China factories

Chat Now Send Email
China factory - Shuoboda Instruments (Hunan) Co., Ltd.

Shuoboda Instruments (Hunan) Co., Ltd.

  • China,Jincheng ,Hunan
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃
China DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃

  1. China DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃
  2. China DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃
  3. China DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃

DSC-200L Heat Flux DSC Differential Scanning Calorimetry Equipment -170 ~ 600℃

  1. MOQ: 1 set
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms ,L/C,T/T
Supply Ability 500 sets/month
Delivery Time 5~8 working days
Packaging Details Plywood box
Temperature Range -170 ~ 600℃
Temperature Resolution 0.001℃
Temperature Fluctuation ±0.01℃
Temperature Repeatability ±0.01℃
Heating Rate 0.1~100 ℃/min
Cooling Rate 0.1~40 ℃/min
Brand Name SHUOBODA
Model Number DSC-200L
Certification ISO/CE
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms ,L/C,T/T Supply Ability 500 sets/month
Delivery Time 5~8 working days Packaging Details Plywood box
Temperature Range -170 ~ 600℃ Temperature Resolution 0.001℃
Temperature Fluctuation ±0.01℃ Temperature Repeatability ±0.01℃
Heating Rate 0.1~100 ℃/min Cooling Rate 0.1~40 ℃/min
Brand Name SHUOBODA Model Number DSC-200L
Certification ISO/CE Place of Origin China
High Light DSC Differential Scanning Calorimetry Equipment ,Heat Flux Differential Scanning Calorimetry Equipment

DSC-200L Differential Scanning Calorimeter (DSC) 

 Product introduction

Differential scanning calorimetry (DSC) technology has been widely used. Differential scanning calorimetry is both a routine quality testing tool, but also a research tool. It measures temperature, heat flow relationship related to materials internal thermal transition. Our company's device is heat flux differential scanning calorimeter, with good repeatability, high accuracy characteristics, especially suitable for accurate measurement of the specific heat. The device is easy to calibrate, using a low melting point, fast and reliable, and with a wide range of applications, especially in materials research and development, performance testing and quality control. Characteristics of the material, such as the glass transition temperature, cold crystallization, phase transition, melting, crystallization, product stability, the curing/crosslinking, oxidation induction, etc. are research areas of differential scanning calorimeter.

 

Differential scanning calorimetry applications are: the curing reaction temperature and thermal effects of polymer materials, material phase change temperature and its thermal effects measurement, polymer materials crystallization, melting temperature and its thermal effects measurement, the glass transition temperature of the polymer material and so on. Subjects of experiment are: solid, liquid, viscous samples, except the gas.

 

Place the specimen and the reference material into the crucibles respectively, heating in the oven to change the temperature of the specimen and the reference material. If hot melt of the specimen as same as the reference material and the specimen has not the thermal effect, the temperature difference between the two is close to "0", then we can get a smooth curve.

As the temperature increases, the specimen produces a thermal effect, but the reference material doesn't produce the thermal effect, it makes the temperature difference between the two, it expresses as the peak in the DTA curve, the bigger temperature difference, the greater the peak, and the more the change number of temperature difference, the more the number of peaks. It is called peak exothermic which peak upward, and it is called peak endothermic which peak downward. 

The picture is a typical DSC curve; it shows four types of changes.

Ⅰ is second order transition; it is the change of level base line.

Ⅱ is the endothermic peak, it caused by the melting changes of the specimen.

Ⅲ is the endothermic peak, it caused by the decomposition reaction of specimen.

Ⅳ is the exothermic peak, it caused by the crystalline phase transition of the specimen.

 

Experimental principle

Materials are often accompanied by thermal effects in the process of physical changes and chemical changes, exothermic and endothermic phenomena reflect the heat enthalpy of the material has changed. DTA can measure the functional relationship of temperature difference between the specimen and the reference material to temperature or time in the same heating conditions.

 

Differential scanning calorimetry is a technique, which in the case of process control temperature, measures the relationship of power difference and temperature between the output material and reference material. Our company's device is heating flux differential scanning calorimeter, the ordinate is heating flow difference of the sample and the reference material, in units of mw. Abscissa is the time (t) or temperature (T), from left to right for the growth (does not meet this requirement should be specified).

 

After putting the specimen and the reference material into crucible, according to the heating rate, if the hot melt of the reference material similar as the specimen, we can get the ideal scanning calorimetric analysis diagram.

 

 

In this picture, T reflects the temperature curve of thermocouple which sticks in the reference material; Line AH reflects the temperature difference curve between the specimen and the reference material. If the specimen without thermal effects, △T between the specimen and the reference material is 0, line AB, DE, GH is smooth baseline in the curve. When the thermal effect occurs, if the temperature of specimen lowers than the temperature of reference material, we can get the endothermic peak like line BCD; otherwise, we can get the exothermic peak like line EFG.

 

The number, position, peak area, direction, height, width, symmetry of the peaks reflects the times of physical changes and chemical changes in the measured temperature range, temperature range which changed, the size, positive and negative of thermal effect. The heights, width, symmetry of the peaks is not only relating with test conditions, but also relating with pharmacokinetics factors in the process of the specimen change, the result is much more complex than the ideal curve.

 

Instrument features

Ÿ New furnace structure, better resolution and baseline stability;

Ÿ Digital gas mass flow meter, precise control of the purge gas flow; Data is directly recorded in the database;

Ÿ The instrument can be bi-directional control (host control, software control); friendly interface, easy to operate.

 

Curve display

 

 

Technical parameters

DSC

DSC-200L Differential Scanning Calorimeter

Temperature   Range

-170 ~ 600℃  

Temperature Resolution

0.001℃

Temperature Fluctuation

±0.01℃

Temperature Repeatability

±0.01℃

Heating Rate

0.1~100 ℃/min

Cooling Rate

0.1~40 ℃/min

Constant temperature time

can be set

Temperature Control Mode

PID temperature control, heating, cooling, constant temperature (full program automatic control)

Scanning method

Heating scan, cooling scan

DSC Range

0~±600mW

DSC resolution

0.01uW

DSC Sensitivity

0.001mW

Gas flow

0-300mL/min

Gas pressure

≤5MPa

Atmosphere Control

Two-way automatic switching (instrument automatically switches)

Program control

can realize six-stage heating constant temperature control, special parameters can be customized

Display

24bit color 7-inch LCD touch-screen display

Data Interface

Standard USB interface

Parameter standards

Equipped with standard samples (indium, tin, lead), users can correct the temperature by themselves

Remark

All the technical indicators can be adjusted according to user needs.

Power supply

AC 220V/50Hz or customized

 

Standard accessories

ITEM NAME

QTY

Host instrument  

1

Soft

1

Data Line      

1

Power Line         

1

Aluminum crucibles

100

Ceramic crucibles     

100

Bag of pure tin grains

1

Fuse 10A     

5

Operation manual  

1

Warranty card   

1

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Exporter

  • Year Established:

    2013

  • Total Annual:

    1,000,000-10,000,000

  • Employee Number:

    1~99

  • Ecer Certification:

    Verified Supplier

Shuoboda Instruments Group as a professional manufacturer & supplier in China, we are committed to provides quality, user friendly and cost-effective products to our partner in all over the world. Our products mainly included Radiation Detection & Protection Equipment,  laboratory scien... Shuoboda Instruments Group as a professional manufacturer & supplier in China, we are committed to provides quality, user friendly and cost-effective products to our partner in all over the world. Our products mainly included Radiation Detection & Protection Equipment,  laboratory scien...

+ Read More

Get in touch with us

  • Reach Us
  • Shuoboda Instruments (Hunan) Co., Ltd.
  • Room 1725, Building 1, Sunshine Jincheng, No. 35 Xinjian East Road, Yuhua District, Hunan Province, China, 410014
  • https://www.lab-testinstrument.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement