China Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter
China Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter

  1. China Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter
  2. China Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter

Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter

  1. MOQ: 1
  2. Price: Negotaible
  3. Get Latest Price
Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 200
Delivery Time 5-8 work days
Packaging Details Wooden package
Size 300 × 300 mm
Thickness Measurement 0-50 mm
Pressure Clamping 0-1000 N
System Accuracy ±3%
Warranty 1 Year
Brand Name Lonroy
Model Number LRPL-III-300
Certification Includes Calibration Certification
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,D/A,D/P,T/T,Western Union Supply Ability 200
Delivery Time 5-8 work days Packaging Details Wooden package
Size 300 × 300 mm Thickness Measurement 0-50 mm
Pressure Clamping 0-1000 N System Accuracy ±3%
Warranty 1 Year Brand Name Lonroy
Model Number LRPL-III-300 Certification Includes Calibration Certification
Place of Origin China
High Light fully automatic thermal conductivity equipment ,protective plate heat flow meter ,differential scanning calorimeter with warranty

Fully Automatic Thermal Conductivity Equipment Protective Plate Heat Flow Meter Method Differential Scanning Calorimeter

LRPL-III-300 Fully Automatic Thermal Conductivity Equipment (Protective Plate Heat Flow Meter Method)

1.Description:
This instrument adopts the internationally popular method of using thermal flow meters to measure the thermal conductivity and thermal resistance. It is equipped with a computer to achieve fully automatic testing and generate experimental reports. It is suitable for testing the thermal properties of low thermal conductivity materials such as insulation materials and refractory materials. With the addition of a sample frame, it can also be used for powder material testing. It is widely used in universities, research institutes, quality inspection departments, factories and mines.
2.Standard

The methods for determining the thermal resistance and thermal conductivity of JIS-1412-2 heat-resistant materials, GB/T10295-2008, ISO 8301:1991 (the steady-state thermal resistance and related properties of insulation materials - the hot flow meter method), and ASTM C518-04 (the test methods for determining steady-state heat flux and heat transfer characteristics using the hot flow meter method).

3.Technical Parameter.

Parameter Specification
Thermal Conductivity 0.0010-3.0000 W/(m·K) (4 decimals)
Accuracy & Repeatability Accuracy: ±3%
Repeatability: ±1%
Sample Specifications  
- Size 300 × 300 mm (Standard)
Customizable
- Thickness 10-50 mm
- Materials Solids, Powders
Temperature Control  
- Hot Surface RT-100°C (Standard)
Up to 300°C (Optional)
Accuracy: ±0.1°C
SCR-controlled plate heater
- Cold Surface -5-99.9°C
Water-cooled precision bath
Accuracy: ±0.1°C
Automation  
- Pressure Clamping 0-1000 N (Resolution: 0.1 N)
- Thickness Measurement 0-50 mm (Resolution: 0.01 mm)
Environmental Control Acrylic wind shield with side door
Protective monitoring system for stability
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Agent,Exporter,Seller

  • Year Established:

    2008

  • Total Annual:

    $5 million -$8 million

  • Employee Number:

    80~200

  • Ecer Certification:

    Verified Supplier

Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes... Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes...

+ Read More

Get in touch with us

  • Reach Us
  • DONGGUAN LONROY EQUIPMENT CO LTD
  • A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
  • https://www.lab-testmachines.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement