China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
China K4169 Cast Superalloy Master Alloy Bar for Investment Casting

  1. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  2. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  3. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  4. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  5. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  6. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  7. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  8. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting
  9. China K4169 Cast Superalloy Master Alloy Bar for Investment Casting

K4169 Cast Superalloy Master Alloy Bar for Investment Casting

  1. MOQ:
  2. Price:
  3. Get Latest Price

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

High Light K4169 cast superalloy bar ,nickel alloy for investment casting ,high temperature master alloy bar
Vacuum-Cast Lots | Lot Record with Every Consignment | ISO 9001 & SGS Certified

K4169 master alloy bar is cast for investment casting shops working on aero engine programmes, in diameters from 8.0 mm to 200 mm, with the grade agreed before the cast and a lot record issued with the material.

Why Aero Casting Programmes Push the Requirement Upstream

An investment casting shop working to an aero programme carries requirements that travel further back than its own gate. The casting is bought against a specification, the specification names the alloy, and the alloy is built from a melt that was charged with additions. When the casting is audited, the questions reach the material that went into the heat: which grade was added, from which lot, and against what agreement.

That is why an order of this kind is settled on the grade and on the record, while the geometry of the bar follows from the charging practice rather than from a component drawing.

铸造高温合金母合金棒

Specifications

Grade K4169
Product Form Cast master alloy bar, round section
Diameter Range 8.0 mm to 200 mm
Melting Route Vacuum melting
Casting Route Bar casting
Grade Agreement Composition and impurity limits fixed before the cast
Lot Record Issued with the consignment, keyed to the grade and the lot number
Cut Length Made to the charging length used at the foundry
Internal Quality Uniform structure assessed where the order requires it
Surface Clean, consistent finish
Packing Rod bundles with protective wrapping, export wooden cases
Freight Terms Quoted to the destination port

Key Strengths

  • Cast to the grade agreed before the melt.
  • Lot record issued with every consignment.
  • Round bar from 8.0 mm to 200 mm, cut to the charging length.
  • Vacuum melting and bar casting on one site.
  • Repeat lots checked against the previous record.

Technical Details

The Lot Record That Travels with the Bar

A lot record is what makes the material checkable after it has left the works. It carries the grade and the lot number, the composition of the cast as it was agreed on the order, and the inspection results held against that cast. When the material reaches the foundry it can be put side by side with the purchase order, and when the finished casting is audited the record answers the question of what went into the heat.

Working to an Agreed Grade on Vacuum-Cast Lots

The order fixes the composition and the impurity limits first, and the cast is made against that agreement. Melting under vacuum is used for these lots, and the bar is cast from the same heat that was checked, so the material that arrives corresponds to the material that was released.

Data a Casting Engineer Asks For Before Charging

Before a new cast goes into the furnace, the engineer wants the grade confirmation, the composition of the lot, the section and the cut length, and the mass of the pieces to be charged. Those items come from the lot record and from the order, which is why the diameter and the cut length are settled at the enquiry stage instead of after the material arrives.

Repeat Lots and What Stays Constant

A casting programme runs on repeats, so a lot ordered this quarter is compared with the lot ordered last quarter. The grade agreement and the record format stay the same between runs, which keeps the incoming inspection routine unchanged and makes a difference stand out when one appears.

Aero and Precision Casting Programmes

Master alloy bar in K4169 is charged in investment casting operations for cast components that run at high temperature. Aero engine castings and the precision casting workshop sit at the centre of that field, alongside automotive turbocharger wheels, chemical pumps and valves, and glass manufacturing hardware.

铸造高温合金母合金棒材精密应用

铸造高温合金母合金棒材产品

Quality Assurance

Each lot is checked against the grade agreed before the cast, and the surface is inspected before packing. The record issued with the lot states the grade and the lot number, so the material can be traced from the consignment back to the cast, and a repeat order can be set against the previous record.

铸造高温合金母合金棒材属性

铸造高温合金母合金棒材应用领域

铸造高温合金母合金棒材对比

铸造高温合金母合金棒材工艺

References

Grade designations follow the cast grade series used for high-temperature alloys in the Chinese standard system. The figures that govern a casting programme are the agreed composition and impurity limits, the lot record issued with the consignment, and the inspection results held against that lot in the works.

Packaging & Delivery

Bar is supplied in rod bundles with protective wrapping and packed in export wooden cases, labelled with the grade, the diameter and the lot number. Production is scheduled over 15-30 days from order confirmation, and freight is quoted to the destination port named on the enquiry.

é“¸é€ é«˜æ¸©åˆé‡‘æ¯åˆé‡‘æ£’æä¾›åº”å Šé…é€

About DLX Alloy

Changzhou DLX Alloy Co., Ltd. has melted and processed alloys since 2002, holds ISO 9001 and SGS certification, and operates a 12,000 m² site with an annual capacity of 10,000 tons. Cast lots for aerospace and precision casting customers are handled the same way as the rest of the range: the grade is agreed before the melt, the cast is checked against that agreement, and the record is issued with the material.

Send the grade, the diameter, the cut length and the quantity for a quotation.

常州DLX合金

FAQ

  1. Q: What does an aero casting programme look for in a master alloy supplier?
    A: An agreed grade, a lot record issued with the material, and a cast that can be checked against that agreement. The geometry of the bar follows the charging practice in the foundry.
  2. Q: Which records are issued with a lot?
    A: A mill test certificate stating the composition of the lot and keyed to the grade and the lot number, with the packing list and the export documents for the destination.
  3. Q: How is the grade agreed before the cast?
    A: The composition and the impurity limits are fixed on the order, and the cast is checked against them before the material is released.
  4. Q: Which diameter and cut length suit a casting shop?
    A: Round bar from 8.0 mm to 200 mm, cut to the charging length used in the foundry, whether that is a full bar or a shorter piece sized for the crucible.
  5. Q: How is a repeat lot kept consistent with the previous one?
    A: The lot record is retained, and a repeat order is set against it so the grade and the limits stay as agreed.
  6. Q: What is the minimum order quantity?
    A: The minimum is set by the diameter and the quantity required, and is confirmed together with the grade when the order is placed.
  7. Q: What is the delivery time?
    A: Production is scheduled over 15-30 days from order confirmation.
  8. Q: How is the bar packed for shipment?
    A: Each bundle is wrapped and cased for the sea leg, and the cases carry the grade, the diameter and the lot number so the consignment can be checked on arrival.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Seller

  • Year Established:

    2002

  • Total Annual:

    1000000-120000000+

  • Employee Number:

    100~150

  • Ecer Certification:

    Verified Supplier

Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...

+ Read More

Get in touch with us

  • Reach Us
  • Changzhou DLX Alloy Co., Ltd.
  • NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
  • https://www.ecer.com/corp/uuufb21-dlx-alloy245.html

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement