| Heattreatment | Solution annealing and aging |
| Type | Bolts |
| Quality Control | 100% Inspected |
| Standard | ASTM B392 |
| Appearance | Silvery |
| Hardness | HRC 40 - 60 |
| Usage | Oil and Gas Industry |
| Use | Ore Mining |
| Payment Terms | by T/T or L/C, Western Union |
| Supply Ability | 100,000,000.00 |
| Delivery Time | It depends on the quantity to be ordered. |
| Packaging Details | Pallets |
| Wearresistance | High |
| Thermalconductivity | 15 - 25 W/m·K |
| Drawing Made | accept |
| Service | OEM\ODM |
| Shape | Irregular Shape/Spherical Powder |
| Grade | cobalt alloy 21 |
| Castingmethod | Investment casting, sand casting |
| Material Grade | cobalt alloy 1, cobalt alloy 3, |
| Hardness Temperature | Up to 1200 Centi-degree |
| Coating Process | SPF Coating,overlay process |
| Cast Process | Wax Lost Process |
| Surface Treatment | Shot Blast |
| Brand Name | Eternal Bliss |
| Model Number | EB26078 |
| Certification | ISO9001-2008 |
| Place of Origin | China |
View Detail Information
Explore similar products
EB Investment Cobalt Chrome Lost Wax Casting Australian Metal Parts
Industrial Rolled TA2 TA1 Titanium Foil Metal Coil Raw Materials for Thermos Cup
TA1 corrosion resistant titanium coil, stretched material 0.1 0.2 0.3 0.4 0.5mm
Titanium foil manufacturers spot sponge titanium pure titanium titanium foil
Product Specification
| Heattreatment | Solution annealing and aging | Type | Bolts |
| Quality Control | 100% Inspected | Standard | ASTM B392 |
| Appearance | Silvery | Hardness | HRC 40 - 60 |
| Usage | Oil and Gas Industry | Use | Ore Mining |
| Payment Terms | by T/T or L/C, Western Union | Supply Ability | 100,000,000.00 |
| Delivery Time | It depends on the quantity to be ordered. | Packaging Details | Pallets |
| Wearresistance | High | Thermalconductivity | 15 - 25 W/m·K |
| Drawing Made | accept | Service | OEM\ODM |
| Shape | Irregular Shape/Spherical Powder | Grade | cobalt alloy 21 |
| Castingmethod | Investment casting, sand casting | Material Grade | cobalt alloy 1, cobalt alloy 3, |
| Hardness Temperature | Up to 1200 Centi-degree | Coating Process | SPF Coating,overlay process |
| Cast Process | Wax Lost Process | Surface Treatment | Shot Blast |
| Brand Name | Eternal Bliss | Model Number | EB26078 |
| Certification | ISO9001-2008 | Place of Origin | China |
| High Light | precision steel casting ,cast cobalt alloys | ||
Precision investment casting services for a variety of high temperature super alloys cobalt-based types.
Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.
We produce High Temperature Superalloy Castings Parts with precision investment process.
Table 1 : Standard Cobalt cobalt alloy Alloy
| Co | Cr | C | W | Mo | Ni | Si | B | Fe | Mn | Others | |
| cobalt alloy 1 | BAL | 33 | 2.45 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
| cobalt alloy 3 | BAL | 31 | 2.5 | 13 | - | 2.5* | 1 | - | 2.5* | 1 | - |
| cobalt alloy 4 | BAL | 31.5 | 1 | 14 | - | 2.0* | 1 | - | 2.0* | 1 | - |
| BAL | 28 | 1.2 | 5 | - | 3.0* | 1 | - | 2.5* | 1 | - | |
| cobalt alloy 12 | BAL | 29 | 1.85 | 9 | - | 2.5* | 1 | - | 2.5* | 1 | - |
| cobalt alloy 20 | BAL | 33 | 2.45 | 17.5 | - | 2.5* | 1 | - | 2.5* | 1 | - |
| cobalt alloy 21 | BAL | 27 | 0.25 | - | 5.5 | 2.5* | 1 | - | 3.0* | 1 | - |
| cobalt alloy 31 | BAL | 26 | 0.5 | 7.5 | - | 10.5 | 1 | - | 2.0* | 1 | - |
| cobalt alloy 190 | BAL | 26 | 3.3 | 14 | - | 1.0 | 1 | - | 8.0 | 0.5 | - |
| cobalt alloy 238 | BAL | 26 | 0.1 | - | 3 | - | 1 | - | 20.0 | 1 | - |
| cobalt alloy 306 | BAL | 25 | 0.4 | 2 | - | 6.0 | 1 | - | 4.0* | 1 | Nb=5 |
| 94 | BAL | 28 | 1 | 19 | - | 5.0 | 1 | - | 2.5* | 1 | V=1 |
| cobalt alloy F | BAL | 25.5 | 1.75 | 12.25 | - | 22.5 | 1 | - | 1.5* | - | - |
| cobalt alloy SF1 | BAL | 19 | 1.3 | 13 | - | 13 | 3 | 2.5 | 3* | 0.5 | Cu=0.5 |
| cobalt alloy SF6 | BAL | 19 | 0.7 | 7 | - | 13 | 2.5 | 1.7 | 3* | 0.5 | Cu=0.5 |
| cobalt alloy SF12 | BAL | 19 | 1 | 9 | - | 13 | 3 | 2 | 3* | 0.5 | Cu=0.5 |
| cobalt alloy SF20 | BAL | 19 | 1.5 | 15 | - | 13 | 3 | 3 | 2* | 0.5 | Cu=0.5 |
| TRIBALOY T400 | BAL | 8 | 0.1* | - | 28 | 3* | 2.4 | - | 3* | - | - |
| TRIBALOY T800 | BAL | 17 | 0.1* | - | 28 | 3* | 3.2 | - | 3* | - | - |
| DELORO 15 | - | - | 0.06* | - | - | BAL | 2.0 | 1.05 | 1.5* | 20 | Cu=20 |
| DELORO 22 | - | 0.70 | 0.10 | - | - | BAL | 2.3 | 1.75 | - | - | - |
| DELORO 40 | - | 7.0 | 0.10 | - | - | BAL | 3.5 | 2.25 | - | - | - |
| DELORO 50 | - | 10.25 | 0.45 | - | - | BAL | 4.0 | 1.85 | 4.0 | - | - |
| DELORO 60 | - | 14.25 | 0.6 | - | - | BAL | 2.0 | 3.5 | 4.0 | - | - |
| DELORO 625 | - | 22 | 0.1 | - | 9 | BAL | - | - | 5 | - | - |
| NISTELLE C | - | 16.5 | 0.12* | 4.5 | 17 | BAL | 0.7 | - | 6.0 | - | - |
| TRIBALOY T700 | - | 15 | 0.10* | - | 32 | BAL | 3.25 | - |
| Hastelloy C22®(UNS N06022)(Max.) | ||||||||||||
| C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
| 0.015 | 0.5 | 0.02 | 0.02 | 0.08 | 20.0-22.5 | Bal. | 12.5-14.5 | 2.5 | 2.0-6.0 | 2.5-3.5 | 0.35 | |
| Hastelloy C276®(UNS N10276)(Max.) | ||||||||||||
| C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | V | |
| 0.01 | 1 | 0.04 | 0.03 | 0.08 | 14.5-16.5 | Bal. | 15.0-17.0 | 2.5 | 4.0-7.0 | 3.0-4.5 | 0.35 | |
| Hastelloyx®(UNS N06002)(Max.) | ||||||||||||
| C | MN | P | S | Si | Cr | Ni | Mo | CO | Fe | W | other | |
| 0.05-0.15 | 1 | 0.04 | 0.03 | 1 | 20.5-23.0 | Bal. | 8.0-10.0 | 0.5-2.5 | 17.0-20.0 | 0.2-1.0 | / | |
| Monel 400®(UNS NO4400) (Max.) |
||||||||||||
| C | MN | S | Si | Ni | Cu | Fe | ||||||
| 0.3 | 2 | 0.024 | 0.5 | 63 min | 28-34 | 2.5 | ||||||
| Monel M400®(UNS NO4400)(Max.) |
||||||||||||
| C | MN | S | Si | Ni | Cu | Fe | ||||||
| 0.3 | 2 | 0.024 | 0.5 | 63-70 | 28-34 | 2.5 | ||||||
| Monel R405®(UNS NO4405)(Max.) |
||||||||||||
| C | MN | S | Si | Ni | Cu | Fe | ||||||
| 0.3 | 2 | 0.025-0.06 | 0.5 | 63.0min | 28-34 | 2.5 | ||||||
| Monel K500®(UNS NO5500)(Max.) |
||||||||||||
| C | MN | S | Si | Ni | Cu | Ti | AI | Fe | ||||
| 0.1 | 2 | 0.01 | 0.5 | 63min | 27-33 | 0.86 | 2.3-3.15 | 2 | ||||
| Inconel 600(UNS NO6600)(Max.) | ||||||||||||
| C | MN | S | Si | Cr | Ni | Cu | Fe | |||||
| 0.15 | 1 | 0.015 | 0.5 | 14-17 | 72 min | 0.5 | 6.0-10.0 | |||||
| Inconel 601(UNS NO6601)(Max.) | ||||||||||||
| C | MN | Si | Cr | Ni | CO | AI | Fe | |||||
| 0.05 | 0.3 | 0.2 | 22.5 | 61.5min | 5 | 1.4 | 14.1 | |||||
| Inconel 718(UNS NO7718)(Max.) | ||||||||||||
| Cr | Ni | Mo | CO | Cb+Ta | Ti | AI | Fe | |||||
| 19 | 52.5min | 3.05 | 5 | 5.13 | 0.9 | 0.5 | 18.5 | |||||
| Chemical Analysis of Incoloy 800® uns(N08800) | ||||||||||||
| C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
| 0.1 max | 19.0-23.0 | 30.0-35.0 | 0.15-0.6 | 0.15-0.6 | 39.5min | / | ||||||
| Incoloy800H® UNS(N08810) | ||||||||||||
| C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
| 0.05-0.1 | 19.0-23.0 | 30.0-35.0 | 0.15-0.60 | 0.15-0.60 | 39.5min | 5or coarser | ||||||
| Incoloy800HT® UNS(N08811) | ||||||||||||
| C | Cr | Ni | Ti | AI | Fe | Grain | ||||||
| 0.06-0.10 | 19.0-23.0 | 30.0-35.0 | 0.25-0.60 | 0.25-0.60 | 39.5min | 5or coarser | ||||||
|
Dimensions:as per drawings
|
||||||||||||
Step 1: Getting orders.
Step 2: Process design by technical department
Step 3: Purchase of raw materials and pattern making &checking
Step 4: Inspection of raw materials
Step 5: Melting by middle-frequency induction furnaces
Step 6: Ladle analysis by Spectrometer
Step 7: De-oxidization, slag-removal, tapping
Step 8: Pouring
Step 9: Openning & fettling
Step 10: Surface & dimensional check
Step 11: Heat treatment
Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)
Step 13: Packing
Step 14: Shipping
![]()
1. 16-year Foundry Operation Experience.
2. Friendly & High Efficient Technical & Commercial Communication.
3. Professional Export Practices: Have Exported to +60 Overseas Countries.
Our Trade Show ![]()
Our booth No. 14-A29-5 in Newcast 2015,Germany
Hall 14, Stand No.A29-5.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company,Seller
Year Established:
2013
Total Annual:
3000000-6000000
Ecer Certification:
Verified Supplier
EB China makes metal better. EB China is a professional manufacturer of high alloy castings and forgings with 22-year history. Our main products include corrosion, wear & heat-resistant castings & forgings. Our foundry & forging plant have passed ISO9001,ISO14001,ISO45001 Management Syst... EB China makes metal better. EB China is a professional manufacturer of high alloy castings and forgings with 22-year history. Our main products include corrosion, wear & heat-resistant castings & forgings. Our foundry & forging plant have passed ISO9001,ISO14001,ISO45001 Management Syst...
Get in touch with us
Leave a Message, we will call you back quickly!