China Waspaloy Rod High Temperature Alloy 0.1mm-300mm Nickel Based Superalloy
China Waspaloy Rod High Temperature Alloy 0.1mm-300mm Nickel Based Superalloy

  1. China Waspaloy Rod High Temperature Alloy 0.1mm-300mm Nickel Based Superalloy

Waspaloy Rod High Temperature Alloy 0.1mm-300mm Nickel Based Superalloy

  1. MOQ: 150kgs
  2. Price: Negotiatable
  3. Get Latest Price
Payment Terms L/C,T/T,Western Union,MoneyGram
Supply Ability 300 Ton per Month
Delivery Time 2-30days
Packaging Details Wooden Pallets
Product Surface black or bright
Features Corrosion Resistance
Alloy Nickel alloys
Thickness 0.1mm-300mm
Melting Point 1330-1360°C
Weldability Good
Product Waspaloy
Densitsy 8.19 G/cm³
Electrical Resistivity 0.38 microhm•ft
Magnetic Permeability 1.004
Modulus of Elasticity (Dynamic 211 GPa
Thermal Conductivity 12.6 W/m-°C
Standard UNS N07001
Yield Strength at 0.2% offset 419MPa
Ultimate Tensile Strength 9095MPa
Elongation 52%
Common Name GH4738
Brand Name NikTech
Model Number Waspaloy
Certification ISO 9001:2008
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,T/T,Western Union,MoneyGram Supply Ability 300 Ton per Month
Delivery Time 2-30days Packaging Details Wooden Pallets
Product Surface black or bright Features Corrosion Resistance
Alloy Nickel alloys Thickness 0.1mm-300mm
Melting Point 1330-1360°C Weldability Good
Product Waspaloy Densitsy 8.19 G/cm³
Electrical Resistivity 0.38 microhm•ft Magnetic Permeability 1.004
Modulus of Elasticity (Dynamic 211 GPa Thermal Conductivity 12.6 W/m-°C
Standard UNS N07001 Yield Strength at 0.2% offset 419MPa
Ultimate Tensile Strength 9095MPa Elongation 52%
Common Name GH4738 Brand Name NikTech
Model Number Waspaloy Certification ISO 9001:2008
Place of Origin China
High Light 0.1mm High Temperature Alloy ,300mm High Temperature Alloy ,Corrosion Resistance heat resistant steel alloys

WASPALOY Rod: High-Performance Nickel-Based Superalloy for Extreme Environments

Product Overview

WASPALOY (UNS N07001) is a precipitation-hardenable, nickel-based superalloy renowned for its exceptional strength and oxidation resistance at elevated temperatures. Designed for demanding applications, it maintains high mechanical properties up to approximately 980°C (1800°F), making it ideal for components in gas turbines, aerospace engines, and other high-temperature environments. Its superior performance surpasses that of many conventional alloys, including Alloy 718, in critical applications.​

Chemical Composition

Element Composition (%)
Nickel (Ni) Balance
Chromium (Cr) 18.0 – 21.0
Cobalt (Co) 12.0 – 15.0
Molybdenum (Mo) 3.5 – 5.0
Titanium (Ti) 2.75 – 3.25
Aluminum (Al) 1.2 – 1.6
Carbon (C) 0.02 – 0.10
Silicon (Si) ≤0.10
Manganese (Mn) ≤0.10
Phosphorus (P) ≤0.015
Sulfur (S) ≤0.015
Boron (B) 0.003 – 0.01
Zirconium (Zr) ≤0.08
Copper (Cu) ≤0.10
Iron (Fe) ≤2.0

Mechanical Properties

Condition Tensile Strength (ksi) Yield Strength (ksi) Elongation (%) Hardness (HRC)
Annealed 160 max 95 25 34 – 44
Solution + Aged 160 min 105 25 34 – 44
Spring Temper 200 min 120 20 40 – 50

Physical Properties

Property Value
Density 8.19 g/cm³
Melting Point 1330 – 1360°C (2425 – 2475°F)
Modulus of Elasticity 211 GPa
Thermal Conductivity 19.1 W/m·°C (at 600°C)
Coefficient of Thermal Expansion 12.2 µm/m·°C (20 – 600°C)
Electrical Resistivity 1.24 microhm•m

Applications

WASPALOY rod is utilized in various high-temperature applications, including:​

  • Gas Turbine Engines: Components such as turbine blades, seals, and casings.

  • Aerospace: Parts like spacers, rings, and fasteners.

  • Missile Systems: Critical engine hardware and structural components.

  • Land-Based Gas Turbines: High-performance parts exposed to extreme conditions.​

FAQs

Q1: What is the maximum operating temperature for WASPALOY rod?

A1: WASPALOY rod is designed for use in temperatures up to approximately 980°C (1800°F), depending on the specific application and environmental conditions.​

Q2: Can WASPALOY rod be welded?

A2: Yes, WASPALOY rod can be welded using various techniques, including gas tungsten arc welding (GTAW) and gas metal arc welding (GMAW). It is important to follow proper welding procedures to maintain the alloy's properties .​

Q3: Is WASPALOY rod suitable for high-stress applications?

A3: Yes, WASPALOY rod exhibits excellent strength and resistance to fatigue, making it suitable for high-stress applications in gas turbines and aerospace components .​

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2002

  • Total Annual:

    20000000-80000000

  • Employee Number:

    50~500

  • Ecer Certification:

    Verified Supplier

Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys... Wuxi Nickel New Material Co., Ltd. (Wuxi NikTech) is a high-tech enterprise integrating the production, manufacturing, and research & development of specialty alloy materials. Located in Wuxi, Jiangsu Province, the company specializes in precision alloys, titanium alloys, high-temperature alloys...

+ Read More

Get in touch with us

  • Reach Us
  • Wuxi Nickel New Material Co., Ltd
  • Xinwu District, Wuxi City, Jiangsu Province
  • https://www.niktechmaterial.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement