| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
| Packaging Details | Standard export packaging, or packaging as required |
| Composition | Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements |
| Density | 8.23 g/cm³ |
| Melting Point | 1320-1370°C (2408-2498°F) |
| Tensile Strength | 850-1100 MPa (at room temperature) |
| Yield Strength (0.2% offset) | 450-700 MPa |
| Elongation | 30-50% |
| Thermal Conductivity | 9.8 W/m·K (at 100°C) |
| Specific Heat Capacity | Specific Heat Capacity |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.10 µΩ·m (at 20°C) |
| Magnetic Properties | Non-magnetic |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH3039 alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
High Strength Inconel 230 Alloy Chromium Cobalt Nickel Alloy 8.4g/cm3
Food Processing Nickel Based Superalloy 28 Sanicro 28 Corrosion Resistance
GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation
GH5188 Alloy High Strength Nickel Based Superalloy With Excellent Oxidation
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Composition | Nickel-based superalloy containing Chromium, Cobalt, Iron, and other elements | Density | 8.23 g/cm³ |
| Melting Point | 1320-1370°C (2408-2498°F) | Tensile Strength | 850-1100 MPa (at room temperature) |
| Yield Strength (0.2% offset) | 450-700 MPa | Elongation | 30-50% |
| Thermal Conductivity | 9.8 W/m·K (at 100°C) | Specific Heat Capacity | Specific Heat Capacity |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) | Electrical Resistivity | 1.10 µΩ·m (at 20°C) |
| Magnetic Properties | Non-magnetic | Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH3039 alloy | Place of Origin | China |
| Certification | ISO Certificate | ||
| High Light | Gh3039 nickel based superalloy ,High Strength nickel based superalloy ,Corrosion Resistant nickel based superalloy | ||
GH3039 alloy, a high-performance nickel-based superalloy, excels in demanding environments due to its exceptional mechanical strength, oxidation resistance, and corrosion resistance. Composed primarily of nickel, chromium, cobalt, and iron, GH3039 maintains its integrity and reliability at temperatures up to approximately 1370°C (2498°F). It offers excellent creep and fatigue resistance, crucial for applications in gas turbines, aerospace components, and chemical processing equipment where prolonged exposure to high temperatures and aggressive environments is common. GH3039 alloy's non-magnetic properties and ability to maintain strength over extended service life make it a preferred choice for critical industrial applications requiring high performance and reliability under extreme conditions.
Here's a detailed composition table for GH3039 alloy:
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 51.0 - 55.0 |
| Chromium (Cr) | 19.0 - 22.0 |
| Cobalt (Co) | 15.0 - 20.0 |
| Iron (Fe) | 5.0 - 9.0 |
| Molybdenum (Mo) | 2.5 - 3.5 |
| Titanium (Ti) | ≤ 0.70 |
| Aluminum (Al) | ≤ 0.60 |
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 0.50 |
| Silicon (Si) | ≤ 0.50 |
| Phosphorus (P) | ≤ 0.015 |
| Sulfur (S) | ≤ 0.010 |
| Boron (B) | ≤ 0.006 |
GH3039 alloy is primarily composed of nickel, chromium, cobalt, and iron, with minor additions of molybdenum, titanium, aluminum, and trace elements to achieve its desired properties for high-temperature and corrosion-resistant applications.
![]()
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other
Year Established:
2022
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...
Get in touch with us
Leave a Message, we will call you back quickly!