China EN 1.4547 Stainless Steel Tube SCH80S Good Pitting And Stress Corrosion
China EN 1.4547 Stainless Steel Tube SCH80S Good Pitting And Stress Corrosion

  1. China EN 1.4547 Stainless Steel Tube SCH80S Good Pitting And Stress Corrosion
  2. China EN 1.4547 Stainless Steel Tube SCH80S Good Pitting And Stress Corrosion

EN 1.4547 Stainless Steel Tube SCH80S Good Pitting And Stress Corrosion

  1. MOQ: Negotiable
  2. Price: Negotiable
  3. Get Latest Price
Payment Terms L/C, T/T, D/A, D/P
Supply Ability 50TONS/30DAYS
Delivery Time 30 DAYS
Packaging Details In bundles with waterproof material,or wooden crate packing
Material 1.4547
Standard DIN, EN
SIZE SCH80S
technique Cold-drawn
Advantage good pitting resistance
package woven packing
OD 6-830mm
Brand Name zheheng steel
Model Number 88.9mm
Certification iso9001
Place of Origin CHINA

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C, T/T, D/A, D/P Supply Ability 50TONS/30DAYS
Delivery Time 30 DAYS Packaging Details In bundles with waterproof material,or wooden crate packing
Material 1.4547 Standard DIN, EN
SIZE SCH80S technique Cold-drawn
Advantage good pitting resistance package woven packing
OD 6-830mm Brand Name zheheng steel
Model Number 88.9mm Certification iso9001
Place of Origin CHINA
High Light EN 1.4547 Stainless Steel Tube Pipe ,SCH80S Stainless Steel Tube Pipe ,corrosion resistance Stainless Steel Seamless Pipe

DIN EN 1.4307 X5CrNi18-10 Stainless Steel Tube SCH80S Good corrosion resistance

 

 

1.4547 (also known as UNS S31254, 254SMO and SS2378) is a high alloy stainless steel with very good corrosion resistance. The steel is used in halogenated environments such as seawater, yan acid and contaminated liu acid. 1.4547 Compared with ordinary stainless steel, it has good resistance to uniform corrosion, especially in acids containing halides. It has a high content of alloying material that makes the steel particularly resistant to dents and crevices corrosion. Steel is also very resistant to stress corrosion cracking.


Advantage:

This kind of steel has very good local corrosion resistance, in seawater, aerated, there are gaps, low speed erosion conditions, has good pitting resistance (PI≥40) and good stress corrosion resistance, is a substitute material for Ni-based alloys and titanium alloys. Secondly, in the performance of high temperature or corrosion resistance, it has more excellent high temperature or corrosion resistance, and is irreplaceable in 304 stainless steel.


Description for our production range:

Name :Stainless Steel seamless Pipe
Standard :EN10216-5 , EN10216-2,DIN 17456 , DIN 17458,ASTM A312,
A213, A269, A511, A789, A790 ETC,GOST 9941 , GOST 5632,
JIS G3459 , JIS G3463,GB/T14975,GB/T14975, GB13296, GB5310, GB9948

 

 
Material Grade :
EN 1.4547
Diameter :OD: 6-830mm
W.T: 0.6mm - 60mm

Length :Up to 13 meter or as customers' request
Tolerance :According to the Standard.
Surface :
Natural Color of annealing & pickling, 180G, 320G, 400G Satin / Hairline
400G, 500G, 600G or 800G Mirror finish
Test :
UT, ET, HT, RT,ect, and others according to the standard,
or as the requests of the customer

 
Chemical Composition
 

Chemical Composition, %
Country (Region) Standard Steel Grade (Steel Number)   C, ≤ Si, ≤ Mn, ≤ P, ≤ S, ≤ Cr Ni Cu Mn N
European Union EN 10216 X1CrNiMoCuN20-18-7
(1.4547)
MIN           19.5 17.5 0.5 6 0.18
MAX 0,020 0.7 1 0,030 0,010 20.5 18.5 1.00 7.00 0.25

 

our products packing:

 
 
other supplement:
1.A999/A999M: Each pipe shall be subjected to the nondestructive electric test or the hydrostatic test, the pipe of test to be used shall be at the option of the mfg, unless otherwise specified in the PO.
2. The Pipe lengths : Unless otherwise agreed upon, all size from NPS 1/8" TO AND INCLUDING nps 8 are available in a length up to 24ft with the permitted range of 15 to 24 ft. Short length are acceptable and the number and min, length shall be agreed upon between mfg and purchaser.
3. The finished pipe shall be reasonably straight and shall have workmanlike finish, Removal of imperfections by grinding is permitted, provided the W.T are not decreased to the less than the permitted in Section 9 of Specification A999/A999M
4. Butt Weld End: According to ANSI B 16.25
5. Pipe Marking: Specified in A999/999M, include "Logo+Standard+SIZE+Heat No.+Lot No.+H.T/E.T/U.T"
6. Packing: Each Pipe end is protected by Plastic cap. Then packed by Anti-rust steel strip, The outside of the bundle is plastic woven bag, or Plastic film.
7. Packing Mark: SIZE + STEEL GRADE+ QTY OF PIECE/WEIGHT/METRE.
8.MTC: BWSS Official Original MTC paper will be supplied for each order.

 

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Trading Company

  • Year Established:

    1995

  • Total Annual:

    6,000,000-8,000,000

  • Employee Number:

    100~150

  • Ecer Certification:

    Verified Supplier

Zheheng steel is one  incorporate of manufacturer, Exporter ,consultant ,stockist company specialized in the area of stainless steel tubing , pipe fittings ,Flanges and other stainless steel grade accessories . It is one-stop-shop company ,our team have more than 20 years experience in sta... Zheheng steel is one  incorporate of manufacturer, Exporter ,consultant ,stockist company specialized in the area of stainless steel tubing , pipe fittings ,Flanges and other stainless steel grade accessories . It is one-stop-shop company ,our team have more than 20 years experience in sta...

+ Read More

Get in touch with us

  • Reach Us
  • Wenzhou Zheheng Steel Industry Co.,Ltd
  • No999 .wenzhou airport wenzhou city,zhejiang china
  • https://www.stainless-steelseamlesspipe.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement