China ASTM A790 Welded Duplex Stainless Steel Pipe S31803/S32205/S32750 for Stress
China ASTM A790 Welded Duplex Stainless Steel Pipe S31803/S32205/S32750 for Stress

  1. China ASTM A790 Welded Duplex Stainless Steel Pipe S31803/S32205/S32750 for Stress

ASTM A790 Welded Duplex Stainless Steel Pipe S31803/S32205/S32750 for Stress

  1. MOQ: 5Ton
  2. Price: Based on grade, size, surface, processing, quantity and current raw material market price.
  3. Get Latest Price
Payment Terms L/C,D/A,D/P,T/T,Western Union
Product Alias Duplex Steel Pipe / Super Duplex Pipe / Ferritic-Austenitic Pipe / 2205 Pipe / 2507 Pipe / S32205 Pipe
Chemical Composition (S32205) Cr 21.0-23.0% / Ni 4.5-6.5% / Mo 2.5-3.5% / N 0.14-0.20% / C ≤ 0.030% / Fe Balance
Material Type Ferritic-Austenitic (Duplex) Stainless Steel
Heat Treatment Solution Annealed (min 1020°C for S32205; min 1025°C for S32750) + Water Quench
Chemical Composition (S32750) Cr 24.0-26.0% / Ni 6.0-8.0% / Mo 3.0-5.0% / N 0.24-0.32% / C ≤ 0.030% / Fe Balance
Key Feature Autogenous welding (no filler); solution annealed & water quenched; 40-60% ferrite-austenite balance; ASTM A923 intermetallic testing
Mechanical Properties (S32750) Tensile ≥800 MPa / Yield ≥550 MPa / Elongation ≥15%
Common Grades S31803 (2205), S32205 (Improved 2205), S32750 (2507 Super Duplex), S32760, S32304, S32101
Mechanical Properties (S32205) Tensile ≥620 MPa / Yield ≥450 MPa / Elongation ≥25%
Packaging Details Standard seaworthy export packing with bundles, waterproof wrapping, pallets or wooden cases.
Delivery Time 7-15
Product Name ASTM A790 Welded Duplex Stainless Steel Pipe
Supply Ability Stock supply, regular production and custom manufacturing available.
Brand Name Shangyou
Certification ISO9001
Place of Origin China

View Detail Information

Inquiry by Email Get Latest Price
Chat online Now Ask for best deal
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C,D/A,D/P,T/T,Western Union Product Alias Duplex Steel Pipe / Super Duplex Pipe / Ferritic-Austenitic Pipe / 2205 Pipe / 2507 Pipe / S32205 Pipe
Chemical Composition (S32205) Cr 21.0-23.0% / Ni 4.5-6.5% / Mo 2.5-3.5% / N 0.14-0.20% / C ≤ 0.030% / Fe Balance Material Type Ferritic-Austenitic (Duplex) Stainless Steel
Heat Treatment Solution Annealed (min 1020°C for S32205; min 1025°C for S32750) + Water Quench Chemical Composition (S32750) Cr 24.0-26.0% / Ni 6.0-8.0% / Mo 3.0-5.0% / N 0.24-0.32% / C ≤ 0.030% / Fe Balance
Key Feature Autogenous welding (no filler); solution annealed & water quenched; 40-60% ferrite-austenite balance; ASTM A923 intermetallic testing Mechanical Properties (S32750) Tensile ≥800 MPa / Yield ≥550 MPa / Elongation ≥15%
Common Grades S31803 (2205), S32205 (Improved 2205), S32750 (2507 Super Duplex), S32760, S32304, S32101 Mechanical Properties (S32205) Tensile ≥620 MPa / Yield ≥450 MPa / Elongation ≥25%
Packaging Details Standard seaworthy export packing with bundles, waterproof wrapping, pallets or wooden cases. Delivery Time 7-15
Product Name ASTM A790 Welded Duplex Stainless Steel Pipe Supply Ability Stock supply, regular production and custom manufacturing available.
Brand Name Shangyou Certification ISO9001
Place of Origin China
ASTM A790 Welded Duplex Stainless Steel Pipe S31803/S32205/S32750 for Stress Corrosion Resisting Service

Shaanxi Shangyou Stainless Steel Co., Ltd. supplies ASTM A790 welded duplex stainless steel pipe for global EPC contractors, oil and gas operators, chemical processors, and marine fabricators requiring high-strength piping with exceptional resistance to stress corrosion cracking. Produced to ASTM A790/A790M, this specification covers seamless and straight-seam welded ferritic/austenitic (duplex) steel pipe intended for general corrosive service, with particular emphasis on resistance to stress corrosion cracking.

ASTM A790 is the primary pipe specification for duplex stainless steel. The pipe shall be made by an automatic welding process without the addition of filler metal. All material shall be solution annealed and water quenched to achieve the target austenite-ferrite microstructure (typically 40-60% ferrite), which is essential for the excellent combination of strength and corrosion resistance that duplex grades offer. The specification covers standard duplex grades (22% Cr, such as S31803/S32205) and super duplex grades (25% Cr, such as S32750/S32760). These steels are susceptible to embrittlement if used for prolonged periods at elevated temperatures, making temperature control critical.

Custom Attributes
Dimension Specification
Product Name
ASTM A790 Welded Duplex Stainless Steel Pipe
Product Alias
Duplex Steel Pipe / Super Duplex Pipe / Ferritic-Austenitic Pipe / 2205 Pipe / 2507 Pipe / S32205 Pipe
Material Type
Ferritic-Austenitic (Duplex) Stainless Steel
Key Feature
Autogenous welding (no filler); solution annealed & water quenched; 40-60% ferrite-austenite balance; ASTM A923 intermetallic testing
Common Grades
S31803 (2205), S32205 (Improved 2205), S32750 (2507 Super Duplex), S32760, S32304, S32101
Chemical Composition (S32205)
Cr 21.0-23.0% / Ni 4.5-6.5% / Mo 2.5-3.5% / N 0.14-0.20% / C ≤ 0.030% / Fe Balance
Chemical Composition (S32750)
Cr 24.0-26.0% / Ni 6.0-8.0% / Mo 3.0-5.0% / N 0.24-0.32% / C ≤ 0.030% / Fe Balance
Mechanical Properties (S32205)
Tensile ≥620 MPa / Yield ≥450 MPa / Elongation ≥25%
Mechanical Properties (S32750)
Tensile ≥800 MPa / Yield ≥550 MPa / Elongation ≥15%
Heat Treatment
Solution Annealed (min 1020°C for S32205; min 1025°C for S32750) + Water Quench
Primary Applications
Oil & Gas / Offshore Platforms / Chemical Processing / Desalination / Pulp & Paper / Marine Environments
Core Specifications
Parameter Available Options
Product Standard
ASTM A790/A790M, ASME SA-790
Grade Equivalents
S31803 (2205), S32205 (Improved 2205), S32750 (2507 Super Duplex), S32760 (Zeron 100), S32304 (2304 Lean Duplex), S32101 (LDX 2101)
Nominal Pipe Size (NPS)
1/4″ to 30″+
Outside Diameter (OD)
13.7mm to 762mm+
Wall Thickness
Schedule 5S, 10S, 40S, 80S per ASME B36.19
Length
Single random, double random, or cut-to-length
Pipe End
Plain End (PE) / Beveled End (BE) / Threaded
Welding Process
Automatic welding, no filler metal added
Heat Treatment
Solution Annealed + Water Quenched (mandatory)
Inspection
Tension Test / Flattening Test / Hydrostatic or NDE Test / ASTM A923 Intermetallic Test (Method A, B, or C) / PMI
Documents
MTC 3.1 / Inspection Reports / Packing List / Heat Number Traceability
Applications and Material Selection Guide

ASTM A790 duplex stainless steel pipe is specified for applications where high strength and resistance to chloride-induced stress corrosion cracking, pitting, and crevice corrosion are required. The PREN (Pitting Resistance Equivalent Number) for S32205 is ~36 and for S32750 is ~42.

