China LRPL-III ASTM C 518 Thermal Conductivity Analyser For Insulation Materials
China LRPL-III ASTM C 518 Thermal Conductivity Analyser For Insulation Materials

  1. China LRPL-III ASTM C 518 Thermal Conductivity Analyser For Insulation Materials

LRPL-III ASTM C 518 Thermal Conductivity Analyser For Insulation Materials

  1. MOQ: 1
  2. Price: Negotaible
  3. Get Latest Price
Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 200
Delivery Time 5-8 work days
Packaging Details Wooden package
Dimensions 250 × 250 × (5-40) mm
Transfer Area 250 × 250 mm (300 × 300 mm optional)
Adjustable Spacing 0-50mm
Thickness Measurement 0-50.00 mm
Warranty 1 Year
Brand Name Lonroy
Model Number LRPL-III
Certification Includes Calibration Certification
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,D/A,D/P,T/T,Western Union Supply Ability 200
Delivery Time 5-8 work days Packaging Details Wooden package
Dimensions 250 × 250 × (5-40) mm Transfer Area 250 × 250 mm (300 × 300 mm optional)
Adjustable Spacing 0-50mm Thickness Measurement 0-50.00 mm
Warranty 1 Year Brand Name Lonroy
Model Number LRPL-III Certification Includes Calibration Certification
Place of Origin China
High Light LRPL-III thermal conductivity analyser ,ASTM C 518 insulation materials tester ,differential scanning calorimeter for insulation

LRPL-III ASTM C 518 Thermal Conductivity Analyser For Insulation Materials Differential Scanning Calorimeter

LRPL-III ASTM C 518 Heat Conductivity Analyzer for Insulation Materials

1.Description:
This instrument uses the internationally popular heat flow meter method to measure thermal conductivity and thermal resistance, and is equipped with a computer to achieve fully automatic testing and generate test reports. It is suitable for testing the thermal conductivity of low thermal conductivity materials such as insulation materials and refractory materials. With the addition of a sample frame, it can also be used to test powder materials. It is widely used in colleges and universities, research institutes, quality inspection agencies, and factories and mines.
2.Standard

GB/T 10295-2008 (Determination of Steady-State Thermal Resistance and Related Properties of Insulation Materials - Thermal Flow Meter Method) and ASTM C518-04 - Test methods for determining steady-state heat flux and heat transfer properties using the thermal flow meter method.

3.Technical Parameter.

Thermal Conductivity 0.0010-3.0000 W/m·K (4 decimal display)
Accuracy Better than 3% ±0.0005 W/m·K
Temperature Control
- Hot Surface Configurable: RT-99.99°C or RT-350.0°C
- Cold Surface 0-99.99°C (Resolution: 0.01°C)
Sample Specifications
- Dimensions 250 × 250 × (5-40) mm
- Test Area 120 × 120 mm
- Materials Solids, Powders
Automated Features
- Pressure System 0-1000 N (Auto-loading, speed adjustable)
- Thickness Measurement 0-50.00 mm (Resolution: 0.01 mm)
Heating Plate
- Transfer Area 250 × 250 mm (300 × 300 mm optional)
- Adjustable Spacing 0-50 mm
Test Environment Acrylic wind shield with side door
Test Duration Approx. 2 hours
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Agent,Exporter,Seller

  • Year Established:

    2008

  • Total Annual:

    $5 million -$8 million

  • Employee Number:

    80~200

  • Ecer Certification:

    Verified Supplier

Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes... Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes...

+ Read More

Get in touch with us

  • Reach Us
  • DONGGUAN LONROY EQUIPMENT CO LTD
  • A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
  • https://www.lab-testmachines.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement