| Product Name | INCOLOY alloy 903 Alloy Round Bar |
| Grades | INCOLOY alloy 903 |
| Processing methods | Shot blasted,Ground,Peeled,Cold working,Machined,etc |
| Surface | Black,Bright,Rrough Turned,Grinding,Centreless Ground,etc |
| Profile | Round Bar,Flat Bar,Forging Parts,Sheets Plates,Forging Piece,etc |
| Price Term | Ex-work,FOB,CIF,CFR, DDU etc. |
| Brand Name | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
| Model Number | INCOLOY alloy 903 |
| Certification | SGS,TUV,BV,ISO,MTC |
| Place of Origin | China |
View Detail Information
Explore similar products
SAE 17-22-AV Alloy Steel Flat Bar 17-22-A V Precipitation Hardening
18-2Mn Alloy Steel Flat Bar Grinding Surface
AISI P20+S Tool Steel 40CrMnMoS 8-6 W-Nr 1.2312 Plate
EV8 UNS S63008 Alloy Steel Flat Bar X53CrMnNiN21-9 W-Nr 1.4871 Cold Rolled Strip
Product Specification
| Payment Terms | T/T | Supply Ability | 100000KGS/Month |
| Delivery Time | Ex-stock for delivery: 3-7 days Production lead time: 45-55days | Packaging Details | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name | INCOLOY alloy 903 Alloy Round Bar | Grades | INCOLOY alloy 903 |
| Processing methods | Shot blasted,Ground,Peeled,Cold working,Machined,etc | Surface | Black,Bright,Rrough Turned,Grinding,Centreless Ground,etc |
| Profile | Round Bar,Flat Bar,Forging Parts,Sheets Plates,Forging Piece,etc | Price Term | Ex-work,FOB,CIF,CFR, DDU etc. |
| Brand Name | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL | Model Number | INCOLOY alloy 903 |
| Certification | SGS,TUV,BV,ISO,MTC | Place of Origin | China |
| High Light | OEM Alloy Steel Flat Bar ,INCOLOY 903 Alloy Steel Flat Bar ,INCOLOY 903 | ||
INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy
Description
Our company provides INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy.All of INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Round bar / Wire rod (Diameter): 5.5mm to 800mm
Square bar / Flat bar: 3mm to 800mm
Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)
Products Details
INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy
| Chemical Composition (weight%): | Mechanical Properties Under Final Heat Treatment: |
| C (%): ≤ 0.020 Al(%): ≤ 0.70 Ti(%): ≤ 1.40 Fe(%): ≤ 41.0 Co (%): ≤ 15.0 Nb (%): ≤ 3.0 | Condition / Bar: Solution, ageing treated Tensile strength, σb/≥ MPa: 1174 Yield strength, σ0.2/≥ MPa: 900 Elongation, δ ≥(%): 8.0 Reduction of area, ф ≥ (%): 10.0 Hardness | HB: 311 Min |
![]()
Applications:
INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy
combustor,aerospace craft,rocket motor,nuclear reactor,petrochemical equipments,coaly transforming,etc
![]()
![]()
INCOLOY alloy 903 Annealed Alloy Steel Flat Bar 903 Solution Treated Superalloy Flat Bar 903 Quenched and Tempered Flat Bar 903 Peeled Alloy
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 903 Alloy Steel Flat Bar 903 Superalloy Flat Bar 903 Flat Bar 903 Alloy and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.
![]()
Packing method
Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company
Total Annual:
5000000-8000000
Employee Number:
10~30
Ecer Certification:
Active Member
Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un... Baoheng New Material is a specialty metals solutions center serving customers in a variety of industries, including Aerospace, Defense, Space, Fastener, Medical, Power Generation, Oil and Gas, Semiconductor and many others. Our business is based on un...
Get in touch with us
Leave a Message, we will call you back quickly!