Typical applications include:

  • Offshore topside and subsea piping systems
  • Oil and gas production facilities and refining equipment
  • Chemical processing plant piping handling organic acids and chlorides
  • Desalination plants (seawater intake and brine systems)
  • Pulp and paper manufacturing
  • Marine environments and pollution control equipment
  • Heat exchangers and condensers

Key selection considerations: ASTM A790 is unique in that it does not permit filler metal during welding. For welded pipe made with filler metal from plate, ASTM A928 applies instead. The solution annealing and water quenching are mandatory to prevent the formation of detrimental intermetallic phases (sigma, chi) that severely degrade toughness and corrosion resistance. ASTM A923 intermetallic testing is critical and often required by EPC specifications—Method C (ferric chloride corrosion test) is the most stringent. Select S31803/S32205 for standard 22% Cr duplex service; S32750 for super duplex 25% Cr applications requiring higher strength and corrosion resistance. Note that duplex steels are susceptible to embrittlement at elevated temperatures and should not be used for prolonged service above 300-400°C.

Processing, Packaging and After-Sales

Shangyou Stainless Steel provides value-added processing including custom cutting, beveling, and end protection for duplex pipes.

All pipes are packed with export-standard protection including protective end caps, steel strapping, waterproof wrapping, and wooden pallets or steel frames.

Quality documents include MTC 3.1, inspection reports, packing list, and heat number traceability. Third-party inspection (SGS, TUV, BV) can be arranged upon request.

Frequently Asked Questions

1.What is ASTM A790?

ASTM A790 is the standard specification for seamless and welded duplex (ferritic/austenitic) stainless steel pipe, with particular emphasis on resistance to stress corrosion cracking.

2. What is the difference between ASTM A790 and ASTM A928?

ASTM A790 covers duplex pipe welded without filler metal (autogenous welding); ASTM A928 covers duplex pipe welded with filler metal from plate. Use A928 when filler metal is added.

3. What grades are available under ASTM A790?

S31803 (2205), S32205 (Improved 2205), S32750 (2507 Super Duplex), S32760, S32304 (2304), and S32101.

4. Is heat treatment required for ASTM A790?

Yes, all pipes must be solution annealed and water quenched to achieve the required 40-60% austenite-ferrite microstructure and prevent intermetallic phases.

5. What is the PREN rating of duplex grades?

S32205 has PREN ~36; S32750 has PREN ~42, indicating excellent pitting resistance.

6. What testing is required for ASTM A790?

Tension test, flattening test, hydrostatic or NDE test, and ASTM A923 intermetallic test (Method A, B, or C).

7. What is the ASTM A923 intermetallic test?

It detects detrimental intermetallic phases (sigma, chi) from improper heat treatment. Method C (ferric chloride corrosion test) is most stringent.

8. What are typical applications for A790 duplex pipe?

Offshore oil & gas, subsea systems, chemical processing, desalination, pulp & paper, and marine environments.

9. What documents are provided with delivery?

MTC 3.1, inspection reports, packing list, and heat number traceability.

10. Can A790 duplex pipe be used at elevated temperatures?

Duplex steels are susceptible to embrittlement at elevated temperatures and should not be used for prolonged periods at high temperatures.

Request a Quote

Need ASTM A790 welded duplex stainless steel pipe for oil & gas, chemical, desalination, or marine applications? Send requirements including grade (S31803/S32205/S32750), NPS/WT/length, end finish, quantity, and service conditions.

Shangyou Stainless Steel provides custom sizes, processing, and export solutions for global B2B customers.

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2022

  • Total Annual:

    >$10 million

  • Employee Number:

    >100

  • Ecer Certification:

    Verified Supplier

About Us Shaanxi Shangyou Stainless Steel Co., Ltd. is a professional stainless steel manufacturer and global supplier specializing in the production and export of stainless steel pipes, sheets, coils, strips, bars, wires, profiles, and nickel alloy products. Our Expertise With exte... About Us Shaanxi Shangyou Stainless Steel Co., Ltd. is a professional stainless steel manufacturer and global supplier specializing in the production and export of stainless steel pipes, sheets, coils, strips, bars, wires, profiles, and nickel alloy products. Our Expertise With exte...

+ Read More

Get in touch with us

  • Reach Us
  • Shaanxi Shangyou Stainless Steel Co., Ltd.
  • No. 09, Zone E, Zhongchu Logistics, Lintong District, Xi'an City, Shaanxi Province
  • https://www.stainless-steelss.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement