China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners

  1. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  2. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  3. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  4. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  5. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  6. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners
  7. China High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners

High-Strength Superalloy Wire GH3044 Dia 0.5-6.0mm for High Temp Fasteners

  1. MOQ:
  2. Price:
  3. Get Latest Price

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

High Light GH3044 superalloy wire 0.5-6.0mm ,high temp nickel alloy wire ,superalloy wire for fasteners

Solid-solution strengthened GH3044 nickel-chromium superalloy wire engineered for critical high-temperature fasteners, aerospace structural components, and high-heat springs. Manufactured through high-purity vacuum metallurgy and multi-pass precision drawing for superior thermal stability and fatigue strength.

high temperature fastener wire Customized service available

Product Overview

The high-temperature fastening sector demands raw materials with flawless surface quality, uniform chemical distribution, and consistent mechanical response across fluctuating thermal gradients. GH3044 superalloy wire delivers an optimal combination of high thermal creep strength and environmental resistance up to 900°C in structural loading, while maintaining oxidation resilience up to 1200°C.

Through strict Vacuum Induction Melting (VIM) followed by Electroslag Remelting (ESR), our manufacturing process minimizes trace harmful impurities, controls gas content to ultra-low levels, and eliminates segregation. Multi-stage precision drawing combined with intermediate protective-atmosphere annealing yields high dimensional precision across the 0.5mm to 6.0mm diameter range, ensuring excellent formability and extended tool life during fastener manufacturing.

high temperature fastener wire details

Technical Specifications
Chemical Composition (Weight %)
Element Content (%)
Carbon (C) ≤ 0.10
Chromium (Cr) 23.50 – 26.50
Tungsten (W) 13.00 – 16.00
Molybdenum (Mo) ≤ 1.50
Iron (Fe) ≤ 4.00
Manganese (Mn) ≤ 0.50
Silicon (Si) ≤ 0.60
Phosphorus (P) ≤ 0.013
Sulfur (S) ≤ 0.013
Nickel (Ni) Balance
Physical & Thermal Properties
Property Typical Value
Density 8.89 g/cm³
Melting Range 1350 – 1400 °C
Coefficient of Thermal Expansion (20–800°C) 14.8 × 10⁻⁶ / K
Thermal Conductivity (800°C) ~ 24.5 W/(m·K)
Maximum Continuous Working Temperature Up to 1200 °C (Oxidation Resistance)
Continuous Structural Service Temperature Up to 900 °C
Mechanical Properties & Dimensional Availability
Parameter Hard / Spring Temper Solution Annealed State
Diameter Range 0.50 mm – 6.00 mm 0.50 mm – 6.00 mm
Diameter Tolerance High Precision Class (±0.008 mm to ±0.025 mm) High Precision Class (±0.010 mm to ±0.030 mm)
Tensile Strength (Rm) 950 – 1350 MPa 700 – 900 MPa
Elongation (A5) ≥ 10 % ≥ 30 %
Surface Finish Bright Drawn / Polished / Centerless Ground Bright Annealed / Pickled
Key Characteristics of High-Strength GH3044 Superalloy Wire
  • High-Temperature Oxidation & Carburization Resistance: With a high chromium (23.5–26.5%) and tungsten (13–16%) matrix, GH3044 forms a dense, self-healing protective oxide scale, preventing degradation in aggressive oxidizing and combustion atmospheres.
  • Superior High-Temperature Creep & Rupture Strength: Tungsten solid solution strengthening provides robust microstructural stability, resisting relaxation and thermal creep when fasteners are subjected to intense mechanical stress at elevated temperatures.
  • Precision Dimensional Accuracy for Fastener Tooling: Multi-die continuous drawing achieves tight diameter tolerances and consistent ovality, maximizing die life during high-speed cold heading and thread rolling.
  • Uniform Grain Structure & Defect-Free Surface: 100% eddy current testing and micro-cleanliness screening ensure absence of seams, slivers, scratches, or central piping, ensuring crack-free heading and cold forming.
  • Excellent Cold Heading and Machinability: Balanced work-hardening rate allows seamless upsetting, thread rolling, and machining into intricate bolt and screw geometries without premature failure.

high temperature fastener wire comparison

Industrial Applications
  • Aerospace & Turbine Structural Fasteners: Engine casing bolts, flange studs, high-temperature lockwires, turbine shroud pins, and thermal shield fasteners.
  • Industrial Furnace & Kiln Fixtures: Heat-treatment furnace conveyor links, high-temperature tie rods, threaded hangers, and structural pins operating above 800°C.
  • Petrochemical & Thermal Processing Equipment: Reactor vessel clamping bolts, high-pressure pyrolysis tube fasteners, and heat exchanger structural supports.
  • High-Heat Spring & Retaining Rings: Heavy-duty thermal compression springs, retaining clips, and elastic sealing components under continuous heat loads.
  • Exhaust & Turbocharger Assemblies: Automotive and marine turbocharger studs, exhaust manifold hardware, and sensor mounting fasteners.

high temperature fastener wire application field

Why Choose Changzhou DLX Alloy for Superalloy Wire Sourcing
  • Integrated Vacuum Metallurgy & Processing: From high-purity VIM+ESR melting, hot forging, and multi-pass precision drawing to continuous protective atmosphere annealing, we control every metallurgical phase in-house.
  • Robust Supply Capability: With a stable production capacity of 1,200 tons/month, we ensure scalable output, reliable lead times, and seamless batch-to-batch consistency for large-scale fastener manufacturers and global distributors.
  • Stringent Quality Verification: Every batch undergoes comprehensive spectrometer chemical verification, full-range tensile testing, high-temperature stress rupture analysis, eddy current surface testing, and metallographic grain size evaluation with full material test certificates.
  • Tailored Packaging & Dynamic Commercial Flexibility: Available in precision layer-wound spools, continuous carrier coils, or cut-to-length straight rods. MOQ is dynamically configured based on diameter and temper requirements to support specialized trial batches and volume production.

production plant

our certifications

Frequently Asked Questions
Q1: What makes GH3044 wire preferred over standard stainless steel wires for fasteners?

A: Standard stainless steels suffer severe oxidation, grain coarsening, and rapid loss of yield strength above 600°C. GH3044 is fortified with 13–16% tungsten and 23.5–26.5% chromium in a nickel matrix, retaining structural rigidity, creep resistance, and oxidation resistance up to 900–1200°C.

Q2: Can GH3044 wire be directly cold-headed into bolts and rivets?

A: Yes. In the annealed condition, GH3044 exhibits sufficient ductility (elongation ≥30%) for cold heading and thread rolling. For extreme head upset ratios, warm heading or intermediate induction annealing can be incorporated into your production flow.

Q3: What surface finishes and packaging options are available for Dia 0.5–6.0mm wire?

A: We provide bright drawn, polished, or centerless ground finishes. Packaging options include precision plastic spools (DIN160/DIN200/DIN250) for fine diameters, continuous steel-frame carrier coils for automated cold-headers, and straight-cut rods packed in reinforced wooden cases.

Q4: How do you verify and ensure the internal cleanliness of GH3044 wire?

A: We utilize dual-vacuum melting (VIM + ESR) and conduct inline continuous eddy current testing along with ultrasonic inspection on the master billet stage. Every production heat is fully analyzed for chemical composition, non-metallic inclusions, and mechanical integrity.

Q5: What is the typical Minimum Order Quantity (MOQ) and lead time?

A: Our MOQ is dynamically aligned with your required diameter and surface temper. Standard sizes with ongoing production cycles feature short dispatch cycles, while customized diameters and specialized packaging are scheduled with flexible volume requirements.

high temperature fastener wire testing equipment

OEM services

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Seller

  • Year Established:

    2002

  • Total Annual:

    1000000-120000000+

  • Employee Number:

    100~150

  • Ecer Certification:

    Verified Supplier

Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ... Changzhou DLX Alloy Co., Ltd. was established in 2002 and has passed ISO9001 international quality management system certification and SGS certification.We initially focused on the production of resistance alloys. Over the past 20 years, we have continued to conduct research and development and now ...

+ Read More

Get in touch with us

  • Reach Us
  • Changzhou DLX Alloy Co., Ltd.
  • NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu
  • https://www.ecer.com/corp/uuufb21-dlx-alloy245.html

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement