China Centreless Ground Nickel Alloy Bar Superalloy Bar INCOLOY Alloy 810
China Centreless Ground Nickel Alloy Bar Superalloy Bar INCOLOY Alloy 810

  1. China Centreless Ground Nickel Alloy Bar Superalloy Bar INCOLOY Alloy 810
  2. China Centreless Ground Nickel Alloy Bar Superalloy Bar INCOLOY Alloy 810

Centreless Ground Nickel Alloy Bar Superalloy Bar INCOLOY Alloy 810

  1. MOQ: Negotiations
  2. Price: Negotiations
  3. Get Latest Price
Payment Terms T/T
Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 810 Alloy Round Bar
Grades INCOLOY alloy 810
Processing methods Peeled,Cold working,Machined,etc
Surface Grinding,Centreless Ground,etc
Profile Forging Parts,Sheets Plates,Forging Piece,etc
Price Term Ex-work,FOB,etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number INCOLOY alloy 810
Certification SGS,TUV,BV,ISO,MTC
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 810 Alloy Round Bar Grades INCOLOY alloy 810
Processing methods Peeled,Cold working,Machined,etc Surface Grinding,Centreless Ground,etc
Profile Forging Parts,Sheets Plates,Forging Piece,etc Price Term Ex-work,FOB,etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL Model Number INCOLOY alloy 810
Certification SGS,TUV,BV,ISO,MTC Place of Origin China
High Light Centreless Ground nickel alloy bar ,INCOLOY Alloy 810 nickel alloy bar

INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Round Bar 810 Bar

 

 

Description

 

 

Our company provides INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 Annealed Bar.

All of INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 annealed Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Round Bar 810 Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

 

 

Products Details

 

 

INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 Annealed Bar

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.25
Si (%): ≤ 0.80
Mn (%): ≤ 0.90
Cr (%):≤ 21.0
Ni (%):≤ 32

Al(%):≤ 0.50
Fe (%): Remainder

Tensile strength, σb/≥ MPa: 550
Yield strength, σ0.2/MPa: 215
Elongation, δ ≥(%): 25.0
Reduction of area, ф ≥ (%): -
Hardness via heat treatment /HBW: -

 

 

 

Applications: 

 

INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 Annealed Bar

Tall oil distillation columns and equipments,Food processing equipments,Hydrometallurgy, heat exchangers,Oil and gas production equipments,Pulp mill bleach systems,Seawater handling equipments,etc

 

INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 Annealed Bar

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 810 Alloy Round Bar 810 Superalloy Round Bar 810 Hot rolled Round Bar 810 Annealed Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, FedEx/DHL/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company

  • Total Annual:

    5000000-8000000

  • Employee Number:

    10~30

  • Ecer Certification:

    Active Member

      Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...       Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...

+ Read More

Get in touch with us

  • Reach Us
  • Mianyang Baoheng New Material Technology Co.,Ltd
  • Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
  • https://www.ss-bars.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement