China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy

  1. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
  2. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
  3. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
  4. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
  5. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy
  6. China ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy

ASTM Inconel Alloy 718 Round Bar 718 Inconel Sheet Nickel Based Superalloy

  1. MOQ: 200KG
  2. Price: To negotiate
  3. Get Latest Price
Payment Terms T/T, L/C
Supply Ability 50~80 TONS per MONTH
Delivery Time 45~60days
Packaging Details Wooden Box, size as per guests' request
Shape Wire,Strip,Rod,Pipe,Plate
Alloy Type Nickel-based Superalloy
Raw Materials NI Rem,CR18%,Co9% ,MO2.75%
Executive standard ASTM
Delivery State Soft State
Application Used for disc, brake, fastener, blade and etc
Features High temperature resistance
Size Negotiable
Brand Name KAIXIN
Model Number KX-Alloy IN P718
Certification ISO9001:2015
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T, L/C Supply Ability 50~80 TONS per MONTH
Delivery Time 45~60days Packaging Details Wooden Box, size as per guests' request
Shape Wire,Strip,Rod,Pipe,Plate Alloy Type Nickel-based Superalloy
Raw Materials NI Rem,CR18%,Co9% ,MO2.75% Executive standard ASTM
Delivery State Soft State Application Used for disc, brake, fastener, blade and etc
Features High temperature resistance Size Negotiable
Brand Name KAIXIN Model Number KX-Alloy IN P718
Certification ISO9001:2015 Place of Origin China
High Light ASTM Inconel Alloy ,Round Inconel Alloy ,Inconel 718 round bar

KX Inconel 718 Plus Nickel Alloy Wire Round Bar Tube Steel Sheet Light Rod On Inconel Alloy

 

Product Description and Application

 

Inconel718 plus is a new type of nickel-based precipitation-hardened alloy, which is widely concerned at home and abroad because of its excellent comprehensive mechanical properties below 700°C, good thermal working and welding properties, suitable cost. At present, this material has been promoted and applied in several well-known aero-engine companies, which are used in disc parts, brakes, fasteners, blades and etc. In addition, Inconel718 Plus is also commonly used in copper extrusion mold.

 

Process Performance and Requirements

 

  • Product Fusion Process

 

 Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)

 

  • Product Chemical Composition 

 

Element C Ni Cr Mo W Co Fe Nb Ti Al P B
Inconel718 plus 0.02 Rem 18 2.75 1 9 10 5.45 0.7 1.45 0.01 0.004

 

  • Product Physical Property

 

Density 8.25g/cm3
Melting Temperature Range 1260~1340℃

 

  • Product Mechanical Property

 

Hardness:

The hardness is about 20-30HRC after solid solution heat treatment and about 38-45HRC after annealing

 

  • Productive Process

 

 

 

 

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Trading Company

  • Year Established:

    2007

  • Total Annual:

    10000000-30000000

  • Employee Number:

    150~200

  • Ecer Certification:

    Verified Supplier

Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as preci... Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as preci...

+ Read More

Get in touch with us

  • Reach Us
  • Danyang Kaixin Alloy Material Co., Ltd.
  • The North East of Danlv Bridge, Aerospace Industry Park, Lvcheng Town,Danyang City,Jiangsu Province
  • https://www.kaixin-alloy.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement