China factories

China factory - Mianyang Baoheng New Material Technology Co.,Ltd

Mianyang Baoheng New Material Technology Co.,Ltd

  • China,Mianyang
  • Active Member

Leave a Message

we will call you back quickly!

Submit Requirement
China Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801
China Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

  1. China Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801
  2. China Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

Shot Blasted Ground Superalloy Nickel Alloy Bar INCOLOY 801

  1. MOQ: Negotiations
  2. Price: Negotiations
  3. Get Latest Price
Payment Terms T/T
Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 801 Alloy Round Bar
Grades INCOLOY alloy 801
Processing methods Shot blasted,Ground,Peeled,Machined,etc
Surface Rrough Turned,Grinding,Centreless Ground,etc
Profile Round Bar,Flat Bar,Forging Parts,Sheets Plates,etc
Price Term Ex-work,FOB, DDU etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number INCOLOY alloy 801
Certification SGS,TUV,BV,ISO,MTC
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 801 Alloy Round Bar Grades INCOLOY alloy 801
Processing methods Shot blasted,Ground,Peeled,Machined,etc Surface Rrough Turned,Grinding,Centreless Ground,etc
Profile Round Bar,Flat Bar,Forging Parts,Sheets Plates,etc Price Term Ex-work,FOB, DDU etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL Model Number INCOLOY alloy 801
Certification SGS,TUV,BV,ISO,MTC Place of Origin China
High Light Shot blasted nickel alloy bar ,INCOLOY 801 nickel alloy bar ,INCOLOY 801

INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar

 

 

Description

 

 

Our company provides INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar.

All of INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Length: Fixed length or random length or based on the customer's special requirement.

 

 

Products Details

 

 

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.05
Cr (%): ≤ 20.5 
Ni (%): ≤ 32.0
Cu (%): ≤ 0.150

Ti (%): ≤ 1.10

Fe(%): ≤ 45.5

Tensile strength, σb/≥ MPa: 450
Yield strength, σ0.2/MPa: 170
Elongation, δ ≥(%): 30.0
Reduction of area, ф ≥ (%): -
Hardness via heat treatment /HBW: -

 

 

 

Applications: 

 

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

Superalloy is widely used to produce the high temperature components for gas turbine in the field of aviation, naval vessels and industry, such as turbine blade, guide blade, turbine disc, high pressure compressor disc, combustor, and also production of energy conversion devices, such as aerospace craft, rocket motor, nuclear reactor, petrochemical equipments, coaly transforming and so on.

 

INCOLOY alloy 801 Rrough Turned Alloy Round Bar 801 Superalloy Round Bar 801 Grinding Round Bar 801 Q+T Bar

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 801 Alloy Round Bar 801 Superalloy Round Bar 801 Round Bar 801 Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Packing method

Wooden Pallet BOX,based on the customer's special requirement,etc

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company

  • Total Annual:

    5000000-8000000

  • Employee Number:

    10~30

  • Ecer Certification:

    Active Member

      Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...       Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...

+ Read More

Get in touch with us

  • Reach Us
  • Mianyang Baoheng New Material Technology Co.,Ltd
  • Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
  • https://www.ss-bars.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement