| Payment Terms | L/C, T/T, Western Union, MoneyGram |
| Supply Ability | 300 tons per month |
| Delivery Time | 20~40 Days |
| Packaging Details | Packed in Spool Carton box, Coil package with polybag,then in woodencase |
| Product Name | Hastelloy C4 pipe |
| Material | Ni Cr Mo |
| Elongation (≥ %) | 40 % |
| Density | 8.89 G/cm3 |
| Brinell Hardness HB | ≤220 |
| Tensile Strength | 690 MPA |
| Yield Strength | 276 MPa |
| Application | Engine components and combustion chamber |
| Melting Point | 1330-1380°C |
| Thermal Conductivity | 9.4 W/m-K |
| Brand Name | Runlai |
| Model Number | C4 |
| Certification | CE,ROHS,ISO 9001 |
| Place of Origin | China |
View Detail Information
Explore similar products
8.89 G/Cm3 Hastelloy C276 Hastelloy Alloy Nickel Hasteloy C276 Sheet Plate
Nickle Alloy Plate Sheet Hastelloy C22 C276 Ni Cr Mo Nickel Based C4 Hastelloy
625 718 725 750 800 825 Chemical Industry Nickel Alloy B2 Incoloy Monel Nickle
Nickel Chromium Alloy Hastelloy C22 Wire SN6276 UNS N10276 Hastelloy C-276
Product Specification
| Payment Terms | L/C, T/T, Western Union, MoneyGram | Supply Ability | 300 tons per month |
| Delivery Time | 20~40 Days | Packaging Details | Packed in Spool Carton box, Coil package with polybag,then in woodencase |
| Product Name | Hastelloy C4 pipe | Material | Ni Cr Mo |
| Elongation (≥ %) | 40 % | Density | 8.89 G/cm3 |
| Brinell Hardness HB | ≤220 | Tensile Strength | 690 MPA |
| Yield Strength | 276 MPa | Application | Engine components and combustion chamber |
| Melting Point | 1330-1380°C | Thermal Conductivity | 9.4 W/m-K |
| Brand Name | Runlai | Model Number | C4 |
| Certification | CE,ROHS,ISO 9001 | Place of Origin | China |
| High Light | 690 MPA hastelloy pipe ,C4 hastelloy pipe ,690 MPA hastelloy tube | ||
Chemical Processing Industry Hastelloy C4 Pipe 690 MPA Resistant To Stress Corrosion Cracking
Product Introduction
Hastelloy C4 pipe is a high-performance nickel-based alloy pipe with excellent corrosion resistance and high temperature stability, which is widely used in the chemical processing industry. Its main chemical components include nickel (Ni) 60-70%, chromium (Cr) 14-18%, molybdenum (Mo) 14-17%, iron (Fe) 3-7%, etc. These components give it excellent tolerance to a variety of acidic media, chlorides and other corrosive media in oxidizing and reducing environments. The physical properties of Hastelloy C4 pipe include density 8.64 g/cm³, melting point 1325-1370°C, tensile strength 760 MPa, yield strength 345 MPa, and elongation 50%. This alloy pipe can still maintain good mechanical properties and oxidation resistance in high temperature environments, and is suitable for the manufacture of chemical reactors, heat exchangers, distillation towers and other equipment. It has good processing performance and can be formed by conventional welding, cold rolling, hot rolling and other processes, and is suitable for the manufacture of parts with complex structures. Hastelloy C4 pipe has strict implementation standards and complies with ASTM B575 and ASME SB575 standards, ensuring its wide application in chemical, petroleum, aerospace and other fields.
Parameter
| Hastelloy Alloy | Ni | Cr | Co | Mo | FE | W | Mn | C | V | P | S | Si |
| C-4 | Balance | 14-18 | 2 Max | 14-17 | 3.0 Max | 1.0 Max | 0.015 Max | 0.04 Max | 0.03 Max | 0.08 Max |
| ASTM | Alloy | Type | UNS | Misc./Shape |
| ASTM B574 Bar | Hastelloy C-4 | Nickel | N06455 | Bar |
| ASTM B575 Plate | Hastelloy C-4 | Nickel | N06455 | Plate |
| ASTM B575 Strip | Hastelloy C-4 | Nickel | N06455 | Strip |
| ASTM B575 Sheet | Hastelloy C-4 | Nickel | N06455 | Sheet |
| ASTM B619 Welded Pipe | Hastelloy C-4 | Nickel | N06455 | Welded Pipe |
| ASTM B622 Seamless Tubing | Hastelloy C-4 | Nickel | N06455 | Seamless Tubing |
| ASTM B366 Fittings | Hastelloy C-4 | Nickel | N06455 | Fittings |
| ASTM B574 Wire | Hastelloy C-4 | Nickel | N06455 | Wire |
Specific Applications
Advantages and Characteristics
Contact Us
Email:fbwlau@cnrunlai.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
Q&A
How does Hastelloy C4 pipe compare to Hastelloy C276 pipe?
Hastelloy C4 performs well in strong acid environments such as hydrochloric acid and sulfuric acid, while Hastelloy C276 performs better in environments such as wet chlorine and hypochlorite.
What specifications can Hastelloy C4 pipe be customized?
Hastelloy C4 pipe can be customized with different outer diameters, wall thicknesses and lengths to meet specific needs.
How is Hastelloy C4 pipe packaged?
Hastelloy C4 pipe is usually packaged in wooden or iron boxes to ensure safe transportation and storage.
What is the high temperature resistance of Hastelloy C4 pipe?
Hastelloy C4 pipe can maintain good performance in high temperature environments and is suitable for high temperature corrosive environments.
![]()
![]()
Company Details
Business Type:
Manufacturer,Exporter,Trading Company
Year Established:
2008
Total Annual:
200000000-30000000
Employee Number:
8~15
Ecer Certification:
Active Member
CHANGZHOU LIANGRU INTERNATIONAL TRADE CO., LTD.specialized in production of Resistance Heating Alloy, Nickel Chromium Alloy, Iron Chromium Aluminum Alloy, Nickel Aluminum Alloy, Manganin, Copper Nickel Alloy, thermocouple wire, pure nickel and other precision alloy materials in the form of round wir... CHANGZHOU LIANGRU INTERNATIONAL TRADE CO., LTD.specialized in production of Resistance Heating Alloy, Nickel Chromium Alloy, Iron Chromium Aluminum Alloy, Nickel Aluminum Alloy, Manganin, Copper Nickel Alloy, thermocouple wire, pure nickel and other precision alloy materials in the form of round wir...
Get in touch with us
Leave a Message, we will call you back quickly!