| Payment Terms | L/C,D/A,D/P,T/T,Western Union |
| Supply Ability | 200 |
| Delivery Time | 5-8 work days |
| Packaging Details | Wooden package |
| Dimensions | 250 × 250 × (5-40) mm |
| Transfer Area | 250 × 250 mm (300 × 300 mm optional) |
| Adjustable Spacing | 0-50mm |
| Thickness Measurement | 0-50.00 mm |
| Warranty | 1 Year |
| Brand Name | Lonroy |
| Model Number | LRPL-III |
| Certification | Includes Calibration Certification |
| Place of Origin | China |
View Detail Information
Explore similar products
TG Thermogravimetry Apparatus/TGA Thermo Gravimetric Analyzer/Thermogravimetric
ASTM E1354 ISO 5660 ASTM E1354 ISO 5660 Cone Calorimeter Analyzer BS 476 Cone
Fully Automatic Oxygen Bomb Calorimeter DM3300 Certification Includes Calibratio
ASTM D3895 ASTM D3895 DSC Differential Scanning Calorimeter Full-color LCD Touch
Product Specification
| Payment Terms | L/C,D/A,D/P,T/T,Western Union | Supply Ability | 200 |
| Delivery Time | 5-8 work days | Packaging Details | Wooden package |
| Dimensions | 250 × 250 × (5-40) mm | Transfer Area | 250 × 250 mm (300 × 300 mm optional) |
| Adjustable Spacing | 0-50mm | Thickness Measurement | 0-50.00 mm |
| Warranty | 1 Year | Brand Name | Lonroy |
| Model Number | LRPL-III | Certification | Includes Calibration Certification |
| Place of Origin | China | ||
| High Light | LRPL-III thermal conductivity analyser ,ASTM C 518 insulation materials tester ,differential scanning calorimeter for insulation | ||
1.Description:
This instrument uses the internationally popular heat flow meter method to measure thermal conductivity and thermal resistance, and is equipped with a computer to achieve fully automatic testing and generate test reports. It is suitable for testing the thermal conductivity of low thermal conductivity materials such as insulation materials and refractory materials. With the addition of a sample frame, it can also be used to test powder materials. It is widely used in colleges and universities, research institutes, quality inspection agencies, and factories and mines.
2.Standard
GB/T 10295-2008 (Determination of Steady-State Thermal Resistance and Related Properties of Insulation Materials - Thermal Flow Meter Method) and ASTM C518-04 - Test methods for determining steady-state heat flux and heat transfer properties using the thermal flow meter method.
3.Technical Parameter.
| Thermal Conductivity | 0.0010-3.0000 W/m·K (4 decimal display) |
| Accuracy | Better than 3% ±0.0005 W/m·K |
| Temperature Control | |
| - Hot Surface | Configurable: RT-99.99°C or RT-350.0°C |
| - Cold Surface | 0-99.99°C (Resolution: 0.01°C) |
| Sample Specifications | |
| - Dimensions | 250 × 250 × (5-40) mm |
| - Test Area | 120 × 120 mm |
| - Materials | Solids, Powders |
| Automated Features | |
| - Pressure System | 0-1000 N (Auto-loading, speed adjustable) |
| - Thickness Measurement | 0-50.00 mm (Resolution: 0.01 mm) |
| Heating Plate | |
| - Transfer Area | 250 × 250 mm (300 × 300 mm optional) |
| - Adjustable Spacing | 0-50 mm |
| Test Environment | Acrylic wind shield with side door |
| Test Duration | Approx. 2 hours |
Company Details
Business Type:
Manufacturer,Agent,Exporter,Seller
Year Established:
2008
Total Annual:
$5 million -$8 million
Employee Number:
80~200
Ecer Certification:
Verified Supplier
Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong, is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to pr... Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong, is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to pr...