China Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability
China Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability

  1. China Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability
  2. China Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability
  3. China Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability

Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability

  1. MOQ: 1 piece
  2. Price: USD20-USD200,000
  3. Get Latest Price
Application Aircraft engine part
Supply Ability Upon Order
Industry Turbine
Grade 214
Usage Seal
Delivery Time in one month
Material Haynes 214
Method brazing
Packaging Details plywood crates
Advantage Very low cross coupling
Process Vacuum Brazed
Model Number VBHSTT
Place of Origin China
Certification ISO9001
Brand Name PASIA

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Application Aircraft engine part Supply Ability Upon Order
Industry Turbine Grade 214
Usage Seal Delivery Time in one month
Material Haynes 214 Method brazing
Packaging Details plywood crates Advantage Very low cross coupling
Process Vacuum Brazed Model Number VBHSTT
Place of Origin China Certification ISO9001
Brand Name PASIA

Vacuum Brazed Nickel Superalloy Honeycomb Seal with Full Traceability

 

The Vacuum Brazed Nickel Superalloy Honeycomb Seal is a critical gas-path sealing component mounted in the annular groove of aero-engine casings, closely surrounding the rotating blade tips. The product is precision-formed from 0.05–0.1mm thick nickel-based superalloy foil into a regular hexagonal honeycomb structure, with the honeycomb core securely joined to the support ring via vacuum brazing.

 

Integrating nickel-based superalloy materials, precision vacuum brazing technology, and full-process quality traceability, this product is engineered for extreme aero-engine operating conditions and serves as a key enabler for improving engine efficiency and reducing fuel consumption.

 

2. Working Principle & Technical Features

 

2.1 Honeycomb Sealing Principle

 

The honeycomb seal features hexagonal cells ranging from 0.8 mm to 3.0 mm in diameter, with a maximum cell depth of 13 mm. During engine operation, the rotating blade tips, driven by centrifugal force, gently cut into the honeycomb structure, forming an optimal radial clearance fit. This "active wear" design allows the honeycomb core to function as a sacrificial abradable layer, protecting blades from dangerous contact with the rigid casing while minimizing gas-path leakage to the greatest extent.

 

2.2 Performance Comparison

 

Parameter Traditional Labyrinth Seal This Product

Gas-path leakage loss Baseline 50‑70% reduction

Operating temperature Limited Turbine-stage capable

Blade protection None Abradable honeycomb core

Process traceability Limited Full-chain traceable

 

3. Core Advantages

 

3.1 Nickel-Based Superalloy Material System

 

The honeycomb core is manufactured from GH536 (Hastelloy X) nickel-based superalloy, which exhibits excellent structural stability and oxidation resistance under combustor-grade high-temperature gases and thermal cycling conditions. Support ring (casing) materials can be selected from GH4169, GH907, GH600, or stainless steel depending on service conditions. This nickel-based material system ensures reliable performance in environments exceeding 900°C.

 

3.2 Vacuum Brazing Process

 

Vacuum brazing is the core manufacturing process for this product. Nickel-based brazing alloys (such as BNi‑2, BNi‑4, and BNi‑5) are used to join the honeycomb core to the support ring in a vacuum furnace.

 

Critical Process Controls:

 

Parameter Control Range

Brazing temperature 1030‑1180°C (depending on brazing alloy)

Soaking time Strictly controlled at 6‑15 minutes

Brazing filler amount Approximately 2× the volume required to fill the joint

Vacuum level Ensures oxidation-free, optimal wettability

 

Proprietary stepwise cooling control effectively prevents distortion of the honeycomb assembly during the brazing thermal cycle, ensuring dimensional stability. Vacuum brazed joint strength reaches approximately 50% of the base metal, meeting the stringent mechanical property requirements of aero-engines.

 

3.3 Full-Process Traceability

 

In the aero-engine industry, every single component's quality is a matter of flight safety. This product features an end-to-end traceability system:

 

Traceability Stage Data Captured Customer Value

Raw material Foil grade, batch, physical properties Source control

Honeycomb forming Stamping parameters, cell size, wall thickness Geometric accuracy guarantee

Assembly & tack welding Positioning parameters, assembly clearance Accurate alignment

Vacuum brazing Temperature profile, vacuum level, soak time Thermal cycle control verified

Non-destructive testing Fluorescent penetrant, X-ray records Zero defects policy

Final inspection Roundness, flatness, PCD hole diameter Right-first-time delivery

 

Each product carries a unique traceability code, allowing customers to retrieve all manufacturing and inspection data instantly — every part traceable, every step accountable.

 

4. Applications

 

4.1 Typical Installation Locations

· Compressor stator honeycomb seal segments
· Combustor front seal ring assemblies
· Turbine outer shroud honeycomb arcs
· Low‑pressure turbine rotor honeycomb assemblies

 

Engineered for Precision – Technical Specifications

 

Our honeycomb seal product line supports the following flexible specifications:

 

Parameter Specification Range
Material Options Stainless Steel, Haynes 214, Hastelloy X, High-Temperature Alloy, Carbon Steel
Honeycomb Cell Size 0.8 mm – 5.6 mm (0.8 mm, 1.6 mm, 2.0 mm, 3.2 mm, 4.2 mm, 5.6 mm, etc.)
Cell Wall Thickness 0.08mm, 0.1mm, 0.13 mm, 0.15 mm, 0.2 mm (customizable)
Product Forms Rings, Segments, Strips, Rectangular Sheets etc
Manufacturing Processes Automatic Laser Welding, Vacuum Brazing etc

 

Advantages

 

1 Very low cross coupling
2 Higher direct damping that labyrinth seals
3 More forgiving than labyrinth seals in the event of a rotor-stator rub
4 Variety of materials available to serve a wide range of applications
5 Capable of sustaining higher temperatures than conventional labyrinth seals
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2008

  • Total Annual:

    3 million-10 million

  • Employee Number:

    100~120

  • Ecer Certification:

    Site Member

With more than 20 years’ experience on designing and manufacturing honeycomb and metal product, Pasia Honeycomb Products Co. Ltd is versatile on supplying diversified honeycomb and sandwich products to clients of various industries including construction, transportation, marine, industrial equ... With more than 20 years’ experience on designing and manufacturing honeycomb and metal product, Pasia Honeycomb Products Co. Ltd is versatile on supplying diversified honeycomb and sandwich products to clients of various industries including construction, transportation, marine, industrial equ...

+ Read More

Get in touch with us

  • Reach Us
  • Pasia Honeycomb Products Co., Ltd
  • 1200 N Fuxing Rd Wutong District 314500 Zhejiang P. R. China
  • https://www.honeycombcompositepanels.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement