| Payment Terms | full payment by L/C or 20% down payment, balance before shipment |
| Delivery Time | within 20 working days |
| Packaging Details | Standard seaworth package |
| Grade: | 316L |
| Standard: | ASTM, EN, GB, JIS |
| Length: | 1000-2000mm |
| Thickness: | 0.3-3.0 |
| Width: | 1000-6000mm |
| Place of Origin: | China |
| Technique: | Cold Rolled |
| Surface: | 2B or Polishing |
| Brand Name | BAOSTEEL,TISCO, |
| Model Number | 317L |
| Certification | ISO |
| Place of Origin | China |
View Detail Information
Explore similar products
1% Nickel Stainless Steel Cold Rolled Coil , Anti Corrosion 201 Steel Strip Coil
Bright Annealing Stainless Steel Strip Coil 304 BA / 430BA Raw Material
SUS321 Stainless Steel Sheet Roll High Corrosion Resistance Prime Grade
310S Stainless Steel Coil
Product Specification
| Payment Terms | full payment by L/C or 20% down payment, balance before shipment | Delivery Time | within 20 working days |
| Packaging Details | Standard seaworth package | Grade: | 316L |
| Standard: | ASTM, EN, GB, JIS | Length: | 1000-2000mm |
| Thickness: | 0.3-3.0 | Width: | 1000-6000mm |
| Place of Origin: | China | Technique: | Cold Rolled |
| Surface: | 2B or Polishing | Brand Name | BAOSTEEL,TISCO, |
| Model Number | 317L | Certification | ISO |
| Place of Origin | China |
The higher molybdenum and chromium content of 317L provides excellent corrosion resistance compared to stainless steel grades like 304 or 316, and it resists phosphoric acid, sulfuric acid, and chloride pitting/crevice corrosion. The low carbon content of this grade of 317 also provides resistance to sensitization during welding, which allows it to maintain its corrosion resistance at grain boundaries and prevent intergranular stress corrosion cracking.
| 化学成分 | 物理性能 | |||||||||||||
| Chemical Composition(%) | Physical Property | |||||||||||||
| C | Si | Mn | P | S | Cr | Ni | Ti | N | Cu | Mo | 屈服强度 Y.S. (Mpa) | 抗拉强度 T.S( Mpa) | 延伸率EL/% | 硬度 HARDNESS |
| Min | Min | Min | Min | Min | Min | Min | Min | Min | Min | Min | Min | Min | Min | Min |
| 18.000 | 11.000 | 3.000 | 205 | 517 | 35.0 | |||||||||
| Max | Max | Max | Max | Max | Max | Max | Max | Max | Max | Max | Max | Max | Max | Max |
| 0.030 | 0.750 | 2.000 | 0.045 | 0.030 | 20.000 | 15.000 | 0.100 | 4.000 | 95 RB | |||||
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company,Seller,Other
Year Established:
2017
Total Annual:
20 Million-100 Million
Ecer Certification:
Site Member
Company Overview Established in 2017,JUYE METAL is located in Ningbo City,which is one of the largest international port cities in China, with convenient transportation facilities and mature commercial service network for steel products. Although We are a young company, our founder and key leade... Company Overview Established in 2017,JUYE METAL is located in Ningbo City,which is one of the largest international port cities in China, with convenient transportation facilities and mature commercial service network for steel products. Although We are a young company, our founder and key leade...
Get in touch with us
Leave a Message, we will call you back quickly!