China INCOLOY 903 Alloy Steel Flat Bar Superalloy Bar OEM Welcome
China INCOLOY 903 Alloy Steel Flat Bar Superalloy Bar OEM Welcome

  1. China INCOLOY 903 Alloy Steel Flat Bar Superalloy Bar OEM Welcome
  2. China INCOLOY 903 Alloy Steel Flat Bar Superalloy Bar OEM Welcome

INCOLOY 903 Alloy Steel Flat Bar Superalloy Bar OEM Welcome

  1. MOQ: Negotiations
  2. Price: Negotiations
  3. Get Latest Price
Payment Terms T/T
Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 903 Alloy Round Bar
Grades INCOLOY alloy 903
Processing methods Shot blasted,Ground,Peeled,Cold working,Machined,etc
Surface Black,Bright,Rrough Turned,Grinding,Centreless Ground,etc
Profile Round Bar,Flat Bar,Forging Parts,Sheets Plates,Forging Piece,etc
Price Term Ex-work,FOB,CIF,CFR, DDU etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number INCOLOY alloy 903
Certification SGS,TUV,BV,ISO,MTC
Place of Origin China

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms T/T Supply Ability 100000KGS/Month
Delivery Time Ex-stock for delivery: 3-7 days Production lead time: 45-55days Packaging Details Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name INCOLOY alloy 903 Alloy Round Bar Grades INCOLOY alloy 903
Processing methods Shot blasted,Ground,Peeled,Cold working,Machined,etc Surface Black,Bright,Rrough Turned,Grinding,Centreless Ground,etc
Profile Round Bar,Flat Bar,Forging Parts,Sheets Plates,Forging Piece,etc Price Term Ex-work,FOB,CIF,CFR, DDU etc.
Brand Name PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL Model Number INCOLOY alloy 903
Certification SGS,TUV,BV,ISO,MTC Place of Origin China
High Light OEM Alloy Steel Flat Bar ,INCOLOY 903 Alloy Steel Flat Bar ,INCOLOY 903

INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy 

 

 

Description

 

 

Our company provides INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy.All of INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

 

  • Material:Metal,INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy
  • Shape:Superalloy Flat Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

 

 

Products Details

 

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.020
Si (%): -
Mn (%):-
Cr (%): -
Ni (%): ≤ 38
Mo (%): -

Al(%): ≤ 0.70
Cu (%): -

Ti(%): ≤ 1.40

Fe(%): ≤ 41.0

Co (%): ≤ 15.0

Nb (%): ≤ 3.0

Condition / Bar: Solution, ageing treated
Tensile strength, σb/≥ MPa: 1174
Yield strength, σ0.2/≥ MPa: 900
Elongation, δ ≥(%): 8.0
Reduction of area, ф ≥ (%): 10.0
Hardness | HB: 311 Min

 

 

 

Applications: 

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

combustor,aerospace craft,rocket motor,nuclear reactor,petrochemical equipments,coaly transforming,etc

 

INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy

 

 

FAQ 

 

 

Q: How do you control the quality?

 

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

 

 

Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company

  • Total Annual:

    5000000-8000000

  • Employee Number:

    10~30

  • Ecer Certification:

    Active Member

      Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...       Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others.       Our business is based on un...

+ Read More

Get in touch with us

  • Reach Us
  • Mianyang Baoheng New Material Technology Co.,Ltd
  • Building 4A, Cross-border E-commerce Industrial Park, Shiqiaopu, High-tech Zone, Mianyang City, SC, China
  • https://www.ss-bars.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement