| Type | Potassium Chloride Zinc Brightener |
| Cathode Current Density | 1-5 A/dm² |
| Packaging Details | 25kg/drum |
| pH Value | 4.8–5.8 |
| Payment Terms | T/T |
| Features | Rack & Barrel Compatible |
| Delivery Time | 5-8 work day |
| Potassium Chloride | 180–240 g/L |
| Operating Temperature | 10–60 ℃ |
| Model Number | DS-418 |
| Place of Origin | China |
View Detail Information
Explore similar products
R·G-2008 Alkaline Zinc Plating Process For Auto Fasteners Furniture Hardware
Cyanide Free Alkaline Zinc Plating Process High Concentration Good Dispersion
R·G-2004 Alkaline Zinc Plating Process Cyanide Free For Furniture Hardware
LAN-918 Potassium Chloride Rapid Galvanizing Brightener High Corrosion
Product Specification
| Type | Potassium Chloride Zinc Brightener | Cathode Current Density | 1-5 A/dm² |
| Packaging Details | 25kg/drum | pH Value | 4.8–5.8 |
| Payment Terms | T/T | Features | Rack & Barrel Compatible |
| Delivery Time | 5-8 work day | Potassium Chloride | 180–240 g/L |
| Operating Temperature | 10–60 ℃ | Model Number | DS-418 |
| Place of Origin | China | ||
| High Light | Potassium Chloride Zinc Plating Brightener ,Rack Zinc Plating Brightener ,Barrel Zinc Plating Brightener | ||
| Item | Rack Plating | Barrel Plating |
|---|---|---|
| Potassium Chloride | 180–240 g/L | 180–240 g/L |
| Zinc Chloride | 60–80 g/L | 40–60 g/L |
| Boric Acid | 25–30 g/L | 30 g/L |
| DS 418A Brightener | 0.3–1.5 mL/L | 0.3–1.5 mL/L |
| DS 418B Softener | 20–30 mL/L | 20–30 mL/L |
| pH Value | 4.8–5.8 | 4.8–5.8 |
| Current Density | 1–6 A/dm² | 0.1–3 A/dm² |
| Operating Temperature | 10–60 ℃ | 10–60 ℃ |
Maintenance and Management of Tank Liquid
When the impurities exceed a certain limit, the high current parts become dull or perforated, and the low current parts turn white and cannot be coated. The coating is rough. At this time, only 0.5mLA hydrogen peroxide (30%) needs to be added, followed by 1-2g/L zinc powder and activated carbon. After thorough stirring, let it settle and then remove the cylinder foot to restore normal operation. You can also use the WZN acidic impurity remover from Aobang Company: 1-2g/L, which can be circulated and filtered in the filter machine, and the effect is good! No need to clean the cylinder.
Consumption:
After the plating solution treatment, it is recommended to add 1/5 of the opening amount of brightener and softener.
DS418A Brightener 80~120mL/KAH
DS418B Softener 80~120mL/KAH
process flow
Chemical degreasing, acid washing, weak acid etching, galvanizing, polishing, passivation, hot water sealing, drying, and final product.
Company Details
Business Type:
Manufacturer
Year Established:
2002
Employee Number:
>2000
Ecer Certification:
Verified Supplier
Overview of Aobang Established in 2002, the company comprises: Wuhan AoBang Surface Technology Co., Ltd. Wuhan AoHua Surface Engineering Co., Ltd. Lane (International) Chemicals Co., Ltd. Jerry's (International) Surface Technology Co., Ltd. Omex New Materials Co., Ltd. AoBang Surface Technology R... Overview of Aobang Established in 2002, the company comprises: Wuhan AoBang Surface Technology Co., Ltd. Wuhan AoHua Surface Engineering Co., Ltd. Lane (International) Chemicals Co., Ltd. Jerry's (International) Surface Technology Co., Ltd. Omex New Materials Co., Ltd. AoBang Surface Technology R...