| Supply Ability | 1000000kg per Month |
| Water Damage Resistance | Sealing performance remains after water immersion |
| Product Form | Solid blocks |
| Base Material | Asphalt base, SBS polymer modified |
| Softening Point | ≥70‑90℃ |
| Cone Penetration | ≤70~180 (0.1mm), five grades available |
| Low‑temperature Performance | Flexible, no brittle cracking |
| Packaging Details | Carton or Metal Barrel |
| Melting Temperature | 180‑200℃ |
| Brand Name | shhous |
| Model Number | Type I,Type II,Type III,Type Ⅳ,Type Ⅴ |
| Place of Origin | Shandong, China |
| Certification | ISO |
View Detail Information
Explore similar products
Black Pavement Crack Sealant For Road And Bridge Expansion Joints With Strong
Weather Resistant Asphalt Crack Sealant Solid blocks For Preventive Highway
Special Crack Asphalt Joint Sealant Adhesive For Joint Sealing And Waterproofing
Strong Adhesion To Asphalt Hot Pour Crack Sealant For Highway Pavement Crack
Product Specification
| Supply Ability | 1000000kg per Month | Water Damage Resistance | Sealing performance remains after water immersion |
| Product Form | Solid blocks | Base Material | Asphalt base, SBS polymer modified |
| Softening Point | ≥70‑90℃ | Cone Penetration | ≤70~180 (0.1mm), five grades available |
| Low‑temperature Performance | Flexible, no brittle cracking | Packaging Details | Carton or Metal Barrel |
| Melting Temperature | 180‑200℃ | Brand Name | shhous |
| Model Number | Type I,Type II,Type III,Type Ⅳ,Type Ⅴ | Place of Origin | Shandong, China |
| Certification | ISO | ||
| High Light | low temperature asphalt joint sealant ,pavement asphalt joint sealant ,pavement asphalt to concrete joint sealant | ||
1. Strong Adhesion: Firm bonding to asphalt and cement-concrete pavements. Resists debonding under freeze-thaw and water immersion for stable waterproof sealing.
2. Superior High-low Temperature Performance: No flowing or tire-sticking at high temperature; flexible at low temperature without brittle cracking. Multiple grades available for wide service temperature of-40℃~80℃.
3. High Deformation Compatibility: 30-70% elastic recovery rate. Accommodates repeated thermal movement of cracks and resists fracture under pavement displacement.
4. Excellent Weather & Aging Resistance: UV-resistant, resistant to de-icing salt, acid-alkali and water erosion. Service life reaches 3-8 years under normal outdoor conditions.
5. Good Workability: Solid blocks melt at 180-200℃ with favorable fluidity to achieve full and compact crack filling.
6. Fast Curing: Quick cooling-curing enables fast traffic reopening and short road closure time.
7. Wear & Rolling Resistance: Withstands repeated tire loading, prevents material pull-out and blocks silt intrusion into joints.
8. Cost-effective Preventive Maintenance: Seals cracks to protect pavement base and slow down road deterioration, cutting heavy repair costs.
| No. | Performance Indicators | Type I | Type II | Type III | Type Ⅳ | Type Ⅴ |
| 1 | Penetration(25℃,5s,150g)(0.1 mm) | ≤70 | 50-90 | 70-110 | 90-150 | 120-180 |
| 2 | Compression Resilience Recovery Rate(25℃)(%) | 30-70 | ||||
| 3 | Viscosity(190℃)(Pa·s) | 1-4 | ||||
| 4 | Density(g/cm³) | ≤1.50 | ≤1.45 | ≤1.4 | ≤1.35 | ≤1.3 |
1. Crack Pretreatment: Remove dust, gravel and loose aggregates by crack cleaner and high-pressure air blower. Keep cracks dry and clean; dry wet areas completely.
2. Material Melting: Load modified asphalt sealant into melter, heat to 180-200℃ and stir evenly. Avoid local over-heating and carbonization.
3. Crack Pouring: Inject molten sealant into cracks via pouring gun for compact filling. Keep material surface 1-2 mm above pavement to offset shrinkage upon cooling.
4. Cooling & Curing: Allow natural cooling until fully cured. Prolong cooling time in low-temperature conditions.
5. Cleaning & Traffic Opening: Trim excess sealant on pavement. Reopen traffic after full curing.
Application Scenarios
1. Asphalt Pavements: Repair and sealing of transverse and longitudinal cracks for highways, municipal roads and rural roads.
2. Cement-concrete Pavements: Filling expansion joints, construction joints and settlement joints.
3. Bridge Projects: Sealing of bridge deck cracks and expansion joints.
4. Industrial Sites: Factory roads, parking lots and plaza pavements.
5. Special Sites: Airport runways and freight yard pavement joints.
6. Maintenance Works: Preventive road maintenance, old road reconstruction and sealing for joints between old and new pavements.
![]()
![]()
Company Details
Business Type:
Manufacturer,Exporter
Year Established:
2000
Total Annual:
17790000-17790000
Employee Number:
150~200
Ecer Certification:
Verified Supplier
Weifang Shihua Chemical Building Materials Co., Ltd. Founded in 1994, the company has a registered capital of RMB 100.86 million and covers a plant area of over 30,000 square meters. It mainly manufactures more than 100 types of products across five major series, including Shihua‑brand po... Weifang Shihua Chemical Building Materials Co., Ltd. Founded in 1994, the company has a registered capital of RMB 100.86 million and covers a plant area of over 30,000 square meters. It mainly manufactures more than 100 types of products across five major series, including Shihua‑brand po...