China factories

Chat Now Send Email
China factory - Jiangyin Chengxin Alloy Material Co., Ltd ,

Jiangyin Chengxin Alloy Material Co., Ltd ,

  • China,Changzhou ,Jiangsu
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal
China Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal

  1. China Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal
  2. China Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal
  3. China Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal

Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal

  1. MOQ: TBD
  2. Price:
  3. Get Latest Price
Payment Terms T/T,D/P
Supply Ability 30 Tons per day
Delivery Time 7 days
Packaging Details Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Place of Orig China
Name Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375
Density 8.89 g/cm³
Melting range 1288-1343 ℃
Tensile strength Rm N/mm² 1100
Yield strength RP0.2 N/mm² 790
Elongation A5 % 20
Brand Name Senphus
Model Number Monel K500/UNS N05500/2.4375
Certification ISO9001
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T,D/P Supply Ability 30 Tons per day
Delivery Time 7 days Packaging Details Packed with waterproof paper or weave bag, into pallets or wooden case. Special packaging requirements can also be accommodated.
Place of Orig China Name Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375
Density 8.89 g/cm³ Melting range 1288-1343 ℃
Tensile strength Rm N/mm² 1100 Yield strength RP0.2 N/mm² 790
Elongation A5 % 20 Brand Name Senphus
Model Number Monel K500/UNS N05500/2.4375 Certification ISO9001
Place of Origin China
High Light Non-Magnetic Monel K500Non-Magnetic UNS N05500Non-Magnetic 2.4375

Monel K500 Bar/Rod/Wire/Forging/Plate/Strip UNS N05500 2.4375 Non-Magnetic Ideal for Stress Corrosion Cracking and High-Stress Applications


Monel K500 wire (UNS N05500, W.Nr. 2.4375) is a nickel-copper alloy with enhanced strength and hardness due to aluminum and titanium additions. It offers excellent corrosion resistance, particularly in marine and chemical environments, while maintaining superior mechanical properties at high temperatures. The alloy is precipitation-hardened, improving yield and tensile strength over Monel 400.

Monel K500 is available in various forms, including bar, rod, wire, forging, plate, and strip, making it suitable for marine engineering, oil and gas, aerospace, and chemical processing. It resists chloride-induced stress corrosion cracking and retains ductility even in cryogenic conditions. Common applications include pump shafts, valve components, springs, and fasteners. It is widely used where strength and corrosion resistance are critical.


Trade Code

GB ASTM W-Nr.

NS 6500
Ni68Cu28Al

H 05500

N 05500

Monel K500

2.4375


Chemical Composition Wt.% % Ni Cu Fe C Mn Si S Al Ti
Min 63 27           2.3 0.35
Max   33 2 0.25 1.5 0.5 0.01 3.15 0.85


Physical Constants Density(g/cm³) 8.89
Melting Range(℃) 1288-1343


Minimum mechanical properties of alloy at room temperature Typical mechanical properties Tensile strength Rm N/mm² Yield strength RP 0.2 N/mm² Elongation A5 %
Annealing treatment 1100 790 20


Monel K500 (UNS N05500 / 2.4375) is a high-performance nickel-copper alloy with added aluminum and titanium, known for its excellent corrosion resistance, high strength, and good mechanical properties in extreme environments. Here are its key features:

Key Features of Monel K500 wire

  1. High Strength & Hardness

    • Precipitation-hardened for increased mechanical strength

    • Retains strength at high temperatures

  2. Excellent Corrosion Resistance

    • Resistant to seawater, acids, and harsh chemicals

    • Superior resistance to stress corrosion cracking and pitting

    • Performs well in both fresh and saltwater environments

  3. Good Thermal & Cryogenic Performance

    • Retains toughness down to subzero temperatures

    • Can be used in marine and cryogenic applications

  4. Non-Magnetic in the Annealed Condition

    • Becomes slightly magnetic after precipitation hardening

  5. Wear & Erosion Resistance

    • High resistance to cavitation and erosion in turbulent flow conditions

  6. Good Workability & Weldability

    • Can be machined, welded, and fabricated using standard techniques


Monel K500 (UNS N05500, 2.4375) is a nickel-copper alloy known for its excellent corrosion resistance, high strength, and good mechanical properties at elevated temperatures. Below are its common applications based on different forms:

1. Bar/Rod/Wire Applications

  • Marine Industry: Used in propeller shafts, fasteners, and pump shafts due to its excellent corrosion resistance in seawater.

  • Aerospace Components: Employed in landing gear components and springs due to its high strength and fatigue resistance.

  • Oil & Gas Industry: Used in drill collars, valve stems, and downhole components due to its resistance to sour gas environments (H₂S).

  • Chemical Processing: Applied in heat exchangers, pump shafts, and agitators for handling acidic and alkaline environments.

2. Forging Applications

  • Pump and Valve Components: Used in pump impellers, valve seats, and casings for seawater and chemical environments.

  • High-Stress Fasteners: Suitable for bolts, nuts, and studs in extreme marine and aerospace conditions.

  • Bearings and Gears: Preferred for high-strength, corrosion-resistant gears and bearings in harsh environments.

3. Plate/Strip Applications

  • Shipbuilding: Used in hull reinforcements and bulkhead linings for corrosion protection.

  • Heat Exchangers & Pressure Vessels: Ideal for plates in heat exchangers exposed to aggressive chemicals.

  • Aerospace Structural Components: Applied in fuel tanks, structural reinforcements, and exhaust systems.

4. General Applications Across All Forms

  • Marine and Offshore Engineering (submarine parts, cable sheathing)

  • Petrochemical and Refining Equipment

  • Medical and Pharmaceutical Processing Equipment

  • Power Generation (turbine blades, nuclear reactor components)


Monel® K500 is a precipitation-hardened nickel-copper alloy known for its exceptional strength, corrosion resistance, and excellent performance in marine and chemical environments. Due to its added aluminum and titanium content, Monel K500 offers higher mechanical strength and hardness compared to Monel 400, while maintaining resistance to seawater, acids, and alkalis.

Many buyers are interested in the current Monel K500 price or Monel K500 price per kg when sourcing materials for high-performance applications. Pricing depends on factors such as size, form (bar, sheet, pipe, etc.), and order volume. To ensure material quality and traceability, it’s important to work with experienced Monel K 500 suppliers who can provide certified products and timely delivery.

Whether for aerospace fasteners, marine shafts, pump parts, or chemical processing components, Monel K500 remains a top choice for applications requiring strength under pressure and resistance to corrosion in aggressive environments.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Exporter,Seller

  • Year Established:

    2003

  • Total Annual:

    230000000-240000000

  • Employee Number:

    1400~1500

  • Ecer Certification:

    Verified Supplier

Company Overview: Jiangyin Chengxin Alloy Material Co., Ltd has more than 20 years of experience as the lead.ing alloy wire manufacturer in China. We offer a wide range of services from fine wire drawing toresistance wire manufacturing. Since the beginning, our specialty has been the quality and pre... Company Overview: Jiangyin Chengxin Alloy Material Co., Ltd has more than 20 years of experience as the lead.ing alloy wire manufacturer in China. We offer a wide range of services from fine wire drawing toresistance wire manufacturing. Since the beginning, our specialty has been the quality and pre...

+ Read More

Get in touch with us

  • Reach Us
  • Jiangyin Chengxin Alloy Material Co., Ltd ,
  • Building 3, No. 29, Beitanghe East Road, Qinglong Street, Tianning District, Changzhou City, Jiangsu Province
  • https://www.heatingalloywire.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement