China Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy
China Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

  1. China Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy
  2. China Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

Solid Solution Reinforced Nickel Based Superalloys , GH3536 Hastelloy X Alloy

  1. MOQ: 50kg
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms T/T
Supply Ability 1000kg per week
Delivery Time 30-35 days
Packaging Details Plywood case
Equal grades GH536, Hastelloy X, N06002
Melting range 1295°C~1381°C
Density 8.28g/cm3
Magnetic No
Forms of supply Plate, strip, tube, bar, forging, ring, casting
Product Name Nickel Cobalt Alloy
Brand Name XUNSHI
Model Number GH3536
Certification ISO9001
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 1000kg per week
Delivery Time 30-35 days Packaging Details Plywood case
Equal grades GH536, Hastelloy X, N06002 Melting range 1295°C~1381°C
Density 8.28g/cm3 Magnetic No
Forms of supply Plate, strip, tube, bar, forging, ring, casting Product Name Nickel Cobalt Alloy
Brand Name XUNSHI Model Number GH3536
Certification ISO9001 Place of Origin China
High Light nickel based alloys ,cobalt based alloy

GH3536 Nickel Based Solid Solution Reinforced Superalloy Hastelloy X

 

 

GH3536 is a Nickel Based Solid Solution Reinforced Superalloy. It is equal to Hastelloy X alloy.

It has good resistance to oxidation and corrosion resistance, under 900 ℃ have moderate to lasting and creep strength, cold and hot working good formability and weldability.

Applicable to the manufacture of aircraft engine combustion chamber components and other high temperature parts, use for a long time under 900 ℃, short-time working temperature of 1080 ℃. In 600 ~ 1200 ℃ high temperature can withstand the stress and resistance to oxidation and corrosion resistance of the alloy. The matrix elements can be divided into iron base superalloy, nickel base superalloy and cobalt base superalloy. According to the preparation process, it can be divided into deformation superalloy, casting superalloy and powder metallurgy superalloy. According to the reinforcement method, there are solid solution enhancement, precipitation enhancement, oxide dispersion enhancement and fiber enhancement (see metal enhancement). High temperature components such as turbine blades, guide blades, turbine discs, high-pressure compressors and combustors for aerospace, naval vessels and industrial gas turbines. It is also used in the manufacture of energy conversion devices such as space vehicles, rocket engines, nuclear reactors, petrochemical equipment and coal conversion

 

Chemical composition

 

Element C Cr Ni Co W Mo Al Ti
Weight(%) 0.05~0.15 20.50~23.00 Rem 0.50~2.50 0.20~1.00 8.00~10.00 0.50 max 0.15 max
Element Fe B Mn Si P S Cu  
Weight(%) 17.00~20.00 0.010 max 1.00 max 1.00 max 0.025 max 0.015 max 0.500 max  

 

Characters of GH3536

  •  Good workability.
  •  At 900 ℃ with medium of lasting and creep strength.
  •  Good oxidation resistance and corrosion resistance.
  •  Suitable for application in a long time of aircraft engine combustor under 900 ℃ and reheater components.
  •  Good welding performance and cold and hot working formability.

Application of GH3536

  •  Industrial and aircraft steam turbine (burner, rectifier, structural cover)
  •  Industrial furnace components, supporting roller, grid plate, ribbon and radiation pipe
  •  Spiral pipes in a petrochemical furnace
  •  High temperature gas cools the nuclear reactor 

Forms and sizes of supply

Plate 0.50~4.0mm

Strip: 0.05~0.80mm

Tube: diameter 4~20mm, wall thickness 1.0~2.0mm

Wire: diameter 0.20~10.00mm

Bar: diameter upto 300mm

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2015

  • Total Annual:

    1000-1200

  • Employee Number:

    100~120

  • Ecer Certification:

    Verified Supplier

Suzhou Xunshi New Material Co., Ltd (refered as Xunshi afterwards) is a professional supplier of high performance alloys. Our factory is specialized in manufacturing Nickel alloys & Cobalt alloys for 10+ years,with a company mission to provide a high quality, reliable source for precision... Suzhou Xunshi New Material Co., Ltd (refered as Xunshi afterwards) is a professional supplier of high performance alloys. Our factory is specialized in manufacturing Nickel alloys & Cobalt alloys for 10+ years,with a company mission to provide a high quality, reliable source for precision...

+ Read More

Get in touch with us

  • Reach Us
  • Suzhou Xunshi New Material Co., Ltd
  • Room E-407, No.2, XugongQiao Road, Kunshan City, Jiangsu, 215332 China
  • https://www.nickel-cobaltalloy.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement