Range | 1332-1380 ℃ |
| Type | Nickel Pipe | Low Temperature Resistance | Down To -253°C |
| Specific Heat Capacity | 0.431 J/g-°C | Brand Name | DLX |
| Model Number | Inconel Alloy | Place of Origin | China Jiangsu |
| Certification | CE,ROHS | ||
| High Light | inconel alloy For Business ,Business inconel alloy | ||
The Incoloy Alloy 20 Plate Sheet is a type of alloy product made from Inconel Alloy that is specifically designed to provide high resistance to acid attack and pitting corrosion. It is commonly used in chemical processing equipment, heat exchangers, and storage tanks. The high resistance to corrosion makes it ideal for use in harsh environments where other materials may fail.
In addition to its corrosion resistance, the Incoloy Alloy 20 Plate Sheet has other notable properties. Its specific heat capacity is 0.431 J/g-°C, which means that it can absorb a large amount of heat before its temperature increases. This property makes it ideal for use in high-temperature applications where heat transfer is critical.
The Incoloy Alloy 20 Plate Sheet also has an elongation of 30%, which means that it can be formed into various shapes without cracking or breaking. This property makes it easier to work with and allows for more flexibility in design.
Finally, the Incoloy Alloy 20 Plate Sheet has excellent low-temperature resistance, with the ability to withstand temperatures down to -253°C. This property makes it ideal for use in cryogenic applications where other materials may become brittle and fail.
Overall, the Incoloy Alloy 20 Plate Sheet is a versatile alloy product that offers excellent corrosion resistance, high strength, and other notable properties. It is a popular choice for use in chemical processing equipment, heat exchangers, and storage tanks, among other applications. If you are looking for an alloy steel metal that can withstand harsh environments and high temperatures, the Incoloy Alloy 20 Plate Sheet is an excellent choice.
The Inconel Alloy from DLX is commonly used in the aerospace, chemical processing, and nuclear industries. Its high elongation of 30% makes it ideal for use in applications where high temperatures and pressures are present. The solid solution + acid white surface finish of this product also makes it highly resistant to corrosion, which is especially important in harsh industrial environments.
One of the primary applications of Inconel Alloy is in the aerospace industry. The alloy's excellent mechanical properties make it ideal for use in aircraft engines, where it can withstand high temperatures and pressures. Inconel Alloy is also used in the chemical processing industry, where it is commonly used in heat exchangers and other equipment that comes in contact with corrosive chemicals. The nuclear industry also relies on Inconel Alloy for its resistance to radiation and corrosion, making it a popular choice for components in nuclear reactors.
Inconel Alloy's yield strength of 310 MPa makes it a reliable choice for a wide range of applications. Its high-temperature resistance and corrosion resistance make it an excellent choice for use in extreme environments. Whether you're working in the aerospace, chemical processing, or nuclear industries, DLX's Inconel Alloy is a reliable choice for all your alloy steel metal needs.
Our team of experts provides technical support and services for Inconel Alloy product to ensure maximum performance and efficiency. We offer comprehensive material testing, analysis, and evaluation to identify any potential issues and provide solutions to enhance the durability of the product. Our services also include custom fabrication, welding, and machining to meet the specific needs of our customers. In addition, we offer training and consultation services to ensure proper installation, operation, and maintenance of the product. We are committed to providing high-quality technical support and services to ensure customer satisfaction and maximize the lifespan of the Inconel Alloy product.
Product Packaging:
Shipping:
Q: What is the brand name of this product?
A: The brand name of this product is DLX.
Q: What is the model number of this product?
A: The model number of this product is Inconel Alloy.
Q: Where is this product manufactured?
A: This product is manufactured in China.
Q: What are the key properties of Inconel Alloy?
A: Inconel Alloy is a nickel-chromium alloy known for its high temperature resistance, corrosion resistance, and strength. It can withstand extreme environments such as high pressure and high temperature.
Q: What are some common applications of Inconel Alloy?
A: Inconel Alloy is commonly used in aerospace, chemical processing, nuclear power generation, and marine engineering industries, among others.
Company Details
Business Type:
Manufacturer,Seller
Year Established:
2002
Total Annual:
1000000-120000000+
Employee Number:
100~150
Ecer Certification:
Verified Supplier
Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...
Get in touch with us
Leave a Message, we will call you back quickly!