China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel
China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel

  1. China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel
  2. China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel
  3. China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel
  4. China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel
  5. China Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel

Nickel - Base Superalloy Steel Pipe Incoloy A - 286 7.94 G / Cm³ Alloy Steel

  1. MOQ: 1000kg
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms L/C, T/T
Supply Ability 200 tons per year
Delivery Time 6-8 weeks
Packaging Details In bundles in wooden box
Brand Name Torich
Model Number Alloy Steel Pipe Incoloy A-286
Certification CE PED
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C, T/T Supply Ability 200 tons per year
Delivery Time 6-8 weeks Packaging Details In bundles in wooden box
Brand Name Torich Model Number Alloy Steel Pipe Incoloy A-286
Certification CE PED Place of Origin China
High Light alloy steel tube ,alloy steel seamless tube

Alloy Steel Pipe Incoloy A-286

 

Charactistic of material:

 

Chemical composition:

 

C: ≤0.08 Cr:13.5-16.0 Ni:24.0-27.0 Mo:1.00-1.50 Ti:1.75-2.30 Fe:remaind V:0.10-0.50 B:0.001-0.010 Mn:1.00-2.00 Al ≤0.04 Si:≤1.00 P:≤0.030 S:≤0.020 

 

Fe-25Ni-15Cr base superalloy + molybdenum,titanium,aluminum,Vanadium

 

Physical properties:

 

Density 7.94 g/cm³ 0.287 lb/in³
Melting Point 1430°C 2600°F
Coefficient of Expansion 16.4 μm/m °C (20 - 100°C) 9.1 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity 71.5 kN/mm² 10370 ksi
Modulus of Elasticity 205 kN/mm² 29733 ksi

 

Incoloy A-286 heat-treatment

Variety of materials Heat Treatment
Bar, pie 980~1000℃,1~2h,Oil cooler+700~720℃,12~16h,Air Cooling
Hot-rolled sheet, cold-rolled plate 980~1000℃,Air Cooling+700~720℃,12~16h,Air Cooling
Cold drawn bar 980~1000℃,1~2h,Oil cooler+700~720℃,16h,Air Cooling
Ring blanks 980~990℃,1~2h,Oil cooler+700~720℃,16h,Air Cooling
Cold heading cold drawing 980~1000℃,Water or oil cooling+700~720℃,16h,Air Cooling

 

 

High yield strength and durability 

creep strength

good processing plasticity and satisfactory welding performance

 

Incoloy A-286 is use in aerospace area.

 

Related standard:

SAE AMS5731 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti

 

SAE AMS 5732 Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and Rings15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30VConsumable Electrode Melted1800 °F (982 °C) Solution and Precipitation Heat Treated

 

AMS 5737

AMS 5525

 

Similar garde:UNSS66286 (USA), ZbNCT25 (France), PQA286 (USA)

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Importer,Exporter,Trading Company,Seller

  • Year Established:

    1997

  • Total Annual:

    25000000-30000000

  • Employee Number:

    100~200

  • Ecer Certification:

    Verified Supplier

Company Overview A Professional Steel Tube Manufacturer and Solution Provider TORICH INTERNATIONAL LIMITED integrates steel tube manufacturing, international trade, warehousing, technical support and customized processing. Our manufacturing operations cover cold drawing, cold rolling, heat treat... Company Overview A Professional Steel Tube Manufacturer and Solution Provider TORICH INTERNATIONAL LIMITED integrates steel tube manufacturing, international trade, warehousing, technical support and customized processing. Our manufacturing operations cover cold drawing, cold rolling, heat treat...

+ Read More

Get in touch with us

  • Reach Us
  • TORICH INTERNATIONAL LIMITED
  • Suite 1604-3, Hongan Plaza, #258 Die Yuan Road, Yinzhou District, Ningbo City, China
  • https://www.precision-steeltube.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement