China factories

Chat Now Send Email
China factory - DONGGUAN LONROY EQUIPMENT CO LTD

DONGGUAN LONROY EQUIPMENT CO LTD

  • China,Dongguan ,Guangdong
  • Verified Supplier
  1. Home
  2. Products
  3. About Us
  4. Contact Us

Leave a Message

we will call you back quickly!

Submit Requirement
China ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat
China ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat

  1. China ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat
  2. China ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat

ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat

  1. MOQ: 1
  2. Price: Negotaible
  3. Get Latest Price
Payment Terms L/C,D/A,D/P,T/T,Western Union
Supply Ability 200
Delivery Time 5-8 work days
Packaging Details Wooden package
Heat Flux Range 0.5-2000 W/m²
Transfer Area 400 × 400 mm
Adjustable Spacing 0-100 mm
Thermal Conductivity 0.001-1.000 W/m·K (Plates)
Warranty 1 Year
Brand Name Lonroy
Model Number LRPL-400
Certification Includes Calibration Certification
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,D/A,D/P,T/T,Western Union Supply Ability 200
Delivery Time 5-8 work days Packaging Details Wooden package
Heat Flux Range 0.5-2000 W/m² Transfer Area 400 × 400 mm
Adjustable Spacing 0-100 mm Thermal Conductivity 0.001-1.000 W/m·K (Plates)
Warranty 1 Year Brand Name Lonroy
Model Number LRPL-400 Certification Includes Calibration Certification
Place of Origin China
High Light ASTM C518 thermal conductivity machine ,automatic heat flux DSC ,plate method differential scanning calorimeter

ASTM C518 LRPL-400 ASTM C518 Automatic Thermal Conductivity Machine Plate Heat Flux Method Differential Scanning DSC

LRPL-400 ASTM C518 Thermal Conductivity Machine (Plate Heat Flux Method)

1.Description:
This instrument adopts the internationally popular method of using thermal flow meters to measure thermal conductivity and thermal resistance. It is equipped with a computer to achieve fully automatic testing and generate experimental reports. It is redesigned based on the DRPL-I type flat plate thermal flow meter for thermal conductivity testing instrument produced by our company, and is capable of meeting the testing requirements of 400×400×(5-80) insulation bricks.
This instrument is based on the steady-state plate method testing principle. A stable temperature is added to the hot surface, and the heat passes through the sample to the cold surface. The transferred heat flow is measured. Then, the thermal conductivity and thermal resistance can be calculated based on the thickness of the sample and the heat transfer area. This testing method is simple, fast, and has good repeatability. It is very suitable for research and development in material heat transfer. It can be used for testing of rocks and soils, foams, cement, insulation materials, etc., and is widely applied in universities, research institutes, quality inspection, factories and mines.
2. Standard

ASTM C518-04 - Test method for steady-state heat flux and heat transfer characteristics using the heat flow meter; GB10295-88 - Determination of steady-state thermal resistance and related properties of insulation materials (by heat flow meter method).

 

3. Technical Parameter.

Parameter Specification
Thermal Conductivity 0.001-1.000 W/m·K (Plates)
Accuracy: ±3%
Temperature Measurement
- Hot Surface RT-99.99°C
Class 0.2 digital display
Resolution: 0.01°C
- Cold Surface 5-99.99°C
Class 0.2 digital display
Resolution: 0.01°C
Temperature Control
- Hot Surface RT-99.99°C
SCR-controlled plate heater
Resolution: 0.01°C
- Cold Surface Precision thermostatic bath
Heat Flux Range 0.5-2000 W/m²
Resolution: 0.25 W/m²
Heating Plate  
- Transfer Area 400 × 400 mm
- Adjustable Spacing 0-100 mm
Automation Computer-controlled testing
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Agent,Exporter,Seller

  • Year Established:

    2008

  • Total Annual:

    $5 million -$8 million

  • Employee Number:

    80~200

  • Ecer Certification:

    Verified Supplier

Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes... Dongguan Lonroy Equipment Co., Ltd, located in Dongguan, Guangdong,  is a leading company specializing in the research and development, manufacturing and sales of high-tech and high-precision testing equipment. With 20 years of industry experience, we are committed to providing excellent tes...

+ Read More

Get in touch with us

  • Reach Us
  • DONGGUAN LONROY EQUIPMENT CO LTD
  • A31, 11 Floor, No 1 Building, Minjian Jinrong Building, No 111 Guantai Road, Sanyuanli Community, Nancheng Street, Dongguan, Guangdong, China
  • https://www.lab-testmachines.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement