China Inconel 617 Superalloy Oxidation Resistant Plate For Petrochemical Reactors
China Inconel 617 Superalloy Oxidation Resistant Plate For Petrochemical Reactors

  1. China Inconel 617 Superalloy Oxidation Resistant Plate For Petrochemical Reactors

Inconel 617 Superalloy Oxidation Resistant Plate For Petrochemical Reactors

  1. MOQ: 150kgs
  2. Price: Negotiatable
  3. Get Latest Price
Payment Terms ,L/C,T/T,Western Union,MoneyGram
Supply Ability 300 Ton per Month
Delivery Time 2-30days
Packaging Details Wood box for Rod
Heat Treatment Annealing
Application Heat Exchanger
Advantage Fast Delivery Time
Surface Finish Solid solution + acid white
Place Of Orig China
Surface Treatment Anodized,Brushed,Mill Finished,Polished
Condition Hard / Soft
Yield Strength 240 MPa
Business Type Manufaturer
Grade Inconel 617 / UNS N07617 / W.Nr.2.4663
Width As Your Request
Finish Condition Soft ,anneled
Thermal Expansion 13-17 µm/mK
Density 8.36Mg/㎡
Melting Range 1332-1380
Electrical Resistivity 1.22µΩ-m (26°C)
Brand Name NikTech
Model Number Inconel 617
Certification ISO 9001:2008
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms ,L/C,T/T,Western Union,MoneyGram Supply Ability 300 Ton per Month
Delivery Time 2-30days Packaging Details Wood box for Rod
Heat Treatment Annealing Application Heat Exchanger
Advantage Fast Delivery Time Surface Finish Solid solution + acid white
Place Of Orig China Surface Treatment Anodized,Brushed,Mill Finished,Polished
Condition Hard / Soft Yield Strength 240 MPa
Business Type Manufaturer Grade Inconel 617 / UNS N07617 / W.Nr.2.4663
Width As Your Request Finish Condition Soft ,anneled
Thermal Expansion 13-17 µm/mK Density 8.36Mg/㎡
Melting Range 1332-1380 Electrical Resistivity 1.22µΩ-m (26°C)
Brand Name NikTech Model Number Inconel 617
Certification ISO 9001:2008 Place of Origin China
High Light inconel 617 plate ,Heat Exchanger inconel 617 plate ,Petrochemical Reactors inconel material

Inconel 617 (NiCr23Co12Mo) Superalloy | Oxidation-Resistant Plates for Petrochemical Reactors | Custom Machining Available

 

Inconel 617 rods are engineered to deliver exceptional performance in high-temperature and corrosive environments. This nickel-chromium-cobalt-molybdenum alloy offers a superior combination of strength, oxidation resistance, and metallurgical stability, making it an ideal choice for demanding industrial applications.

 

Chemical Composition of Inconel 617 Rods

The precise chemical composition of Inconel 617 contributes to its outstanding properties:​

Element Composition (%)
Nickel (Ni) 44.5 min
Chromium (Cr) 20.0–24.0
Cobalt (Co) 10.0–15.0
Molybdenum (Mo) 8.0–10.0
Aluminum (Al) 0.8–1.5
Carbon (C) 0.05–0.15
Iron (Fe) 3.0 max
Manganese (Mn) 1.0 max
Silicon (Si) 1.0 max
Sulfur (S) 0.015 max
Titanium (Ti) 0.6 max
Copper (Cu) 0.5 max
Boron (B) 0.006 max

 

 

Mechanical Properties of Inconel 617 Rods

Inconel 617 rods exhibit impressive mechanical properties:​

Property Value
Tensile Strength 106.5 ksi (734 MPa)
Yield Strength (0.2%) 46.3 ksi (319 MPa)
Elongation 68%
Hardness (Brinell) 172

 

Physical Properties of Inconel 617 Rods

The physical characteristics of Inconel 617 include:​

Property Value
Density 0.302 lb/in³
Melting Range 2430-2510°F

 

 

Applications of Inconel 617 Rods

Due to their robust properties, Inconel 617 rods are utilized in various high-demand sectors:​

  • Aerospace: Components such as combustion cans and transition liners in gas turbines.​

  • Power Generation: High-temperature components in both fossil-fueled and nuclear power plants

  • Chemical Processing: Catalyst-grid supports in nitric acid production and heat-treating baskets.​

  • Metal Refining: Reduction boats in molybdenum refining.​

​Source: Special Metals Corporation

Frequently Asked Questions (FAQs)

Q: What makes Inconel 617 rods suitable for high-temperature applications?

A: The alloy's high nickel and chromium content provides exceptional oxidation resistance, while cobalt and molybdenum contribute to its high-temperature strength.​

Q: Can Inconel 617 rods be welded?

A: Yes, Inconel 617 rods can be readily welded using conventional techniques, ensuring ease of fabrication.​

Q: Are Inconel 617 rods resistant to corrosion?

A: Absolutely. The alloy exhibits excellent resistance to a wide range of corrosive environments, making it ideal for chemical processing applications.​

Q: What forms are Inconel 617 rods available in?

A: Inconel 617 is available in various forms, including rods, sheets, plates, and tubes, catering to diverse industrial requirements.​

Q: How does Inconel 617 compare to other high-temperature alloys?

A: Inconel 617 offers a unique combination of strength, oxidation resistance, and metallurgical stability, distinguishing it from other high-temperature alloys.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2002

  • Total Annual:

    20000000-80000000

  • Employee Number:

    50~500

  • Ecer Certification:

    Verified Supplier

Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys... Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys...

+ Read More

Get in touch with us

  • Reach Us
  • Wuxi Nickel New Material Co., Ltd
  • Xinwu District, Wuxi City, Jiangsu Province
  • https://www.niktechmaterial.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement