| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
| Packaging Details | Standard export packaging, or packaging as required |
| Density | ~8.9 g/cm³ (0.321 lb/in³) |
| Melting Point | ~1350-1450°C (2460-2640°F) |
| Tensile Strength | ~850 MPa (123 ksi) |
| Yield Strength | ~700 MPa (102 ksi) |
| Elongation | ~15% |
| Thermal Conductivity | ~14 W/m·K (8.4 BTU·in/hr·ft²·°F) |
| Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
| Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures |
| Applications | Aerospace, gas turbines, and high-temperature structural components |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH36 Alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Inconel 600 Alloy High Temperature Nickel Chromium Alloy Oxidation Resistant
Chemical Processing Nickel Based Alloys 30 Sheets / Plates / Bars UNS N08031
High Strength Nickel Chromium Molybdenum Alloy 59 UNS N06059
GH136 Alloy is a nickel-based superalloy with high strength and excellent
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Density | ~8.9 g/cm³ (0.321 lb/in³) | Melting Point | ~1350-1450°C (2460-2640°F) |
| Tensile Strength | ~850 MPa (123 ksi) | Yield Strength | ~700 MPa (102 ksi) |
| Elongation | ~15% | Thermal Conductivity | ~14 W/m·K (8.4 BTU·in/hr·ft²·°F) |
| Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) | Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures |
| Applications | Aerospace, gas turbines, and high-temperature structural components | Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH36 Alloy | Place of Origin | China |
| Certification | ISO Certificate | ||
| High Light | high strength nickel based alloys ,high strength nickel based superalloy | ||
GH36 Alloy is a high-performance nickel-based superalloy renowned for its exceptional mechanical properties and resistance to high-temperature environments. It is specifically designed to offer high strength and durability in demanding applications such as aerospace and industrial machinery.
Key Properties and Features:
High-Temperature Strength: GH36 Alloy maintains robust mechanical properties, including high tensile strength (~850 MPa or 123 ksi) and yield strength (~700 MPa or 102 ksi), at elevated temperatures up to approximately 1350-1450°C (2460-2640°F). This makes it suitable for components subjected to intense thermal stresses.
Oxidation and Corrosion Resistance: The alloy is highly resistant to oxidation and high-temperature corrosion, ensuring longevity and performance in harsh environments. This property is crucial for applications in gas turbines, jet engines, and other high-temperature systems where resistance to oxidative degradation is essential.
Mechanical Properties: GH36 exhibits good elongation (~15%), contributing to its ability to withstand mechanical stresses and deformation without failure. This feature is important for structural integrity and reliability in critical applications.
Thermal Conductivity: With a thermal conductivity of approximately 14 W/m·K (10 BTU·in/hr·ft²·°F), GH36 efficiently manages heat dissipation, which is beneficial for maintaining thermal stability in high-performance applications.
Applications: Commonly used in aerospace components, high-temperature gas turbines, and other industrial applications where high strength, oxidation resistance, and thermal stability are required. GH36's combination of properties makes it a preferred choice for environments demanding exceptional performance and reliability.
GH36 Alloy's high strength and resistance to extreme conditions make it a trusted material for advanced engineering applications, providing durability and reliability in critical components exposed to severe environments.
Here’s a composition table for GH36 Alloy:
| Element | Composition Range (%) |
|---|---|
| Nickel (Ni) | 60.0 - 65.0 |
| Chromium (Cr) | 15.0 - 20.0 |
| Cobalt (Co) | 5.0 - 10.0 |
| Molybdenum (Mo) | 2.0 - 4.0 |
| Iron (Fe) | ≤ 6.0 |
| Titanium (Ti) | 1.0 - 2.0 |
| Aluminum (Al) | 1.0 - 2.0 |
| Carbon (C) | ≤ 0.10 |
| Manganese (Mn) | ≤ 0.5 |
| Silicon (Si) | ≤ 0.5 |
| Sulfur (S) | ≤ 0.01 |
These values provide general guidelines. For precise specifications or detailed applications, consult specific standards or suppliers.
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other
Year Established:
2022
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...
Get in touch with us
Leave a Message, we will call you back quickly!