UNS no. | N07818 |
Equal name | ATI 718Plus, Allvac 718Plus |
Spec | AMS 5441, AMS 5442 |
Avialable forms | ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings. |
Density | 8.25g/cm |
Brand Name | XUNSHI |
Model Number | N07818 |
Certification | ISO9001:2015 |
Place of Origin | China |
View Detail Information
Explore similar products
Electrode Melted Round Bar Nickel Inconel , PREP EIGA 3D Printing Inconel 939
Inconel 718 High Strength Nickel Alloy Corrosion Resistant Forged Round Bar
Thickness 0.04-2.0mm Inconel Nickel Alloy 718 Cold Rolled Strip ASTM B670 UNS
IN-738 Inconel High Temperature Nickel Alloys Hot Corrosion Resistance Round Bar
Product Specification
Payment Terms | T/T | Supply Ability | 5000kg per month |
Delivery Time | 45-60 days | Packaging Details | Plywood case |
UNS no. | N07818 | Equal name | ATI 718Plus, Allvac 718Plus |
Spec | AMS 5441, AMS 5442 | Avialable forms | ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings. |
Density | 8.25g/cm | Brand Name | XUNSHI |
Model Number | N07818 | Certification | ISO9001:2015 |
Place of Origin | China | ||
High Light | N07818 nickel superalloy ,AMS 5442 nickel superalloy ,nickel base superalloy |
Inconel 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the high temperature capability and thermal stability of Waspaloy alloy while retaining the processing characteristics of 718 alloy. It is double vacuum melted (VIM/ESR/VAR). This VIM/VAR process ensures excellent microcleanliness and tight compositional control. Triple melting, with electroslag remelting between the VIM and VAR operations, minimizes the possibility of macrosegregation, increases microcleanliness, and is preferred for premium quality jet engine rotating component applications. Inconel 718Plus alloy has at least a 100°F (55°C) operating temperature advantage over 718 alloy. 718Plus alloy also has advantages over Waspaloy and other higher temperature capable, nickel-base alloys due to its higher strength, superior formability, better wear resistance, and a resistance to weld cracking. 718Plus alloy is a lower cost option than Waspaloy or Rene 41 alloy due to its lower intrinsic raw materials cost and improved hot workability which provides higher material yields, resulting in a lower cost finished part.
Chemical composition
Element | C | Mn | Si | P | S | Cr | Ni | Mo | Nb | Ti | Al | Co | W | B | Cu | Pb | Bi | Se | Fe |
Weight(%) | 0.01-0.05 | 0.35 max | 0.35 max | 0.004-0.020 | 0.0025 max | 17.00-21.00 | Rem | 2.50-3.10 | 5.20-5.80 | 0.50-1.00 | 1.20-1.70 | 8.00-10.00 | 0.80-1.40 | 0.003-0.008 | 0.30 max | 0.0005 max | 0.00003 max | 0.0003 max | 8.00-10.00 |
Hardness
HRC 25 - 35(solution heat treated depending on quench rate)
HRC 42 - 48(fully aged condition)
Tensile Strength, Ultimate 1480 MPa
Application
These products have been typically used for parts requiring high resistance to creep and stress rupture up to 1400°F(760°C) and oxidation resistance up to 1800°F(982°C), but usage is not limited to such applications.
Available forms
718Plus alloy is available in all product forms: ingot, billet, block, forged round bar, hot-rolled shapes and rectangles, bar, rod, wire, plate, sheet, strip, and castings.
Company Details
Business Type:
Manufacturer
Year Established:
2015
Total Annual:
1000-1200
Employee Number:
100~120
Ecer Certification:
Verified Supplier
Suzhou Xunshi New Material Co., Ltd (refered as Xunshi afterwards) is a professional supplier of high performance alloys. Our factory is specialized in manufacturing Nickel alloys & Cobalt alloys for 10+ years,with a company mission to provide a high quality, reliable source for precision... Suzhou Xunshi New Material Co., Ltd (refered as Xunshi afterwards) is a professional supplier of high performance alloys. Our factory is specialized in manufacturing Nickel alloys & Cobalt alloys for 10+ years,with a company mission to provide a high quality, reliable source for precision...