| Product Name | AISI 660 Alloy Steel Plates |
| Grades | AISI 660 |
| Processing methods | Cold working,Machined |
| Surface | Bright , Centreless Ground etc. |
| Profile | Round Bar , Flat Bar , Forging Parts |
| Price Term | Ex-work |
| Brand Name | ANSTEEL,TISCO,BAOSTEEL,PANGANGGROUP |
| Model Number | AISI 660 |
| Certification | SGS,TUV,BV,ISO,MTC |
| Place of Origin | China |
View Detail Information
Explore similar products
NiCr19CoMo W-Nr 2.4973 Alloy Steel Plates Rene 41 UNS N07041 Wire Rod
AMS 6532 Alloy Steel Plates UNS K92580 Forging Piece
AMS 5604 Alloy Steel Plates UNS s17400 AISI 630 F593 Plates
W1C-8 UNS T72301 Alloy Steel Plates C85W W-Nr 1.1830 SK85 STC5 Metal Flat Plate
Product Specification
| Payment Terms | T/T | Supply Ability | 50000KGS/Month |
| Delivery Time | Ex-stock for delivery: 3-7 days Production lead time: 30-42 days | Packaging Details | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name | AISI 660 Alloy Steel Plates | Grades | AISI 660 |
| Processing methods | Cold working,Machined | Surface | Bright , Centreless Ground etc. |
| Profile | Round Bar , Flat Bar , Forging Parts | Price Term | Ex-work |
| Brand Name | ANSTEEL,TISCO,BAOSTEEL,PANGANGGROUP | Model Number | AISI 660 |
| Certification | SGS,TUV,BV,ISO,MTC | Place of Origin | China |
| High Light | AISI 660 Alloy Steel Plates ,AISI 660 Superalloy Steel Plates ,AISI 660 Turbine Blade Steel | ||
AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel
Description
Our company provides AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
All of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Products Details
AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
| Chemical Composition (weight%): | |
| C | ≤ 0.08 |
| Si | ≤ 1.00 |
| Mn | ≤ 2.00 |
| P | ≤ 0.040 |
| S | ≤ 0.030 |
| Cr | 13.5 ~ 16.0 |
| Ni | 24.0 ~ 27.0 |
| Mo | 1.00 ~ 1.50 |
| Ti | 1.90 ~ 2.35 |
| Cu | ≤ 0.025 |
| Al | ≤ 0.035 |
| B | 0.0010 ~ 0.010 |
| Mechanical Properties Under Final Heat Treatment: | |
| Condition / Bar: Solution treated, precipitation hardened | |
| Tensile strength, σb/≥ MPa | 950 |
| Yield strength, σ0.2/≥ MPa | 650 |
| Elonghation, δ ≥(%) | 12.0 |
| Reduction of area, ф ≥ (%) | - |
| Hardness | HB | - |
![]()
Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers' requirements.
The alloy is usually produced by AOD / VIM VOD followed by electroslag refining (ESR) or VAR if necessary for special purpose.
![]()
![]()
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
![]()
Submit an enquiry for the displaying steel materials you are interested in TODAY!
Sales Engineer: sales@ss-bars.com
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company
Total Annual:
5000000-8000000
Employee Number:
10~30
Ecer Certification:
Active Member
Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un... Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un...
Get in touch with us
Leave a Message, we will call you back quickly!