China Inconel 625 Welding Wire (Ni-Cr-Mo Superalloy) ERNiCrMo-3 Filler Metal for High
China Inconel 625 Welding Wire (Ni-Cr-Mo Superalloy) ERNiCrMo-3 Filler Metal for High

  1. China Inconel 625 Welding Wire (Ni-Cr-Mo Superalloy) ERNiCrMo-3 Filler Metal for High

Inconel 625 Welding Wire (Ni-Cr-Mo Superalloy) ERNiCrMo-3 Filler Metal for High

  1. MOQ: 15kg
  2. Price: 26-35
  3. Get Latest Price
Payment Terms T/T
Supply Ability 40–60 tons/month
Delivery Time 3–7 days (standard sizes)
Packaging Details Spool Wire / Rod Form
Process Compatibility MIG / TIG / SAW / Arc Spray / Flame Spray
Working Temperature Up to 1000°C
Mechanical Strength High (Suitable for load & thermal cycling)
Corrosion Resistance Excellent, incl. Chlorides & Oxidizing chemicals
Condition Spool Wire / Rod Form
Spool Weight 1kg / 5kg / 15kg / Custom
Supply Capacity 40–60 tons/month
Lead Time 3–7 days (standard sizes)
Brand Name HUONA
Model Number WIRE
Certification SGS
Place of Origin CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 40–60 tons/month
Delivery Time 3–7 days (standard sizes) Packaging Details Spool Wire / Rod Form
Process Compatibility MIG / TIG / SAW / Arc Spray / Flame Spray Working Temperature Up to 1000°C
Mechanical Strength High (Suitable for load & thermal cycling) Corrosion Resistance Excellent, incl. Chlorides & Oxidizing chemicals
Condition Spool Wire / Rod Form Spool Weight 1kg / 5kg / 15kg / Custom
Supply Capacity 40–60 tons/month Lead Time 3–7 days (standard sizes)
Brand Name HUONA Model Number WIRE
Certification SGS Place of Origin CHINA
High Light Inconel 625 ERNiCrMo-3 Thermal Spray Wire ,NiCrMo Superalloy Coating Material ,High Temperature Corrosion Resistant Wire

Inconel 625 Welding Wire (Ni-Cr-Mo Superalloy)

ERNiCrMo-3 Filler Metal for High-Temperature & Corrosion-Resistant Welding
Available Diameters: 1.0 mm / 1.2 mm / 1.6 mm


Product Overview

Inconel 625 welding wire (ERNiCrMo-3) is a nickel-chromium-molybdenum-niobium superalloy filler metal.
It provides exceptional resistance to high-temperature oxidation, seawater corrosion, chloride pitting, crevice corrosion, and stress-corrosion cracking.

Commonly used for joining and overlaying Ni-based alloys, stainless steels, and dissimilar metals in chemical processing, marine, aerospace, energy and offshore equipment.


Chemical Composition (Typical)

Element Content (%)
Nickel (Ni) Balance
Chromium (Cr) 20.0 – 23.0
Molybdenum (Mo) 8.0 – 10.0
Niobium + Tantalum (Nb+Ta) 3.15 – 4.15
Iron (Fe) ≤ 5.0
Others Trace

Conforms to: ASTM / AWS ERNiCrMo-3 (Inconel 625)


Key Features

  • Excellent corrosion resistance in seawater, acids, and chloride media

  • High temperature strength & oxidation stability up to ~980°C

  • Crack-resistant welds with strong metallurgical bonding

  • Suitable for dissimilar metal welding (Ni-base ↔ stainless steel)

  • Smooth feeding & stable arc characteristics


Application Areas

  • Chemical & Petrochemical: Heat exchangers, reactors, pipelines

  • Marine & Offshore: Pump shafts, seawater system components

  • Aerospace: Engine components, exhaust systems

  • Nuclear & Power Generation: Boiler tubing, overlay protection

  • Repair & Overlay Cladding: Wear + corrosion protective surfacing


Technical Specifications

Item Value
Alloy Grade Inconel 625
AWS Grade ERNiCrMo-3
Material Type Ni-Cr-Mo-Nb Superalloy
Main Diameters (主推) 1.0 mm / 1.2 mm / 1.6 mm
Other Diameters 2.0 / 2.4 / 3.2 mm on request
Form Spool Wire / Straight Rod
Welding Processes TIG / MIG / SAW / Arc Spray / Flame Spray
Service Temperature Up to ~980°C
Coating Appearance (Sprayed) Dense silver-gray metallic finish

Packaging & Supply

  • Spools: 1kg / 5kg / 15kg / 20kg

  • Rods: 5kg per plastic tube

  • OEM & private label branding available

  • Export pallet packing available

Stock: Regular inventory available
Capacity: ~40–60 tons/month
Lead Time: 3–7 days (standard) | 10–15 days (custom)


Custom Attributes (可直接复制到环球广贸 / 阿里后台)

Attribute Name Attribute Value
Product Name Inconel 625 Welding Wire
AWS Grade ERNiCrMo-3
Alloy Type Ni-Cr-Mo-Nb Superalloy
Main Diameters 1.0 mm / 1.2 mm / 1.6 mm
Wire Form Spool / Rod
Welding Methods TIG / MIG / SAW / Arc Spray / Flame Spray
Temperature Resistance Up to ~980°C
Corrosion Resistance Excellent in seawater & chloride media
Packaging Spool / Tube / Carton / Pallet
Monthly Supply 40–60 tons
Origin China


6j13 Electric Resistance Alloy, Manganin Strip for Shunt
6j13 Electric Resistance Alloy, Manganin Strip for Shunt
6j13 Electric Resistance Alloy, Manganin Strip for Shunt
6j13 Electric Resistance Alloy, Manganin Strip for Shunt
6j13 Electric Resistance Alloy, Manganin Strip for Shunt

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Exporter

  • Year Established:

    2008

  • Total Annual:

    8000000-100000000

  • Employee Number:

    100~120

  • Ecer Certification:

    Verified Supplier

Huona (Shanghai) New Material Co., Ltd. Was established in 2008, currently have three divisions: Magnesium Division, Thermal Spray Division and Functional Material Division.Magnesium Division produces magnesium metal products. Various models of high-quality magnesium alloy plate, magnesium rods, hig... Huona (Shanghai) New Material Co., Ltd. Was established in 2008, currently have three divisions: Magnesium Division, Thermal Spray Division and Functional Material Division.Magnesium Division produces magnesium metal products. Various models of high-quality magnesium alloy plate, magnesium rods, hig...

+ Read More

Get in touch with us

  • Reach Us
  • Huona (Shanghai) New Material Co., Ltd.
  • 1900 Mudanjiang Road, Baoshan District, 201999, Shanghai, China
  • https://www.nicralloy.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement