| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
| Packaging Details | Standard export packaging, or packaging as required |
| Composition | Nickel-based superalloy containing Chromium, Iron, and Nickel |
| Density | 8.08 g/cm³ |
| Melting Point | 1370-1425°C (2498-2597°F) |
| Yield Strength (0.2% offset) | 700-900 MPa (at room temperature) |
| Elongation | 45-55% |
| Thermal Conductivity | 11.6 W/m·K (at 100°C) |
| Specific Heat Capacity | 424 J/kg·K (at 20°C) |
| Coefficient of Thermal Expansion | 12.2 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.15 µΩ·m (at 20°C) |
| 1.15 µΩ·m (at 20°C) | Non-magnetic |
| Hardness | HRB 95 (max) |
| Applications | Gas turbine components, aerospace components, high-temperature applications |
| Brand Name | Zhonggong Special Metallurgy |
| Model Number | GH3030 alloy |
| Place of Origin | China |
| Certification | ISO Certificate |
View Detail Information
Explore similar products
Temperature Resistant Inconel 706 Nickel Based Alloys For Aerospace Components
High Strength Inconel 718 Rod Anti Deformation High Temperature Bolts / Nuts /
Good Weldability Nickel Based Alloys 625 UNS N06625 Customized Dimensions
Corrosion Resistant Nickel Based Alloy 926 For Extreme Industrial Environments
Product Specification
| Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
| Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
| Composition | Nickel-based superalloy containing Chromium, Iron, and Nickel | Density | 8.08 g/cm³ |
| Melting Point | 1370-1425°C (2498-2597°F) | Yield Strength (0.2% offset) | 700-900 MPa (at room temperature) |
| Elongation | 45-55% | Thermal Conductivity | 11.6 W/m·K (at 100°C) |
| Specific Heat Capacity | 424 J/kg·K (at 20°C) | Coefficient of Thermal Expansion | 12.2 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.15 µΩ·m (at 20°C) | 1.15 µΩ·m (at 20°C) | Non-magnetic |
| Hardness | HRB 95 (max) | Applications | Gas turbine components, aerospace components, high-temperature applications |
| Brand Name | Zhonggong Special Metallurgy | Model Number | GH3030 alloy |
| Place of Origin | China | Certification | ISO Certificate |
| High Light | temperature resistant nickel based alloys ,temperature resistant nickel based superalloy ,aerospace components nickel based alloys | ||
GH3030 alloy, also known as Inconel Alloy 718, is a nickel-based superalloy renowned for its exceptional combination of high-temperature strength, corrosion resistance, and oxidation resistance. It is widely used in various industries where reliability under extreme conditions is paramount.
Key Features:
High-Temperature Strength: GH3030 retains significant mechanical strength at elevated temperatures up to approximately 700°C (1300°F), making it suitable for applications in gas turbines, aerospace components, and high-temperature industrial environments.
Corrosion and Oxidation Resistance: The alloy exhibits excellent resistance to corrosion and oxidation in a wide range of aggressive environments, including aqueous and high-temperature gases.
Chemical Composition: GH3030 is composed primarily of nickel (about 52%), chromium (20-24%), iron (5-15%), and smaller amounts of niobium, titanium, and aluminum. This composition contributes to its superior mechanical and thermal properties.
Mechanical Properties: It offers high tensile and yield strength, with good ductility and toughness even after prolonged exposure to high temperatures.
Applications: Common applications include components for gas turbines, jet engines, aerospace parts, industrial furnaces, and high-temperature chemical processing equipment.
Processing and Fabrication: GH3030 can be processed using conventional methods such as forging, machining, and welding. Its weldability and formability allow for versatile manufacturing capabilities.
Non-Magnetic Properties: GH3030 is non-magnetic in the annealed condition, making it suitable for applications where magnetic interference must be minimized.
GH3030 alloy is recognized for its reliability and performance in demanding environments, offering a balance of strength, resistance to environmental degradation, and ease of fabrication that meets the stringent requirements of high-performance industries.
Here's a typical composition table for GH3030 alloy (Inconel Alloy 718):
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 19.0 - 21.0 |
| Iron (Fe) | 18.5 - 20.0 |
| Niobium (Nb) | 5.0 - 5.5 |
| Molybdenum (Mo) | 2.8 - 3.3 |
| Titanium (Ti) | 0.65 - 1.15 |
| Aluminum (Al) | 0.2 - 0.8 |
| Cobalt (Co) | ≤ 1.0 |
| Manganese (Mn) | ≤ 0.35 |
| Silicon (Si) | ≤ 0.35 |
| Copper (Cu) | ≤ 0.30 |
| Carbon (C) | ≤ 0.08 |
| Sulfur (S) | ≤ 0.015 |
| Phosphorus (P) | ≤ 0.015 |
This composition table outlines the typical ranges of key elements present in GH3030 alloy (Inconel Alloy 718), providing insight into its chemical makeup essential for its high-temperature strength and corrosion resistance properties.
![]()
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other
Year Established:
2022
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Active Member
Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...