| Payment Terms | T/T |
| Delivery Time | 5-7days |
| Packaging Details | 1KG/BOTTLE |
| Main Raw Material | Polyurethane |
| Usage | Rubber Coating, silver oil colored-oil, Laser etching oil. |
| Application Method | Spray |
| State | Liquid Coating |
| Color | Color Card |
| Application | Key pads, wristbands, other silicone product |
| Warranty | 6 months without any mixing |
| Appearance | Pasty |
| Brand Name | KangLiBang |
| Certification | ROHS,SGS |
| Place of Origin | Guangdong, China |
View Detail Information
Explore similar products
Silicone Rubber Screen Printing Ink Cured At High Temperature
Silicone Rubber Polyurethane (PU) Coating Ink
Silicone Rubber Spraying Conductive Coating Ink
Silicone Soft Touching Spraying Coating Ink Cured At High Temperature
Product Specification
| Payment Terms | T/T | Delivery Time | 5-7days |
| Packaging Details | 1KG/BOTTLE | Main Raw Material | Polyurethane |
| Usage | Rubber Coating, silver oil colored-oil, Laser etching oil. | Application Method | Spray |
| State | Liquid Coating | Color | Color Card |
| Application | Key pads, wristbands, other silicone product | Warranty | 6 months without any mixing |
| Appearance | Pasty | Brand Name | KangLiBang |
| Certification | ROHS,SGS | Place of Origin | Guangdong, China |
| High Light | rubber silicone based ink ,rubber silicone based screen printing ink ,coating silicone based ink | ||
Silicone Rubber Spraying Coating Ink Cured At High Temperature
Product Description
This ink mainly used for silicone rubber spraying coating ink, cured at high temperature (180~220℃).Characterized by smooth feeling, friction resisting, dust proof , well Covering power and adhesive power. Suit for the spraying coating necessaries of silver oil, colored-oil, Laser etching oil.
Application
Mainly applied to silicone bracelet, silicone cellphone case, silicone keypad and other silicone rubber products.
Application Ratio
Silicone ink: 100g
Mixer(catalyst): 2~3g
Thinner: 300~500g
Processing
1. Pick out appropriate ink at ratio (100/2-3) into a cleaning barrel, mixed with catalyst thoroughly.
2. Diluting for three to five times with thinner (Toluene, White Gas or Dimethyl- benzene).
3. About 5-10min mixing
4. Filtrating with 300 mesh filter screen for twice before spraying.
5. Max 12hours working time for mixed ink.
6. Keeping 22℃ working temperature
All the above physical data only for reference.
Baking method
A.Oven:Baking at 180℃ for 20 minutes.
B.IR strip: Baking at constant temperature 200℃ for 7 minutes
Attention
1. This agent including volatile solvent, please keep ventilating and far away from heat and open flame.
2. Avoid skin contact for a long time and vapor inhalation
3. Washing with soap once skin contact.
Storage
Stored at room temperature for 6 months with any mixing.
Packing
1KG/Bottle.
Application range:
![]()
Company Details
Business Type:
Manufacturer
Year Established:
2010
Total Annual:
5000000-10000000
Employee Number:
50~100
Ecer Certification:
Verified Supplier
Shenzhen Kanglibang Science & Technology Co., Ltd was founded in 2010, focusing on the development of new adhesive materials. It is a national-level specialized and special "little giant" enterprise integrating the research and development, manufacturing, sales and service of adhesive ... Shenzhen Kanglibang Science & Technology Co., Ltd was founded in 2010, focusing on the development of new adhesive materials. It is a national-level specialized and special "little giant" enterprise integrating the research and development, manufacturing, sales and service of adhesive ...
Get in touch with us
Leave a Message, we will call you back quickly!