| Density | ~8.3 g/cm³ |
| Melting Point | ~1390°C (2530°F) |
| Thermal Conductivity | ~11-12 W/m·K |
| Yield Strength | ~700 MPa (102 ksi) |
| ~700 MPa (102 ksi) | 900 MPa (130 ksi) |
| Elongation | ~10% |
| Hardness (Rockwell) | ~HRB 90-95 |
| Applications | Aerospace components, gas turbines, and high-temperature industrial parts |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH4145 alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Temperature Resistant Inconel 706 Nickel Based Alloys For Aerospace Components
High Strength Inconel 718 Rod Anti Deformation High Temperature Bolts / Nuts /
Good Weldability Nickel Based Alloys 625 UNS N06625 Customized Dimensions
Corrosion Resistant Nickel Based Alloy 926 For Extreme Industrial Environments
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Density | ~8.3 g/cm³ | Melting Point | ~1390°C (2530°F) |
| Thermal Conductivity | ~11-12 W/m·K | Yield Strength | ~700 MPa (102 ksi) |
| ~700 MPa (102 ksi) | 900 MPa (130 ksi) | Elongation | ~10% |
| Hardness (Rockwell) | ~HRB 90-95 | Applications | Aerospace components, gas turbines, and high-temperature industrial parts |
| Brand Name | Zhonggong Special Metallurgy | Model Number | GH4145 alloy |
| Place of Origin | China | Certification | ISO Certificate |
| High Light | aerospace components nickel based alloys ,aerospace components nickel based superalloy | ||
GH4145 Alloy
GH4145 is a high-performance nickel-based superalloy renowned for its exceptional strength, thermal stability, and resistance to oxidation and corrosion. It is designed for use in demanding high-temperature environments where reliability and durability are critical.
Key Features:
GH4145 alloy’s superior combination of strength, thermal resistance, and corrosion protection makes it an ideal material for critical applications that require reliable performance in challenging conditions.
Here’s a detailed composition table for GH4145 alloy:
| Element | Content Range |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 18.0-21.0% |
| Iron (Fe) | 14.0-17.0% |
| Cobalt (Co) | 8.0-10.0% |
| Molybdenum (Mo) | 2.0-3.0% |
| Titanium (Ti) | 1.5-2.5% |
| Aluminum (Al) | 1.0-1.5% |
| Boron (B) | 0.005-0.015% |
This table provides a clear overview of the chemical composition of GH4145 alloy, detailing the content ranges of its key elements.
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other
Year Established:
2022
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...
Get in touch with us
Leave a Message, we will call you back quickly!