| Supply Ability | 1000000kg per Month |
| Low-temperature Flexibility | No crack or fracture at 0℃ |
| Elongation at Break | ≥600% |
| Construction Method | Roll-on, brush-on, spray-on |
| Safety Feature | Water-based eco-friendly, flameless operation |
| Film Feature | Seamless integral waterproof membrane |
| Product Advantage | Weather-resistant, anti-aging |
| Packaging Details | Metal Barrel |
| Heat Resistance | No flowing, slipping, dripping at 110℃ |
| Application | Roof, basement, tunnel, bridge |
| Brand Name | shhous |
| Model Number | Type L |
| Certification | ISO |
| Place of Origin | Shandong, China |
View Detail Information
Explore similar products
Polymer Modified Asphalt Waterproof Coating For Tunnel Engineering
Polymer Modified Asphalt Bituminous Foundation Coating For Water Proofing
Liquid Polymer Modified Asphalt Emulsion Sealer Coating For Roof Waterproofing
Cold Applied Bituminous Waterproofing Coating Polymer Modified Asphalt For
Product Specification
| Supply Ability | 1000000kg per Month | Low-temperature Flexibility | No crack or fracture at 0℃ |
| Elongation at Break | ≥600% | Construction Method | Roll-on, brush-on, spray-on |
| Safety Feature | Water-based eco-friendly, flameless operation | Film Feature | Seamless integral waterproof membrane |
| Product Advantage | Weather-resistant, anti-aging | Packaging Details | Metal Barrel |
| Heat Resistance | No flowing, slipping, dripping at 110℃ | Application | Roof, basement, tunnel, bridge |
| Brand Name | shhous | Model Number | Type L |
| Certification | ISO | Place of Origin | Shandong, China |
| High Light | base slab bituminous waterproofing coating ,bituminous waterproofing coating anti aging ,underground black bitumen paint | ||
Building construction: Waterproofing works for roofs, basements, toilets, kitchens, balconies; renovation and repair of old roof waterproofing.
Underground engineering: Waterproofing for external basement walls, base slabs, post‑pouring belts, pile heads, pipe‑penetrating joints and other details.
Municipal engineering: Non‑exposed waterproofing for tunnels, culverts, drainage ditches and reservoirs.
Industrial buildings: Waterproofing for factory roofs and equipment foundations.
| No. | Item | Standard Requirements | |
| 1 | Appearance | Uniform after stirring without color difference, gel, agglomerate or obvious asphalt filaments | |
| 2 | Solid Content, % | ≥45 | |
| 3 | Heat Resistance | (80±2)℃, no flowing, sliding or dripping | |
| 4 | Surface Drying Time, h | ≤8 | |
| 5 | Complete Drying Time, h | ≤24 | |
| 6 | Low-temperature Flexibility | Standard Condition | −15℃ |
| 7 | Elongation at Break, % | Standard Condition | ≥600 |
The base surface shall be solid and flat, free of sanding, dust and oil stains. Repair cracks and holes with polymer mortar. Form R50 mm circular arcs at internal and external corners. Compact the areas around pipe roots and water outlets.
No standing water on the substrate, moisture content ≤9%. Apply primer to reinforce loose and sanding base surfaces.
Stir thoroughly with an electric mixer after opening the drum. Do not dilute with water or solvent.
Apply multiple thin coats in cross directions. Apply the next coat only when the previous one is surface‑dry and non‑tacky. Interval: 2‑6 h at normal temperature; 8‑24 h under low‑temperature and humid conditions.
Additional layers with width ≥200 mm shall be applied at internal and external corners, pipe roots, floor drains, expansion joints and water outlets by the two‑coat‑one‑fabric method.
Total dry‑film thickness ≥1.5 mm (subject to design requirements). Theoretical consumption: 2.5‑3.0 kg/㎡.
After construction, cure naturally for 24‑48 h at normal temperature; extend curing time under low‑temperature and high‑humidity conditions. No treading, rain exposure or water immersion before full curing.
After waterproof layer acceptance, construct protective layer of cement mortar or fine‑aggregate concrete. Perform water‑closing test only after full curing.
Suitable construction temperature: 5℃~35℃. Do not construct below 5℃ to avoid coating demulsification and failure.
Do not construct in rainy weather, with standing water on substrate, heavy fog, dew or wind force ≥Grade 5. Ambient humidity shall not exceed 85%.
Sediment at drum bottom is normal; stir well before use. Use up opened material on the same day whenever possible. Seal leftover material tightly. Discard caked or demulsified material.
The reinforcement fabric shall be fully saturated without white core, hollowing or edge curling. Cut and repair hollow areas before continuing coating work.
Storage temperature: 5‑40℃. Store in cool and ventilated place, keep away from heat source, avoid sunlight and frost.
Ensure good ventilation during construction. Avoid prolonged skin contact. In case of eye contact, rinse with plenty of clean water and seek medical advice immediately.
No chiseling or impact by sharp objects before full curing of coating film to prevent damage to waterproof layer.
Company Details
Business Type:
Manufacturer,Exporter
Year Established:
2000
Total Annual:
17790000-17790000
Employee Number:
150~200
Ecer Certification:
Verified Supplier
Weifang Shihua Chemical Building Materials Co., Ltd. Founded in 1994, the company has a registered capital of RMB 100.86 million and covers a plant area of over 30,000 square meters. It mainly manufactures more than 100 types of products across five major series, including Shihua‑brand po... Weifang Shihua Chemical Building Materials Co., Ltd. Founded in 1994, the company has a registered capital of RMB 100.86 million and covers a plant area of over 30,000 square meters. It mainly manufactures more than 100 types of products across five major series, including Shihua‑brand po...
Get in touch with us
Leave a Message, we will call you back quickly!