China factories

China factory - Eternal Bliss Alloy Casting & Forging Co.,LTD.

Eternal Bliss Alloy Casting & Forging Co.,LTD.

  • China,Wuxi ,Jiangsu
  • Verified Supplier

Leave a Message

we will call you back quickly!

Submit Requirement
China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

  1. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  2. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  3. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  4. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  5. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
  6. China Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

  1. MOQ: 30 kg
  2. Price: USD80/kg ~ USD120/kg
  3. Get Latest Price
Heattreatment Solution annealing and aging
Type Bolts
Quality Control 100% Inspected
Standard ASTM B392
Appearance Silvery
Hardness HRC 40 - 60
Usage Oil and Gas Industry
Use Ore Mining
Payment Terms by T/T or L/C, Western Union
Supply Ability 100,000,000.00
Delivery Time It depends on the quantity to be ordered.
Packaging Details Pallets
Wearresistance High
Thermalconductivity 15 - 25 W/m·K
Drawing Made accept
Service OEM\ODM
Shape Irregular Shape/Spherical Powder
Grade cobalt alloy 21
Castingmethod Investment casting, sand casting
Material Grade cobalt alloy 1, cobalt alloy 3,
Hardness Temperature Up to 1200 Centi-degree
Coating Process SPF Coating,overlay process
Cast Process Wax Lost Process
Surface Treatment Shot Blast
Brand Name Eternal Bliss
Model Number EB26078
Certification ISO9001-2008
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Heattreatment Solution annealing and aging Type Bolts
Quality Control 100% Inspected Standard ASTM B392
Appearance Silvery Hardness HRC 40 - 60
Usage Oil and Gas Industry Use Ore Mining
Payment Terms by T/T or L/C, Western Union Supply Ability 100,000,000.00
Delivery Time It depends on the quantity to be ordered. Packaging Details Pallets
Wearresistance High Thermalconductivity 15 - 25 W/m·K
Drawing Made accept Service OEM\ODM
Shape Irregular Shape/Spherical Powder Grade cobalt alloy 21
Castingmethod Investment casting, sand casting Material Grade cobalt alloy 1, cobalt alloy 3,
Hardness Temperature Up to 1200 Centi-degree Coating Process SPF Coating,overlay process
Cast Process Wax Lost Process Surface Treatment Shot Blast
Brand Name Eternal Bliss Model Number EB26078
Certification ISO9001-2008 Place of Origin China
High Light precision steel casting ,cast cobalt alloys

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

.

 

Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.

 

We produce High Temperature Superalloy Castings Parts with precision investment process.

 

Table 1 : Standard Cobalt cobalt alloy Alloy 

  Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -      
  Hastelloy C22®(UNS N06022)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
  Hastelloy C276®(UNS N10276)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W V
  0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
  Hastelloyx®(UNS N06002)(Max.)
  C MN P S Si Cr Ni Mo CO Fe W other
  0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
  Monel 400®(UNS NO4400) (Max.)  
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63 min 28-34 2.5
  Monel M400®(UNS NO4400)(Max.)
  C MN S Si Ni Cu Fe
  0.3 2 0.024 0.5 63-70 28-34 2.5
  Monel R405®(UNS NO4405)(Max.)
  C MN S Si Ni Cu Fe
  0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
  Monel K500®(UNS NO5500)(Max.)  
  C MN S Si Ni Cu Ti AI Fe
  0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
  Inconel 600(UNS NO6600)(Max.)  
  C MN S Si Cr Ni Cu Fe  
  0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
  Inconel 601(UNS NO6601)(Max.)
  C MN Si Cr Ni CO AI Fe
  0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
  Inconel 718(UNS NO7718)(Max.)
  Cr Ni Mo CO Cb+Ta Ti AI Fe
  19 52.5min 3.05 5 5.13 0.9 0.5 18.5
  Chemical Analysis of Incoloy 800® uns(N08800)  
  C Cr Ni Ti AI Fe Grain
  0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
  Incoloy800H® UNS(N08810)
  C Cr Ni Ti AI Fe Grain
  0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
  Incoloy800HT® UNS(N08811)
  C Cr Ni Ti AI Fe Grain
  0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

 

Dimensions:as per drawings

 

 

Production Process

Step 1: Getting orders.

 

Step 2: Process design by technical department

 

Step 3: Purchase of raw materials and pattern making &checking

 

Step 4: Inspection of raw materials

 

Step 5: Melting by middle-frequency induction furnaces

 

Step 6: Ladle analysis by Spectrometer

 

Step 7: De-oxidization, slag-removal, tapping

 

Step 8: Pouring

 

Step 9: Openning & fettling

 

Step 10: Surface & dimensional check

 

Step 11: Heat treatment

 

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

 

Step 13: Packing

 

Step 14: Shipping

 

 

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.

 

 

Our Trade Show

 

Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.

 

 

Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

www.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.
 
 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company,Seller

  • Year Established:

    2013

  • Total Annual:

    3000000-6000000

  • Ecer Certification:

    Verified Supplier

EB China makes metal better. EB China is a professional manufacturer of high alloy castings and forgings with 22-year history. Our main products include corrosion, wear & heat-resistant castings & forgings. Our foundry & forging plant have passed ISO9001,ISO14001,ISO45001 Management Syst... EB China makes metal better. EB China is a professional manufacturer of high alloy castings and forgings with 22-year history. Our main products include corrosion, wear & heat-resistant castings & forgings. Our foundry & forging plant have passed ISO9001,ISO14001,ISO45001 Management Syst...

+ Read More

Get in touch with us

  • Reach Us
  • Eternal Bliss Alloy Casting & Forging Co.,LTD.
  • 1099 Xinhua Road,214104, Xishan District, Wuxi, Jiangsu,China
  • https://www.ebcastings.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement