China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High
China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High

  1. China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High
  2. China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High
  3. China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High
  4. China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High
  5. China Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High

Alloy 800 Plate UNS N08800 Nickel-Iron-Chromium Superalloy ASTM B409 for High

  1. MOQ: Negotiable
  2. Price: Negotiable
  3. Get Latest Price
Supply Ability Negotiable
Width Range 1000mm - 2500mm
Max Service Temperature Up to 1500°F (816°C)
Packaging Details According to Customers' Requests
Thickness Range 3mm - 50mm+
Delivery Time 7 days for Sample Order
UNS Designation N08800 / N08810 / N08811
Length Range 2000mm - 6000mm
Melting Point 1357-1385°C
Density 8.0 g/cm³
Specification ASTM B409 / ASME SB-409
Material Grade Alloy 800 / 800H / 800HT
Payment Terms T/T
Certification ISO 9001:2015, PED 2014/68/EC, API 6A
Place of Origin Hunan, China
Model Number Alloy 800 / UNS N08800 / 1.4876
Brand Name DINGSCO

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Supply Ability Negotiable Width Range 1000mm - 2500mm
Max Service Temperature Up to 1500°F (816°C) Packaging Details According to Customers' Requests
Thickness Range 3mm - 50mm+ Delivery Time 7 days for Sample Order
UNS Designation N08800 / N08810 / N08811 Length Range 2000mm - 6000mm
Melting Point 1357-1385°C Density 8.0 g/cm³
Specification ASTM B409 / ASME SB-409 Material Grade Alloy 800 / 800H / 800HT
Payment Terms T/T Certification ISO 9001:2015, PED 2014/68/EC, API 6A
Place of Origin Hunan, China Model Number Alloy 800 / UNS N08800 / 1.4876
Brand Name DINGSCO
High Light Nickel-Iron-Chromium Superalloy ASTM B409 Certified ,Oxidation Carburization Corrosion Resistant Plate ,High-Temperature Service Up to 1500°F

1. Product Attributes

Material Grade Alloy 800 / 800H / 800HT
UNS Designation N08800 / N08810 / N08811
European Standard 1.4876 (X10NiCrAlTi32-21)
Japanese Standard NCF 800
Chinese Standard NS1101 / NS1102 / NS1103
Specification ASTM B409 / ASME SB-409
Product Form Plate / Sheet
Thickness Range 3mm – 50mm+
Width Range 1000mm – 2500mm
Length Range 2000mm – 6000mm
Surface Finish No.1, 2B, BA, Pickled, Polished
Brand DINGSCO

2. Material Overview

Alloy 800 (UNS N08800) is a nickel-iron-chromium superalloy engineered for exceptional performance in high-temperature environments. With a nominal composition of 30-35% Nickel, 19-23% Chromium, and a minimum of 39.5% Iron, this austenitic alloy delivers outstanding resistance to oxidation, carburization, and corrosion while maintaining structural stability under prolonged thermal exposure.

The alloy remains fully austenitic across its entire service range and resists sigma-phase embrittlement, making it a reliable choice for critical high-temperature components. Its balanced chemistry provides superior creep and stress-rupture properties compared to standard stainless steels.

Key Variants:

• Alloy 800 (UNS N08800): Optimized for general high-temperature applications where creep and rupture strength are not the primary design factors.

• Alloy 800H (UNS N08810): Features a restricted carbon range (0.05-0.10%) and high-temperature annealing for superior creep and stress-rupture properties.

• Alloy 800HT (UNS N08811): Further restricted in carbon, aluminum (0.25-0.60%), and titanium (0.25-0.60%) to maximize high-temperature creep resistance.

3. Chemical Composition

Element Incoloy 800 UNS N08800 (wt%)  Incoloy 800H  UNS N08810 (wt%) Incoloy 800HT UNS N08811 (wt%)
Nickel (Ni) 30.0 – 35.0 30.00 – 35.00 30.00 – 34.00
Chromium (Cr) 19.0 – 23.0 19.00 – 23.00 19.00 – 23.00
Iron (Fe) ≥ 39.5 (Balance) Balance Balance
Carbon (C) ≤ 0.10 ≤ 0.10 ≤ 0.12
Silicon (Si) ≤ 1.0 ≤ 1.00 ≤ 1.00
Manganese (Mn) ≤ 1.5 ≤ 1.50 ≤ 2.00
Aluminum (Al) 0.15 – 0.60 0.15 – 0.60 0.15 – 0.60
Titanium (Ti) 0.15 – 0.60 0.15 – 0.60 0.15 – 0.60
Copper (Cu) ≤ 0.75 ≤ 0.75 —
Phosphorus (P) — ≤ 0.030 ≤ 0.030
Sulfur (S) ≤ 0.015 ≤ 0.015 ≤ 0.015

