| Payment Terms | L/C,T/T,Western Union,MoneyGram |
| Supply Ability | 300 Ton per Month |
| Delivery Time | 2-30days |
| Packaging Details | Wooden Case |
| Special Use | Compressor disks,machine manufacturing |
| Alloy Type | Ni-Cu Alloy |
| Wire Gauge | 0-5, 15-20 |
| Corrosion Resistance | Excellent |
| Shape | Wire,Strip,Rod,Tube,Plate |
| Melting Point | 1300-1350°C |
| Quality Test | MTC (mill Test Certification) |
| Electrical Resistivity | 0.66 µΩ·m (at 20°C) |
| Alloys | Monel Alloy Wire |
| Thermal Stability | Excellent |
| Diameter | 0.02 - 1 Mm, 1-3 Mm, 5-7 Mm |
| Dia | 0.6mm,0.8mm,0.9mm,1.0mm,1.2mm,1.6mm |
| Width | As Your Request |
| Brand Name | NikTech |
| Model Number | Incoloy 825 |
| Certification | ISO 9001:2008 |
| Place of Origin | China |
View Detail Information
Explore similar products
Corrosion Resistant Alloy Incoloy 825 Strip For Extreme Environments
High Temperature Corrosion Resistance Incoloy 825 Rod For Chemical Processing
Incoloy 800 Strip High Temperature Strength Oxidation Carburization Resistance
High Temperature Resistant Incoloy 800H/HT Plate ASTM B409 For Heat Treatment
Product Specification
| Payment Terms | L/C,T/T,Western Union,MoneyGram | Supply Ability | 300 Ton per Month |
| Delivery Time | 2-30days | Packaging Details | Wooden Case |
| Special Use | Compressor disks,machine manufacturing | Alloy Type | Ni-Cu Alloy |
| Wire Gauge | 0-5, 15-20 | Corrosion Resistance | Excellent |
| Shape | Wire,Strip,Rod,Tube,Plate | Melting Point | 1300-1350°C |
| Quality Test | MTC (mill Test Certification) | Electrical Resistivity | 0.66 µΩ·m (at 20°C) |
| Alloys | Monel Alloy Wire | Thermal Stability | Excellent |
| Diameter | 0.02 - 1 Mm, 1-3 Mm, 5-7 Mm | Dia | 0.6mm,0.8mm,0.9mm,1.0mm,1.2mm,1.6mm |
| Width | As Your Request | Brand Name | NikTech |
| Model Number | Incoloy 825 | Certification | ISO 9001:2008 |
| Place of Origin | China | ||
| High Light | 0.6mm incoloy 825 ,0.9mm incoloy 825 ,0.8mm alloy 825 material | ||
Incoloy 825 Coils are solid-solution-strengthened nickel-iron-chromium-molybdenum-copper-titanium alloys formulated to excel where both high-temperature stability and corrosion resistance are essential. Their optimized chemistry—38–46 % Ni, 21–28 % Fe, 19.5–23.5 % Cr, 2.5–3.5 % Mo, 1.5–3 % Cu, 0.6–1.2 % Ti, and 0.2–0.8 % Al—provides tensile strengths ≥ 760 MPa and elongation ≥ 30 % after annealing, without relying on precipitation hardening. These coils maintain mechanical integrity from cryogenic temperatures up to 816 °C in continuous service and up to 982 °C intermittently, exhibiting outstanding resistance to oxidation, carburization, and chloride-stress-corrosion cracking in both oxidizing and reducing atmospheres. Their high Cr and Al contents form protective chromia/alumina scales, while Cu and Ti guard against pitting and crevice attacks in sulfuric, phosphoric, and hydrochloric acid environments. Excellent formability (stamping, slitting, fine-blanking) and weldability (TIG/GTAW, electron-beam) allow fabrication of diaphragms, bellows, springs, and heat-exchanger fins with minimal post-weld treatment. Coils are supplied in thicknesses from 0.1 mm to 5 mm and widths up to 1.2 m, per ASTM B424/ASME SB-424, ASTM B425/ASME SB-425, AMS 5599, and NACE MR0175 requirements.
| Element | Content (%) |
|---|---|
| Nickel (Ni) | 38.0 – 46.0 |
| Iron (Fe) | 21.0 – 28.0 |
| Chromium (Cr) | 19.5 – 23.5 |
| Molybdenum (Mo) | 2.50 – 3.50 |
| Copper (Cu) | 1.50 – 3.00 |
| Titanium (Ti) | 0.60 – 1.20 |
| Aluminum (Al) | 0.20 – 0.80 |
| Manganese (Mn) | ≤ 1.00 |
| Silicon (Si) | ≤ 0.50 |
| Carbon (C) | ≤ 0.050 |
| Sulfur (S) | ≤ 0.030 |
| Property | Annealed Strip (Min.) |
|---|---|
| Ultimate Tensile Strength | ≥ 760 MPa (110 ksi) |
| Yield Strength (0.2 % offset) | ≥ 310 MPa (45 ksi) |
| Elongation (4D) | ≥ 30 % |
| Hardness (Rockwell B) | ≤ 95 HRB |
| Property | Value |
|---|---|
| Density | 8.14 g/cm³ |
| Melting Range | 1385 – 1400 °C |
| Thermal Conductivity (25 °C) | 11.1 W/m·K |
| Specific Heat Capacity (25 °C) | 440 J/kg·K |
| Coefficient of Thermal Expansion | 13.9 µm/m·°C (20–100 °C) |
| Electrical Resistivity (20 °C) | 0.096 µΩ·m |
ASTM B424 / ASME SB-424 — Plate, sheet & strip form
ASTM B425 / ASME SB-425 — Strip & foil form
AMS 5599 — Special-quality strip/sheet
ISO 15156-3 / NACE MR0175 — Sour-service environments
Chemical Processing: Scrubber panels, evaporator tubing, reactor liners in sulfuric and phosphoric acid service
Oil & Gas: Well-piping jackets, offshore platform coils, acid gas sweetening vessels
Marine: Seawater condenser fins, pollution-control equipment, desalination coils
Power Generation: Gas-turbine transition ducts, combustion-chamber liners, heat-exchanger panels
Nuclear: Fuel reprocessing trays, radioactive-waste handling panels
Q1: Why select Incoloy 825 Coils for acidic environments?
Their high Mo and Cu content enhances resistance to reducing acids (sulfuric, phosphoric), while Cr and Ni protect against oxidizing media and chloride stress-corrosion cracking.
Q2: What temperature range can Incoloy 825 Coils handle?
Continuous service up to 816 °C (1500 °F), intermittent exposures to 982 °C (1800 °F), with stable mechanical and corrosion performance across this range.
Q3: Are Incoloy 825 Coils weldable and formable?
Yes—TIG/GTAW and electron-beam welding produce sound joints; excellent ductility (elongation ≥ 30 %) allows stamping, slitting, and fine-blanking with minimal springback.
Company Details
Business Type:
Manufacturer
Year Established:
2002
Total Annual:
20000000-80000000
Employee Number:
50~500
Ecer Certification:
Verified Supplier
Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys... Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys...
Get in touch with us