China LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter Differential
China LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter Differential

  1. China LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter Differential

LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter Differential

  1. MOQ: 1
  2. Price: Negotaible
  3. Get Latest Price
Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 200
Delivery Time 5-8 work days
Packaging Details Wooden package
Power Supply 220V ± 10%, 50Hz
CTE Sample ≤ Ø10 × 20 mm
Max. Load 10N
Temperature Resolution 0.1°C
Warranty 1 Year
Brand Name Lonroy
Model Number LRPY-300
Certification Includes Calibration Certification
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,D/A,D/P,T/T,Western Union Supply Ability 200
Delivery Time 5-8 work days Packaging Details Wooden package
Power Supply 220V ± 10%, 50Hz CTE Sample ≤ Ø10 × 20 mm
Max. Load 10N Temperature Resolution 0.1°C
Warranty 1 Year Brand Name Lonroy
Model Number LRPY-300 Certification Includes Calibration Certification
Place of Origin China
High Light 10N thermal analysis instrument ,plastic expansion meter DSC ,differential scanning calorimeter with warranty

LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter Differential Scanning Calorimeter

LRPY-300 Thermal Analysis Instrument Plastic Expansion Meter

1.Description:

This instrument is mainly used to measure three thermal physical indicators of plastics: the expansion coefficient, the glass transition temperature, and the Vicat softening temperature of thermoplastic. The test for the glass transition temperature complies with GB11998-89 (Method for Measuring the Glass Transition Temperature of Plastics - Thermal Mechanical Analysis Method), and the measurement of the Vicat softening temperature of thermoplastic complies with GB/T1633-2000 ISO 306:1994 (Determination of Vicat Softening Temperature (VST) of Thermoplastic). The instrument is widely used in laboratories of material manufacturing enterprises, quality inspection units, universities, research institutes, etc., for thermal mechanical analysis of plastics and other materials.

2.Technical Parameter.

Parameter Specification
Furnace Temperature Range RT to 300°C
Max. Load 10 N
Power Supply 220V ± 10%, 50Hz
Max. Power Consumption < 0.5 kW
Displacement Measurement

Range: 0–3 mm

Resolution: 0.1 µm

Temperature Resolution 0.1°C
Sample Sizes:
• CTE Sample ≤ Ø10 × 20 mm
• Glass Transition (Tg) Cylinder: Ø(4.5±0.5) × (6.0±1.0) mm
Cube: (4.5±0.5)³ × (6.0±1.0) mm
• Vicat Softening Point Thickness: 3–6.5 mm
Base: 10 mm square or Ø10 mm cylinder
Control & Reporting Fully computer-controlled
Automatic test result recording & report generation
Printable output
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Agent,Exporter,Seller

  • Year Established:

    2008

  • Total Annual:

    $5 million -$8 million

  • Employee Number:

    80~200

  • Ecer Certification:

    Verified Supplier

Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes... Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes...

+ Read More

Get in touch with us

  • Reach Us
  • DONGGUAN LONROY EQUIPMENT CO LTD
  • A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
  • https://www.lab-testmachines.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement