| Payment Terms | L/C, D/A, D/P, T/T, Western Union, MoneyGram |
| Supply Ability | 500 Set/Sets per Month |
| Delivery Time | 5-8WORK DAY |
| Packaging Details | Wooden box |
| Working power supply | AC220V 50Hz/60Hz |
| DSC range | 0~±500mW |
| Temperature range | -150~500°C |
| Heating rate | 0.1~50°C/min |
| Cooling rate | 0.1~10°C/min |
| Brand Name | BAXIT |
| Model Number | GLO-AD09 |
| Place of Origin | CHINA |
View Detail Information
Explore similar products
Programmable Industrial MRO Products , DSC Differential Scanning Calorimetry
Laboratory DSC Differential Scanning Calorimeter
150 Degrees Warming Scan DSC Thermal Analysis Machine
Lab DSC Differential Scanning Calorimeter 600C 0.001mW
Product Specification
| Payment Terms | L/C, D/A, D/P, T/T, Western Union, MoneyGram | Supply Ability | 500 Set/Sets per Month |
| Delivery Time | 5-8WORK DAY | Packaging Details | Wooden box |
| Working power supply | AC220V 50Hz/60Hz | DSC range | 0~±500mW |
| Temperature range | -150~500°C | Heating rate | 0.1~50°C/min |
| Cooling rate | 0.1~10°C/min | Brand Name | BAXIT |
| Model Number | GLO-AD09 | Place of Origin | CHINA |
| High Light | DSC Differential Scanning Calorimeter ,Cold Crystallization Differential Scanning Calorimeter ,AC220V Differential Scanning Calorimeter | ||
TOP1 High-quality DSC analyzer differential scanning calorimeter thermal analyzer by Glomro
QUICK DETAILS
DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).
APPLICATION
Measure heat related physical and chemical changes such as glass transition temperature and melting point. Melting temperature, crystallization and crystallization heat, phase transition reaction heat, product thermal stability, curing/crosslinking, oxidation induction period, reaction kinetics, specific heat, etc.
ADVANTAGES
1, Widescreen touch structure of industrial level, rich display information, including the set temperature, sample temperature, oxygen flow rate,Nitrogen flow, differential thermal signals, all kinds of switch state, flow goes to zero.
2, By controlling the flow of liquid nitrogen to achieve linear cooling, the instrument can linearly cool to minus 150 degrees.
3, USB communication interface, generality is strong, reliable communication don't interrupt, support the restore connection function.
4, the furnace body structure is compact, the heating and cooling rate can be arbitrarily adjustable, can achieve linear cooling and linear heating function. Meet GB/T 22567-2008
5, Improved installation process, all adopt the machinery fixed way, completely to avoid contamination of furnace inside colloid to differential thermal signal.
6. High-precision imported dual temperature sensor ensures high repeatability of sample temperature measurement.
7. The digital gas mass flowmeter automatically switches two air flow rates, with fast switching speed and short settling time.
8, standard standard sample, to facilitate the customer to calibrate the temperature coefficient.
9, software adaptive resolution of the computer screen; support notebooks, desktops, support WIN2000, XP, WIN7, WIN8, WIN10 and other operating systems.
10, support for user self-programming program, to achieve full automation of the measurement process. The software provides dozens of instructions. The user can flexibly combine the instructions according to their own measurement procedures and save them. Complex operations are simplified into one-click operation.
![]()
![]()
![]()
Technical Parameter
| DSC range: | 0~±500mW |
| Temperature range: | -150~500°C |
| Heating rate: | 0.1~50°C/min |
| Cooling rate: | 0.1~10°C/min |
| Temperature Resolution: | 0.01°C |
| Temperature accuracy: | ±0.1°C |
| Temperature repeatability: | ±0.1°C |
| DSC Accuracy: | ±1% |
| DSC Resolution: | 0.1uW |
| Temperature control mode: | Temperature increase, constant temperature, cooling, cycle temperature control (full program automatic control) |
| Curve Scan: | Warming Scan |
| Atmosphere control: | Gas mass flowmeter automatically switches two gases |
| Display mode: | 24bit color, 7-inch LED touch screen display |
| Data Interface: | USB standard interface, supporting the corresponding operating software |
| Parameter Standards: | With standard calibrators, with one-key calibration function, users can calibrate their own temperature |
| Working power supply: | AC220V 50Hz/60Hz |
2. The package will be shipped by DHL/Fedex/TNT/EMS/UPS/China post/EF-Express/Special line, as you have chose in the order.
![]()
Our Services
If you encounter with any problems during the testing process,we promise providing urgent guidence and after-sales sevice within 48 hours and solution providing within 3 working days. If customers require on-site service, the transport and travel expense shall be responsible for the cost.
1. Pre-service
24 Hours online service for customers' consultation.
2. Middle service
-- Fullfill customer's request:
-- Payment method depends on customer.
-- Promptly production and delivery
-- Can provide invoice value if you want to decrease your tax.
3. After sale service
-- One year warranty service and all life maintenance.
-- Technical Egineer are avalible for oversea trainning.
-- Remote control technical consult
Company Details
Business Type:
Manufacturer,Exporter,Trading Company,Seller,Other
Year Established:
2012
Total Annual:
10,000,000-20,000,000
Employee Number:
100~150
Ecer Certification:
Verified Supplier
Shanghai Glomro Industrial Co., Ltd was founded in 2012. Specializing in the production of thermal analysis machine, laboratory instrument, analytical instrument, testing equipment, industrial measurements and instruments products. Products of high quality, fashiona... Shanghai Glomro Industrial Co., Ltd was founded in 2012. Specializing in the production of thermal analysis machine, laboratory instrument, analytical instrument, testing equipment, industrial measurements and instruments products. Products of high quality, fashiona...
Get in touch with us