4. Physical Properties

Property Value Unit
Density 8.0 g/cm³
Melting Point 1357 – 1385 °C
Specific Heat (at 20°C) 460 J/kg·K
Electrical Resistivity (at 20°C) 99 μΩ·cm
Thermal Conductivity (at 20°C) 12.6 W/m·K
Thermal Conductivity (at 100°C) 14.1 W/m·K
Thermal Conductivity (at 200°C) 16.1 W/m·K
Thermal Conductivity (at 500°C) 20.6 W/m·K
Thermal Conductivity (at 800°C) 25.1 W/m·K
Curie Point -115 °C
Magnetic Property Non-Magnetic —

5. Mechanical Properties

Property ASTM B409 (Room Temp.) JIS G4902
Yield Strength (YS, 0.2% Offset) ≥ 205 MPa (N/mm²) ≥ 205 N/mm²
Tensile Strength (TS) ≥ 520 MPa (N/mm²) ≥ 520 N/mm²
Elongation (EL) ≥ 30% ≥ 30%
Hardness (HV) — ≤ 182
Hardness (HB) — ≤ 179

High-Temperature Tensile Strength

Temperature (°C) Tensile Strength (MPa, Typical)
Room Temperature 552
200 485
400 445
600 390
700 245
800 155

6. Corrosion & Oxidation Resistance Comparison

Property Alloy 800 (UNS N08800) SUS 310S NAS 600 (Inconel 600)
Oxidation Resistance (up to 1000°C) Excellent — forms protective Cr₂O₃ scale Good — susceptible above 1050°C Excellent — comparable to Alloy 800
Carburization Resistance Excellent — high Ni content inhibits carbon diffusion Moderate Good
Nitric Acid Corrosion Good Good Good
Stress Corrosion Cracking (SCC) Superior — outperforms standard austenitic SS Moderate — susceptible in chloride environments Excellent
Molten Salt Corrosion Good Moderate Good
Sigma-Phase Embrittlement Resistant — does not precipitate σ phase during service Susceptible Resistant
Intergranular Attack Resistant with proper heat treatment Susceptible after sensitization Resistant

7. Material Characteristics

High-Temperature Strength

Maintains excellent mechanical integrity at elevated temperatures up to 816°C (1500°F). The austenitic structure remains stable without sigma-phase embrittlement even after prolonged exposure, ensuring long-term reliability in critical applications.

Oxidation Resistance

High nickel and chromium content promotes the formation of a protective chromium oxide (Cr₂O₃) scale at elevated temperatures. Oxidation resistance surpasses SUS 310S and approaches that of Inconel 600, particularly above 600°C.

Carburization Resistance

The high nickel content effectively inhibits carbon diffusion into the alloy matrix, preventing carburization-related embrittlement in hydrocarbon processing environments such as ethylene cracking and petrochemical reforming.

Corrosion Resistance

Exhibits good resistance to oxidizing corrosive media including nitric acid and nitric-sulfuric acid mixtures. Stress corrosion cracking resistance is significantly superior to standard austenitic stainless steels.

Weldability

Welds similarly to standard austenitic stainless steel. Compatible with TIG, MIG, and manual arc welding processes. Proper filler metal selection and post-weld heat treatment ensure optimal joint integrity.

Fabrication

Hot working temperature: 1000–1230°C. Simple forming can be performed below 850°C. Avoid the 650–850°C range to prevent cracking. Cold workability matches austenitic stainless steel with slightly lower work hardening characteristics.

Heat Treatment

• Annealing: 980–1100°C followed by rapid cooling

• Stress-Relieving: 780–870°C followed by air cooling

8. Product Image Display

 


9. Supply Forms

Form Specification Available Grades
Plates Thickness: 3mm – 50mm+ | Width: 1000mm – 2500mm | Length: 2000mm – 6000mm Alloy 800 / 800H / 800HT
Sheets Thickness: 0.5mm – 3mm | Width: 1000mm / 1219mm / 1500mm | Length: 2000mm / 2438mm / 3000mm Alloy 800 / 800H / 800HT
Strips / Coils Custom thickness and width per request Alloy 800 / 800H
Custom Cut Parts Water jet, laser, plasma cutting available Alloy 800 / 800H / 800HT

Surface Finishes Available: Hot Rolled (No.1), Cold Rolled (2B), Bright Annealed (BA), Pickled, Polished (180#, 320#, 400#, 600#)

10. Typical Applications

Heat Exchangers & Steam Generators

Tubing and plates for power plant superheaters, steam generator tubing, and high-temperature heat exchangers requiring long-term thermal stability.

Petrochemical & Refinery

Ethylene cracking furnace components, reformer tubes, process piping, and pressure vessels exposed to hydrocarbon streams at elevated temperatures.

Industrial Furnaces

Heat-treating baskets, trays, fixtures, muffles, and radiant tubes operating in carburizing or oxidizing atmospheres.

Nitric Acid Equipment

Condensers, heating coils, and storage vessels for nitric acid and nitric-sulfuric acid mixtures.

Thermocouple Protection Tubes

Sheathed heater outer tubes and thermocouple protection tubes for high-temperature measurement applications.

Heat Treatment Furnace Parts

Components requiring prolonged exposure to temperatures up to 1000°C with resistance to thermal cycling and oxidation.

11. DINGSCO — Professional Nickel Alloy Manufacturer

DINGSCO is a premier manufacturer and supplier of high-performance nickel alloy products, serving global industries with comprehensive material solutions.

Quality Assurance

Our mission is to provide our customers only with the best quality products. As an ISO 9001:2015, PED 2014/68/EC, and API 6A certified manufacturer, we enforce strict quality control at every production stage — from raw material sourcing to final inspection and certification.

ISO 9001:2015 PED 2014/68/EC API 6A


Science & Technology Innovation Strategy

We pay close attention to customer needs, implement product innovation, and leverage our comprehensive range of product types and material grades to provide customers with one-stop service. Continuous improvement drives our material research, process optimization, and equipment upgrades.

Cooperation

We are pleased to help others and glad to accept the hand of others. We actively participate in team collaboration and support decision-making. We share our experience with each other and excel at cooperating with different types of colleagues across the global supply chain.

12. Material Selection

Alloy UNS Key Feature Max Service Temp.
Alloy 800 N08800 General high-temp, oxidation & carburization resistant ~816°C (1500°F)
Alloy 800H N08810 Superior creep & stress-rupture properties ~870°C (1600°F)
Alloy 800HT N08811 Maximum creep resistance for critical applications ~870°C (1600°F)
Inconel 600 N06600 Excellent oxidation resistance, higher Ni content ~1093°C (2000°F)
Inconel 601 N06601 Superior oxidation resistance with Al addition ~1200°C (2190°F)
Incoloy 825 N08825 Enhanced corrosion resistance in reducing environments ~540°C (1000°F)

13. Customized Products

DINGSCO offers comprehensive customization services to meet your exact project specifications:

Custom Dimensions

Plates and sheets cut to your specified length, width, and thickness. Non-standard sizes available upon request with short lead times.

Custom Surface Finish

Choose from hot rolled, cold rolled, pickled, bright annealed, or polished finishes (up to mirror finish) to match your application requirements.

Custom Certification

Full material test certificates (MTC) to EN 10204 3.1 / 3.2. Additional NDT testing (UT, PT, RT) available per project requirements.

Value-Added Processing

Water jet cutting, laser cutting, plasma cutting, bevelling, drilling, and edge preparation services to reduce your downstream processing costs.


Payment & Shipping Terms

Minimum Order Quantity Negotiable
Price Negotiable
Packaging Details According to Customers' Requests
Delivery Time 7 days (Sample Order)
Payment Terms T/T
Supply Ability Negotiable

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Exporter,Seller

  • Year Established:

    1998

  • Total Annual:

    70 million-100 million

  • Employee Number:

    50~60

  • Ecer Certification:

    Verified Supplier

     Hunan Dinghan New Material Technology Co.,Ltd. (DINGSCO) specialized in Nickel Based Corrosion Resistant and High Temperature alloys products which used in the world’s most technically demanding industries and applications. We have complete advanced technology facilities t...      Hunan Dinghan New Material Technology Co.,Ltd. (DINGSCO) specialized in Nickel Based Corrosion Resistant and High Temperature alloys products which used in the world’s most technically demanding industries and applications. We have complete advanced technology facilities t...

+ Read More

Get in touch with us

  • Reach Us
  • Hunan Dinghan New Material Technology Co., LTD
  • No. 2319, Building 2, Dongfang Furong Garden, No. 582 Yuanda 1st Road, Hehuayuan Street,Furong District, Changsha, Hunan Province, China.
  • https://www.nickel-basedalloys.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement